| 高压环境下CMT焊接电弧行为及焊缝性能* |
黄继强1( ),薛龙1,黄军芬1,邹勇1,牛虎理2,唐德渝2 |
1 北京石油化工学院光机电装备技术北京市重点实验室, 北京 102617 2 中国石油集团工程技术研究院, 天津 300451 |
|
| ARC BEHAVIOR AND JOINTS PERFORMANCE OF CMT WELDING PROCESS IN HYPERBARIC ATMOSPHERE |
Jiqiang HUANG1( ),Long XUE1,Junfen HUANG1,Yong ZOU1,Huli NIU2,Deyu TANG2 |
1 Opto-Mechatronic Equipment Technology Beijing Area Major Laboratory, Beijing Institute of Petrochemical Technology, Beijing 102617, China 2 Research Institute of Engineering Technology, China National Petroleum Corporation, Tianjin 300451, China |
引用本文:
黄继强,薛龙,黄军芬,邹勇,牛虎理,唐德渝. 高压环境下CMT焊接电弧行为及焊缝性能*[J]. 金属学报, 2016, 52(1): 93-99.
Jiqiang HUANG,
Long XUE,
Junfen HUANG,
Yong ZOU,
Huli NIU,
Deyu TANG.
ARC BEHAVIOR AND JOINTS PERFORMANCE OF CMT WELDING PROCESS IN HYPERBARIC ATMOSPHERE[J]. Acta Metall Sin, 2016, 52(1): 93-99.
| [1] | Jiang L P, Wang Z H, Jiao X D, Zhou C F, Fang X M, Ma H X. Trans China Weld Inst, 2007; 28(6): 1 | | [1] | (蒋力培, 王中辉, 焦向东, 周灿丰, 房晓明, 马洪新. 焊接学报, 2007; 28(6): 1) | | [2] | Shi Y W,Zhang X P,Lei Y P. Welding Technology in Special Conditions. Beijing: China Machine Press, 2000: 1 | | [2] | (史耀武,张新平,雷永平. 严酷条件下的焊接技术. 北京: 机械工业出版社, 2000: 1) | | [3] | Song B T. Underwater Welding and Cutting. Beijing: China Machine Press, 1989: 5 | | [3] | (宋宝天. 水下焊接及切割. 北京: 机械工业出版社, 1989: 5) | | [4] | Woodward N J. Welding J, 2006; 85(10): 35 | | [5] | Marino R, Blackman S A, Woodward N J. Pipeline World, 2004; 25(6): 11 | | [6] | Suga Y. Welding under Extreme Conditions. Oxford: Pergamon Press, 1989: 207 | | [7] | Richardson I M, Woodward N J, Billingham J. In: Jin S C, Matsui T, Chen J W, Kyozuka Y eds., Proc of 12th Int Conf on Offshore and Polar Arctic Engineering, Kitatyushu: International Society of Offshore and Polar Arctic Engineering, 2002: 295 | | [8] | Dos Santos J F, Manzenrieder H, Cui H, Recoschewitz J. In: Jin S C ed., Proc of 6th Int Conf on Offshore and Polar Arctic Engineering, San Francisco: International Society of Offshore and Polar Arctic Engineering, 1992: 163 | | [9] | Mallieswaran A, Pugazhendhi A, Azhagarasan S. J Adv Technol Eng, 2012; 1(1): 71 | | [10] | Zhao B, Wu C S, Jia C B, Yuan X. Acta Metall Sin, 2013; 49: 797 | | [10] | (赵 博, 武传松, 贾传宝, 袁 新. 金属学报, 2013; 49: 797) | | [11] | Odd M A, Hans F, Ansgar H. Weld J, 2006; 85(6): 52 | | [12] | Xue L, Wang Z H, Zhou C F, Jiao X D. Trans China Weld Inst, 2006; 27(12): 17 | | [12] | (薛 龙, 王中辉, 周灿丰, 焦向东. 焊接学报, 2006; 27(12): 17) | | [13] | Zhou C F, Jiao X D, Xue L, Chen J Q, Fang X M, Wang W Y. Trans China Weld Inst, 2007; 28(2): 5 | | [13] | (周灿丰, 焦向东, 薛 龙, 陈家庆, 房晓明, 王维越. 焊接学报, 2007; 28(2): 5) | | [14] | Hart P, Richardson I M, Nixon J H. Welding World, 2001; 45(11/12): 29 | | [15] | Hart P. Welding Res Abroad, 2001; 49(3): 29 | | [16] | Akselsen O M, Fostervoll H, Carl H A. In: Jin S C ed., Proc of 18th Int Conf on Offshore and Polar Arctic Engineering, Vancouver: International Society of Offshore and Polar Arctic Engineering, 2008: 246 | | [17] | Akselsen O M, Fostervoll H, Ahlen C H. Int J Offshore Polar Eng, 2010; 20: 110 | | [18] | Azar A S, Woodward N, Fostervoll H, Akselsen O M. J Mater Process Technol, 2012; 21(2): 211 | | [19] | Huang J Q, Xue L, Lu T, Niu H L, Tang D Y, Jiang L P. China Welding, 2012; 21(4): 26 | | [20] | Woodward N J. Int J Offshore Polar Eng, 2014; 24: 206 | | [21] | Paidar M, Khodabandeh A, Najafi H, Alireza S R. Int J Adv Manufacture Technol, 2015; 80(1): 183 | | [22] | Yin S Y. Process and Application of Gas Shielded Arc Welding. 2nd Ed., Beijing: China Machine Press, 2012: 441 | | [22] | (殷树言. 气体保护焊工艺基础及应用, 第2版. 北京: 机械工业出版社, 2012: 441) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|