| 镍基粉末高温合金热加工变形过程中显微组织不稳定性对热塑性的影响 |
张明1,2, 刘国权1,2( ), 胡本芙1 |
1 北京科技大学材料科学与工程学院 北京 100083 2 北京科技大学钢铁共性技术协同创新中心 北京 100083 |
|
| Effect of Microstructure Instability on Hot Plasticity During Thermomechanical Processing in PM Nickel-Based Superalloy |
Ming ZHANG1,2, Guoquan LIU1,2( ), Benfu HU1 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
张明, 刘国权, 胡本芙. 镍基粉末高温合金热加工变形过程中显微组织不稳定性对热塑性的影响[J]. 金属学报, 2017, 53(11): 1469-1477.
Ming ZHANG,
Guoquan LIU,
Benfu HU.
Effect of Microstructure Instability on Hot Plasticity During Thermomechanical Processing in PM Nickel-Based Superalloy[J]. Acta Metall Sin, 2017, 53(11): 1469-1477.
| [1] | Gessinger G H, Bomford M J.Powder metallurgy of superalloys[J]. Int. Metall. Rev., 1974, 19: 51 | | [2] | Wilkinson N A.Technological considerations in the forging of superalloy rotor parts[J]. Met. Technol., 1977, 4: 346 | | [3] | Immarigeon J P A, Van Drunen G, Wallace W. The hot working behaviour of Mar M200 superalloy compacts [A]. Superalloys 1976: Proceedings of the Third International Symposium[C]. Seven Springs, PA: TMS, 1976: 463 | | [4] | Coyne J E.Microstructural control in titanium-and nickel-base forgings; An overview[J]. Met. Technol., 1977, 4: 337 | | [5] | Semiatin S L, McClary K E, Rollett A D, et al. Plastic flow and microstructure evolution during thermomechanical processing of a PM nickel-base superalloy[J]. Metall. Mater. Trans., 2013, 44A: 2778 | | [6] | Wu K, Liu G Q, Hu B F, et al.Effect of processing parameters on hot compressive deformation behavior of a new Ni-Cr-Co based P/M superalloy[J]. Mater. Sci. Eng., 2011, A528: 4620 | | [7] | Ning Y Q, Yao Z K, Li H, et al.High temperature deformation behavior of hot isostatically pressed P/M FGH4096 superalloy[J]. Mater. Sci. Eng., 2010, A527: 961 | | [8] | Alniak M O, Bedir F.Modelling of deformation and microstructural changes in P/M René 95 under isothermal forging conditions[J]. Mater. Sci. Eng., 2006, A429: 295 | | [9] | Liu Y H, Ning Y Q, Yao Z K, et al.Plastic deformation and dynamic recrystallization of a powder metallurgical nickel-based superalloy[J]. J. Alloys Compd., 2016, 675: 73 | | [10] | He G A, Liu F, Si J Y, et al.Characterization of hot compression behavior of a new HIPed nickel-based P/M superalloy using processing maps[J]. Mater. Des., 2015, 87: 256 | | [11] | Zhang C, Zhang L W, Li M F, et al.Effects of microstructure and γ′ distribution on the hot deformation behavior for a powder metallurgy superalloy FGH96[J]. J. Mater. Res., 2014, 29: 2799 | | [12] | Zhang H B, Zhang K F, Lu Z, et al.Hot deformation behavior and processing map of a γ′-hardened nickel-based superalloy[J]. Mater. Sci. Eng., 2014, A604: 1 | | [13] | Wu K, Liu G Q, Hu B F, et al.Characterization of hot deformation behavior of a new Ni-Cr-Co based P/M superalloy[J]. Mater. Charact., 2010, 61: 330 | | [14] | Zhang M J, Li F G, Wang S Y, et al.Characterization of hot deformation behavior of a P/M nickel-base superalloy using processing map and activation energy[J]. Mater. Sci. Eng., 2010, A527: 6771 | | [15] | Kandeil A Y, Immarigeon J P A, Wallace W, et al. Flow behaviour of Mar M200 powder compacts during isothermal forging[J]. Met. Sci., 1980, 14: 493 | | [16] | Alniak M O, Bedir F.Change in grain size and flow strength in P/M René 95 under isothermal forging conditions[J]. Mater. Sci. Eng., 2006, B130: 254 | | [17] | Kikuchi S, Ando S, Shu F, et al.Superplastic deformation and microstructure evolution in PM IN-100 superalloy[J]. J. Mater. Sci., 1990, 25: 4712 | | [18] | Yu Q Y, Yao Z H, Dong J X.Deformation and recrystallization behavior of a coarse-grain, nickel-base superalloy Udimet720Li ingot material[J]. Mater. Charact., 2015, 107: 398 | | [19] | Chen J Y, Dong J X, Zhang M C, et al.Deformation mechanisms in a fine-grained Udimet 720LI nickel-base superalloy with high volume fractions of γ′ phases[J]. Mater. Sci. Eng., 2016, A673: 122 | | [20] | Zhang B J, Zhao G P, Zhang W Y, et al.Deformation mechanisms and microstructural evolution of γ+γ′ duplex aggregates generated during thermomechanical processing of nickel-base superalloys [A]. Proceedings of the 13th International Symposium on Superalloys[C]. Seven Springs, PA: TMS, 2016: 487 | | [21] | Exner H E.Analysis of grain-and particle-size distributions in metallic materials[J]. Int. Metall. Rev., 1972, 17: 25 | | [22] | Hu B F, Jin K S, Li H Y, et al.The interaction of recrystallizing interfaces with precipitates in a P/M nickel-base superalloy[J]. J. Univ. Sci. Eng. Beijing, 1993, 15: 14(胡本芙, 金开生, 李慧英等. FGH95合金再结晶界面与晶内析出γ′相的作用[J]. 北京科技大学学报, 1993, 15: 14) | | [23] | Menzies R G, Davies G J, Edington J W.Microstructural changes during recrystallization of powder-consolidated nickel-base superalloy IN-100[J]. Met. Sci., 1981, 15: 217 | | [24] | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242[J]. Metall. Trans., 1984, 15A: 1883 | | [25] | Prasad Y V R K, Seshacharyulu T. Modelling of hot deformation for microstructural control[J]. Int. Mater. Rev., 1998, 43: 243 | | [26] | Immarigeon J A, Floyd P H.Microstructural instabilities during superplastic forging of a nickel-base superalloy compact[J]. Metall. Trans., 1981, 12A: 1177 | | [27] | Lin Y C, Wu X Y, Chen X M, et al.EBSD study of a hot deformed nickel-based superalloy[J]. J. Alloys Compd., 2015, 640: 101 | | [28] | Chen X M, Lin Y C, Wen D X, et al.Dynamic recrystallization behavior of a typical nickel-based superalloy during hot deformation[J]. Mater. Des., 2014, 57: 568 | | [29] | Menzies R G, Edington J W, Davies G J.Superplastic behaviour of powder-consolidated nickel-base superalloy IN-100[J]. Met. Sci., 1981, 15: 210 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|