| Al-Mg-Si合金中针棒状析出相时效析出动力学及强化模拟研究* |
陈瑞,许庆彦( ),柳百成 |
| 清华大学材料科学与工程学院先进成形制造教育部重点实验, 北京 100084 |
|
| MODELLING INVESTIGATION OF PRECIPITATION KINETICS AND STRENGTHENING FOR NEEDLE/ROD-SHAPED PRECIPITATES INAl-Mg-Si ALLOYS |
Rui CHEN,Qingyan XU( ),Baicheng LIU |
| Key Laboratory for Advanced Materials Processing Technology (MOE, School of Materials Science and Engineerin, Tsinghua Universit, Beijing 10008, China |
引用本文:
陈瑞,许庆彦,柳百成. Al-Mg-Si合金中针棒状析出相时效析出动力学及强化模拟研究*[J]. 金属学报, 2016, 52(8): 987-999.
Rui CHEN,
Qingyan XU,
Baicheng LIU.
MODELLING INVESTIGATION OF PRECIPITATION KINETICS AND STRENGTHENING FOR NEEDLE/ROD-SHAPED PRECIPITATES INAl-Mg-Si ALLOYS[J]. Acta Metall Sin, 2016, 52(8): 987-999.
| [1] | Murayama M, Hono K.Acta Mater, 1999; 47: 1537 | | [2] | Maisonnette D, Suery M, Nelias D, Chaudet P, Epicier T.Mater Sci Eng, 2011; A528: 2718 | | [3] | Zhang G J, Liu G, Ding X D, Sun J, Chen K H.Acta Metall Sin, 2003; 39: 803 | | [3] | (张国君, 刘刚, 丁向东, 孙军, 陈康华. 金属学报, 2003; 39: 803) | | [4] | Wang X N, Han L Z, Gu J F.Chin J Nonferrous Met, 2013; 23: 2754 | | [4] | (王小娜, 韩利战, 顾剑锋. 中国有色金属学报, 2013; 23: 2754 ) | | [5] | Vaithyanathan V, Wolverton C, Chen L Q.Phys Rev Lett, 2002; 88: 148 | | [6] | Shercliff H R, Ashby M F.Acta Metall Mater, 1990; 38: 1789 | | [7] | Esmaeili S, Lloyd D J, Poole W J.Acta Mater, 2003; 51: 2243 | | [8] | Yazdanmehr M, Bahrami A, Mousavi Anijdan S H.Comput Mater Sci, 2009; 45: 385 | | [9] | Wang X N, Han L Z, Gu J F.Acta Metall Sin, 2014; 50: 355 | | [9] | (王小娜, 韩利战, 顾剑锋. 金属学报, 2014; 50: 355 ) | | [10] | Wagner R, Kampmann R.In: Cahn R W ed., Materials Science and Technology: a Comprehensive Treatment. Weinheim: John Wiley, 1991: 1 | | [11] | Myhr O R, Grong ?..Acta Mater, 2000; 48: 1605 | | [12] | Maugis P, Gouné M.Acta Mater, 2005; 53: 3359 | | [13] | Zhang C, Cao W, Chen S L, Zhu J, Zhang F, Luo A A, Schmid-Fetzer R.JOM, 2014; 66: 389 | | [14] | Rougier L, Jacot A, Gandin C, Napoli P D, Théry P, Ponsen D, Jaquet V.Acta Mater, 2013; 61: 6396 | | [15] | Myhr O R, Grong ?, Andersen S J.Acta Mater, 2001; 49: 65 | | [16] | Larráyoz lzcara X, Guirao Blank A, Pyczak F, Staron P, Schumann S, Huber N.Mater Sci Eng, 2014; A610: 46 | | [17] | Eivani A R, Anmed H, Zhou J, Duszczyk J.Mater Sci Eng, 2010; A527: 2418 | | [18] | Samars S N.Modell Simul Mater Sci Eng, 2006; 14: 1271 | | [19] | Bahrami A, Miroux A, Sietsma J.Metall Mater Trans, 2012; 43A: 4445 | | [20] | Bardel D, Perez M, Nelias D, Deschamps A, Hutchinson C R, Maisonnette D, Chaise T, Garnier J, Bourlier F.Acta Mater, 2014; 62: 129 | | [21] | Liu G, Zhang G J, Ding X D, Sun J, Chen K H.Mater Sci Eng, 2003; A344: 113 | | [22] | Zhang R J, He Z, Wang X Y, Jie W Q.Mater Lett, 2005; 59: 2765 | | [23] | Du Q, Poole W J, Wells M A.Acta Mater, 2012; 60: 3830 | | [24] | Robson J D, Jones M J, Prangnell P B.Acta Mater, 2003; 51: 1453 | | [25] | Jiang L, Li J K, Cheng P M, Liu G, Wang R H, Chen B A, Zhang J Y, Sun J, Yang M X, Yang G.Mater Sci Eng, 2014; A607: 596 | | [26] | Hillert M. Phase Equilibria Phase Diagrams and Phase Transformations: Their Thermodynamic Basis. 2nd Ed., Cambridge: Cambridge University Press, 2008: 1 | | [27] | Perez M, Dumont M, Acevedo-Reyes D.Acta Mater, 2009; 57: 1318 | | [28] | Chen Q, Jeppsson J, ?gren J.Acta Mater, 2008; 56: 1890 | | [29] | Zhang J, Deng Y L, Zhang X M.Mater Sci Eng, 2013; A563: 8 | | [30] | Khan I N, Starink M J, Yan J L.Mater Sci Eng, 2008; A472: 66 | | [31] | Ahmadi M R, Povoden-Karadeniz E, ?ksúz K I, Falahati A, Eozeschnik E.Comput Mater Sci, 2014; 91: 173 | | [32] | Ardell A J.Metall Trans, 1985; 16A: 2131 | | [33] | Leyson G P M, Hector Jr L G, Curtin W A.Acta Mater, 2012; 60: 3873 | | [34] | Zhao Q L, Holmedal B.Mater Sci Eng, 2013; A563: 147 | | [35] | Sj?lander E, Seifeddine S, Svensson I L.Int J Cast Met Res, 2011; 24: 338 | | [36] | Koppenaal T J, Kuhlmann-Wilsdorf D.Appl Phys Lett, 1964; 4: 59 | | [37] | Kuehman C J, Voorhees P W.Metall Mater Trans, 1996; 27A: 937 | | [38] | Tiryakioglu M, ?kten G, Hudak D.J Mater Sci, 2009; 44: 5754 | | [39] | Esmaeili S.PhD Dissertation, The University of British Columbia, Vancouver, 2003 | | [40] | Gupta A K, Lloyd D J, Court S A.Mater Sci Eng, 2001; A316: 11 | | [41] | Hirth S M, Marshall G J, Court S A, Lloyd D J. Mater Sci Eng, 2001; A319-321: 452 | | [42] | Son S K, Matsumura S, Fukui K, Takeda M.J Alloys Compd, 2011; 509: 241 | | [43] | Ji Y L, Zhong H, Hu P, Guo F.Mater Des, 2011; 32: 2974 |
|
|