| 冷拔珠光体钢的组织演变对其点蚀行为的影响* |
何岳1,向嵩1,2,3( ),石维1,2,刘建敏1,梁宇1,2,陈朝轶1 |
| 1 贵州大学材料与冶金学院, 贵阳 5500252 贵州省材料结构与强度重点实验室, 贵阳 5500253 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| EFFECT OF MICROSTRUCTURAL EVOLUTION ON THE PITTING CORROSION OF COLD DRAWING PEARLITIC STEELS |
Yue HE1,Song XIANG1,2,3( ),Wei SHI1,2,Jianmin LIU1,Yu LIANG1,2,Chaoyi CHEN1 |
1 College of Materials and Metallurgy, Guizhou University, Guiyang 550025, China 2 Guizhou Key Laboratory for Mechanical Behavior and Micro Structure of Materials, Guiyang 550025, China 3 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
何岳,向嵩,石维,刘建敏,梁宇,陈朝轶. 冷拔珠光体钢的组织演变对其点蚀行为的影响*[J]. 金属学报, 2016, 52(12): 1536-1544.
Yue HE,
Song XIANG,
Wei SHI,
Jianmin LIU,
Yu LIANG,
Chaoyi CHEN.
EFFECT OF MICROSTRUCTURAL EVOLUTION ON THE PITTING CORROSION OF COLD DRAWING PEARLITIC STEELS[J]. Acta Metall Sin, 2016, 52(12): 1536-1544.
| [1] | Bhandari J, Khan F, Abbassi R, Garaniya V, Ojeda R.J Loss Prev Process Ind, 2015; 37: 39 | | [2] | Bang C W, Seol J B, Yang Y S, Park C G.Scr Mater, 2015; 108: 151 | | [3] | Lamontagne A, Massardier V, Kléber X, Sauvage X, Mari D.Mater Sci Eng, 2015; A644: 105 | | [4] | Zhang X, Godfrey A, Huang X, Hansen N, Liu Q.Acta Mater, 2011; 59: 3422 | | [5] | Zelin M.Acta Mater, 2002; 50: 4431 | | [6] | Toribio J, González B, Matos J C, Ayaso F J.Int J Fatigue, 2015; 76: 53 | | [7] | Zhao T Z, Zhang S H, Zhang G L, Song H W, Cheng M.Mater Des, 2014; 59: 397 | | [8] | Toribio J, González B, Matos J C.Eng Fract Mech, 2010; 77: 2024 | | [9] | Elices M.J Mater Sci, 2004; 39: 3889 | | [10] | Sánchez J, Fullea J, Andrade C, Gaitero J J, Porro A. Corros Sci, 2008; 50: 1820 | | [11] | Rault V, Vignal V, Krawiec H, Tadjoa O.Corros Sci, 2014; 86: 275 | | [12] | Guo Y, Sun T, Hu J, Jiang Y, Jiang L, Li J.J Alloys Compd, 2016; 658: 1031 | | [13] | Ren Y, Zhao H, Liu W, Yang K.Mater Sci Eng, 2016; C60: 293 | | [14] | Feng X, Lu X, Zuo Y, Zhuang N, Chen D.Corros Sci, 2016; 103: 223 | | [15] | Cheng Y F, Yang C, Luo J L.Thin Solid Films, 2002; 416: 169 | | [16] | Zhang F, Pan J, Lin C. Corros Sci, 2009; 51: 2130 | | [17] | Wang H, Xie J, Yan K P, Duan M, Zuo Y.Corros Sci, 2009; 51: 181 | | [18] | Guo N.PhD Dissertation, Chongqing University, 2012 | | [18] | (郭宁. 重庆大学博士学位论文, 2012) | | [19] | Zhang X D, Godfrey A, Hansen N, Huang X.Acta Mater, 2013; 61: 4898 | | [20] | Zhang X D.PhD Dissertation, Tsinghua Univerisity, Beijing, 2009 | | [20] | (张晓丹. 清华大学博士学位论文, 北京, 2009) | | [21] | Zhang X D, Godfrey A, Liu W, Liu Q.Acta Metall Sin, 2010; 46: 141 | | [21] | (张晓丹, Godfrey A, 刘伟, 刘庆. 金属学报, 2010; 46: 141) | | [22] | Cao C N, Xiao J M.Principles of Material Corrosion. Beijing: Chemical Industry Press, 2004: 48 | | [22] | (曹楚南, 肖纪美. 材料腐蚀学原理. 北京: 化学工业出版社, 2004: 48) | | [23] | Burstein G T, Pistorius P C, Mattin S P.Corros Sci, 1993; 35: 57 | | [24] | Yang D J. Metal Corrosion.Beijing: Metallurgical Industry Press, 1999: 97 | | [24] | (杨德钧. 金属腐蚀学. 北京: 冶金工业出版社, 1999: 97) | | [25] | Yu Y N.Fundamental of Materials Science. Beijing: Higher Education Press, 2012: 421 | | [25] | (余永宁. 材料科学基础. 北京: 高等教育出版社, 2012: 421) | | [26] | Rault V, Vignal V, Krawiec H, Dufour F.Corros Sci, 2015; 100: 667 | | [27] | Li Y J, Choi P, Borchers C, Chen Y Z, Goto S, Raabe D, Kirchheim R.Ultramicroscopy, 2011; 111: 628 | | [28] | Min N, Li W, Li H, Jin X.J Mater Sci Technol, 2010; 26: 776 |
|
|