Please wait a minute...
金属学报  2017, Vol. 53 Issue (6): 760-768    DOI: 10.11900/0412.1961.2016.00468
  本期目录 | 过刊浏览 |
Fe-C-Mn三元合金中奥氏体-铁素体相变的相场模拟
张军1,2,陈文雄2,郑成武2(),李殿中2
1 中国科学技术大学化学与材料科学学院 合肥 2300262 中国科学院金属研究所沈阳材料科学国家(联合)实验室 沈阳 110016
Phase-Field Modeling of Austenite-to-Ferrite Transformation in Fe-C-Mn Ternary Alloys
Jun ZHANG1,2,Wenxiong CHEN2,Chengwu ZHENG2(),Dianzhong LI2
1 School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230026, China
2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
引用本文:

张军,陈文雄,郑成武,李殿中. Fe-C-Mn三元合金中奥氏体-铁素体相变的相场模拟[J]. 金属学报, 2017, 53(6): 760-768.
Jun ZHANG, Wenxiong CHEN, Chengwu ZHENG, Dianzhong LI. Phase-Field Modeling of Austenite-to-Ferrite Transformation in Fe-C-Mn Ternary Alloys[J]. Acta Metall Sin, 2017, 53(6): 760-768.

全文: PDF(2800 KB)   HTML
摘要: 

采用相场法研究了Fe-C-Mn三元合金在临界区等温过程中发生的奥氏体-铁素体相变。基于Gibbs自由能守恒理论,在相场模型中考虑了替换型元素Mn在奥氏体/铁素体相界面内扩散所导致的自由能耗散,描述了Fe-C-Mn三元合金中因Mn在相界面偏聚所导致的相变停滞和相变不完全现象。利用相场模型研究了Mn含量对奥氏体-铁素体相变微观组织转变和相变动力学的影响。结果表明,随着Mn含量的增加,铁素体相的转变速率和体积分数降低,Mn在奥氏体/铁素体相界面内扩散所导致的溶质拖曳现象越明显,相变不完全程度加剧。

关键词 : 相场法,  奥氏体,  铁素体,  Gibbs自由能耗散,  相变不完全    
Abstract:

The effect of Mn on the austenite-to-ferrite transformation has been widely studied by both physical models and experiments due to its technological importance for alloy design in steel industries. In recent years, an increasing interest of this issue is moved onto the effect of alloying element on the migrating interface during the austenite-to-ferrite transformation. For ternary Fe-C-Mn alloys, the interfacial condition is more complicated than that of binary Fe-C alloys in view of the large difference in the diffusivity between the interstitial and substitutional alloying elements. Generally speaking, there are two main concepts, i.e. the paraequilibrium model and the local-equilibrium model, which have been proposed to describe the phase transformation kinetics in ternary Fe-C-Mn alloys based on different assumptions about the diffusion of the substitutional elements. And many modeling attempts have been made to study the effect of Mn on the migration kinetics by using these theories. In this work, a multi-phase-field (MPF) model coupling with a Gibbs-energy dissipation model was developed to simulate the isothermal austenite-to-ferrite transformation in ternary Fe-C-Mn alloys. This model has considered the Mn diffusion inside the migrating interface in a physical manner and takes its effect on the transformation kinetics into account. Comparison simulations were made to analyze the difference in the transformation kinetics and ferrite morphologies with and without considering the energy dissipation at the moving interface. It shows that the incomplete transformation phenomenon does occur due to the Mn diffusion inside interface. The modified MPF model was then used to study the effect of Mn contents on the microstructures and kinetics of the phase transformations. It is found that the ferrite growth along the austenite/austenite boundaries is faster than that in the perpendicular direction. This difference is intensified with increasing the Mn concentration, which hence leads to the ferrite morphology changed from elliptical to flat alike. It also produces a slower transformation kinetics and a larger degree of the incomplete transformation when increasing the Mn concentration.

Key words: phase-field method    austenite    ferrite    Gibbs-energy dissipation    incomplete transformation
收稿日期: 2016-10-21     
基金资助:国家自然科学基金项目Nos.51371169和51401214
图1  相界面处Mn化学势的分布示意图
图2  γ→α相变过程中耗散自由能(ΔGdis)的变化
Parameter (unit) Value Ref.
σα,γ(Jm-2) 0.4 [20,31]
σγ,γ(Jm-2) 0.79 [31]
DintMn(cm2s-1) 0.5exp-247650/RT [20]
MCγ( m2molJ-1s-1) 1RT1.5×10-5exp-142000/RT [32]
MCα( m2molJ-1s-1) 1RT2.2×10-4exp-125000/RT [32]
Mp( mmolJ-1s-1) 0.5exp-140000/RT [32]
表1  模拟所采用的物理参数
图3  973 K等温时单个铁素体晶粒的生长过程
图4  973 K等温时铁素体晶粒的生长动力学
图5  相界面迁移过程中ΔGchem与ΔGdis的变化情况
图6  不同合金的奥氏体-铁素体化学驱动力(ΔGchem)与相变温度(T)的关系
图7  1043 K等温时不同合金相变过程中微观组织演化的模拟结果
图8  1043 K等温时不同合金相变过程中C浓度场演化的模拟结果
图9  不同合金在1043 K等温时的转变动力学
图10  不同Mn含量下相变不完全的转变程度
[1] Purdy G, ?gren J, Borgenstam A, et al.ALEMI: A ten-year history of discussions of alloying-element interactions with migrating interfaces[J]. Metall. Mater. Trans., 2011, 42A: 3703
[2] Christian J W.The Theory of Transformations in Metals and Alloys[M]. 3rd Ed., Oxford: Elsevier Science, 2002: 1
[3] Hillert M.Diffusion and interface control of reactions in alloys[J]. Metall. Trans., 1975, 6A: 5
[4] Zener C.Theory of growth of spherical precipitates from solid solution[J]. J. Appl. Phys., 1949, 20: 950
[5] Hultgren A.Isothermal transformation of austenite[J]. Trans. Am. Soc. Met., 1947, 39: 915
[6] Hillert M, ?gren J.On the definitions of paraequilibrium and orthoequilibrium[J]. Scr. Mater., 2004, 50: 697
[7] Coates D E.Diffusion-controlled precipitate growth in ternary systems I[J]. Metall. Trans., 1972, 3: 1203
[8] Hillert M.Nature of local equilibrium at the interface in the growth of ferrite from alloyed austenite[J]. Scr. Mater., 2002, 46: 447
[9] Sietsma J, van der Zwaag S. A concise model for mixed-mode phase transformations in the solid state[J]. Acta Mater., 2004, 52: 4143
[10] Krielaart G P, Sietsma J, van der Zwaag S. Ferrite formation in Fe-C alloys during austenite decomposition under non-equilibrium interface conditions[J]. Mater. Sci. Eng., 1997, A237: 216
[11] Gamsjager E. Kinetics of the austenite-to-ferrite phase transformation——From the intrinsic to an effective interface mobility [J]. Mater. Sci. Forum, 2007, 539-543: 2570
[12] Purdy G R, Brechet Y J M. A solute drag treatment of the effects of alloying elements on the rate of the proeutectoid ferrite transformation in steels[J]. Acta Metall. Mater., 1995, 43: 3763
[13] Hillert M, Sundman B.A treatment of the solute drag on moving grain boundaries and phase interfaces in binary alloys[J]. Acta Metall., 1976, 24: 731
[14] Hillert M.Solute drag, solute trapping and diffusional dissipation of Gibbs energy[J]. Acta Mater., 1999, 47: 4481
[15] Hillert M, Odqvist J, ?gren J.Comparison between solute drag and dissipation of Gibbs energy by diffusion[J]. Scr. Mater., 2001, 45: 221
[16] Enomoto M.Influence of solute drag on the growth of proeutectoid ferrite in Fe-C-Mn alloy[J]. Acta Mater., 1999, 47: 3533
[17] Zurob H S, Panahi D, Hutchinson C R, et al.Self-consistent model for planar ferrite growth in Fe-C-X alloys[J]. Metall. Mater. Trans., 2013, 44A: 3456
[18] Chen H, van der Zwaag S. A general mixed-mode model for the austenite-to-ferrite transformation kinetics in Fe-C-M alloys[J]. Acta Mater., 2014, 72: 1
[19] Loginova I, Odqvist J, Amberg G, et al.The phase-field approach and solute drag modeling of the transition to massive γ→α transformation in binary Fe-C alloys[J]. Acta Mater., 2003, 51: 1327
[20] Zhu B Q, Chen H, Militzer M.Phase-field modeling of cyclic phase transformations in low-carbon steels[J]. Comput. Mater. Sci., 2015, 108: 333
[21] Moelans N, Blanpain B, Wollants P.Quantitative analysis of grain boundary properties in a generalized phase field model for grain growth in anisotropic systems[J]. Phys. Rev., 2008, 78B: 024113
[22] Zaeem M A, El Kadiri H, Wang P T, et al.Investigating the effects of grain boundary energy anisotropy and second-phase particles on grain growth using a phase-field model[J]. Comput. Mater. Sci., 2011, 50: 2488
[23] Chang K, Moelans N.Effect of grain boundary energy anisotropy on highly textured grain structures studied by phase-field simulations[J]. Acta Mater., 2014, 64: 443
[24] Loginova I, ?gren J, Amberg G.On the formation of Widmanst?tten ferrite in binary Fe-C-phase-field approach[J]. Acta Mater., 2004, 52: 4055
[25] Mecozzi M G, Sietsma J, van der Zwaag S, et al. Analysis of the γ→α transformation in a C-Mn steel by phase-field modeling[J]. Metall. Mater. Trans., 2005, 36A: 2327
[26] Huang C J, Browne D J, McFadden S. A phase-field simulation of austenite to ferrite transformation kinetics in low carbon steels[J]. Acta Mater., 2006, 54: 11
[27] Moelans N.A quantitative and thermodynamically consistent phase-field interpolation function for multi-phase systems[J]. Acta Mater., 2011, 59: 1077
[28] Zhang J, Zheng C W, Li D Z.Modeling of isothermal austenite to ferrite transformation in a Fe-C alloy by phase-field method[J]. Acta Metall. Sin., 2016, 52: 1449
[28] (张军, 郑成武, 李殿中. 相场法模拟Fe-C合金中奥氏体-铁素体等温相变过程[J]. 金属学报, 2016, 52: 1449)
[29] Gustafson P.A thermodynamic evaluation of the C-Fe-W system[J]. Metall. Trans., 1987, 18A: 175
[30] Huang W M.A thermodynamic assessment of the Fe-Mn-C system[J]. Metall. Trans., 1990, 21A: 2115
[31] Savran V I.Austenite formation in C-Mn steel [D]. Delft: Delft University of Technology, 2009
[32] Zheng C W, Raabe D.Interaction between recrystallization and phase transformation during intercritical annealing in a cold-rolled dual-phase steel: A cellular automaton model[J]. Acta Mater., 2013, 61: 5504
[33] Chen H, van der Zwaag S. Analysis of ferrite growth retardation induced by local Mn enrichment in austenite created by prior interface passages[J]. Acta Mater., 2013, 61: 1338
[1] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[2] 赵亚峰, 刘苏杰, 陈云, 马会, 马广财, 郭翼. 铁素体-贝氏体双相钢韧性断裂过程中的夹杂物临界尺寸及孔洞生长[J]. 金属学报, 2023, 59(5): 611-622.
[3] 王滨, 牛梦超, 王威, 姜涛, 栾军华, 杨柯. 含Cu马氏体时效不锈钢的组织与强韧性[J]. 金属学报, 2023, 59(5): 636-646.
[4] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[5] 程远遥, 赵刚, 许德明, 毛新平, 李光强. 奥氏体化温度对Si-Mn钢热轧板淬火-配分处理后显微组织和力学性能的影响[J]. 金属学报, 2023, 59(3): 413-423.
[6] 常立涛. 压水堆主回路高温水中奥氏体不锈钢加工表面的腐蚀与应力腐蚀裂纹萌生:研究进展及展望[J]. 金属学报, 2023, 59(2): 191-204.
[7] 侯旭儒, 赵琳, 任淑彬, 彭云, 马成勇, 田志凌. 热输入对电弧增材制造船用高强钢组织与力学性能的影响[J]. 金属学报, 2023, 59(10): 1311-1323.
[8] 李赛, 杨泽南, 张弛, 杨志刚. 珠光体-奥氏体相变中扩散通道的相场法研究[J]. 金属学报, 2023, 59(10): 1376-1388.
[9] 周红伟, 高建兵, 沈加明, 赵伟, 白凤梅, 何宜柱. 高温低周疲劳下C-HRA-5奥氏体耐热钢中孪晶界演变[J]. 金属学报, 2022, 58(8): 1013-1023.
[10] 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中. 3Mn-0.2C中锰钢形变诱导铁素体动态相变机理[J]. 金属学报, 2022, 58(5): 649-659.
[11] 沈国慧, 胡斌, 杨占兵, 罗海文. 回火温度对含 δ 铁素体高铝中锰钢力学性能和显微组织的影响[J]. 金属学报, 2022, 58(2): 165-174.
[12] 郑椿, 刘嘉斌, 江来珠, 杨成, 姜美雪. 拉伸变形对高氮奥氏体不锈钢显微组织和耐腐蚀性能的影响[J]. 金属学报, 2022, 58(2): 193-205.
[13] 化雨, 陈建国, 余黎明, 司永宏, 刘晨曦, 李会军, 刘永长. 高Cr铁素体耐热钢与奥氏体耐热钢的异种材料扩散连接接头组织演变及力学性能[J]. 金属学报, 2022, 58(2): 141-154.
[14] 韩汝洋, 杨庚蔚, 孙新军, 赵刚, 梁小凯, 朱晓翔. 钒微合金化中锰马氏体耐磨钢奥氏体晶粒长大行为[J]. 金属学报, 2022, 58(12): 1589-1599.
[15] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.