| 合金元素Cu对金属Zr吸氘动力学机制的影响* |
杨云,宋西平( ) |
| 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| INFLUENCE OF ALLOY ELEMENT Cu ON KINETIC MECHANISMS OF DEUTERIUM ABSORPTION IN ZIRCONIUM |
Yun YANG,Xiping SONG( ) |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
杨云,宋西平. 合金元素Cu对金属Zr吸氘动力学机制的影响*[J]. 金属学报, 2016, 52(1): 100-104.
Yun YANG,
Xiping SONG.
INFLUENCE OF ALLOY ELEMENT Cu ON KINETIC MECHANISMS OF DEUTERIUM ABSORPTION IN ZIRCONIUM[J]. Acta Metall Sin, 2016, 52(1): 100-104.
| [1] | Taylor N, Cortes P. Fusion Eng Des, 2014; 89: 1995 | | [2] | Lupelli I, Murari A, Gaudio P, Gelfusa M, Mazon D, Vega J. Fusion Eng Des, 2013; 88: 738 | | [3] | Hong B G. Fusion Eng Des, 2014; 89: 2493 | | [4] | Pampin R, Davis A, Izquierdo J, Leichtle D, Loughlin M J, Sanz J, Turner A, Villari R, Wilson P P H. Fusion Eng Des, 2013; 88: 454 | | [5] | Kanouff M P, Gharagozloo P E, Salloum M, Shugard A D. Chem Eng Sci, 2013; 91: 212 | | [6] | Shugard A D, Buffleben G M, Johnson T A, Robinson D B. J Nucl Mater, 2014; 447: 304 | | [7] | Bhattacharyya R, Mohan S. Renew Sust Energy Rev, 2015; 41: 872 | | [8] | Ablitzer C, Le Guyadec F, Raynal J, Génin X, Duhart-Barone A. J Nucl Mater, 2013; 432: 135 | | [9] | Totemeier T C. J Nucl Mater, 2000; 278: 301 | | [10] | Le Guyadec F, Génin X, Bayle J P, Dugne O, Duhart-Barone A, Ablitzer C. J Nucl Mater, 2010; 396: 294 | | [11] | Jat R A, Sawant S G, Rajan M B, Dhanuskar J R, Kaity S, Parid S C. J Nucl Mater, 2013; 443: 316 | | [12] | Hu X X, Terrani K A, Wirth B D. J Nucl Mater, 2014; 448: 87 | | [13] | Glazoffa M V, Tokuhiro A, Rashkeev S N, Sabharwalla P. J Nucl Mater, 2014; 444: 65 | | [14] | Zheng J, Zhou X S, Mao L, Zhang H J, Liang J H, Sheng L S, Peng S. Int J Hydrogen Energy Mater, 2015; 40: 4597 | | [15] | Lanzania L, Ruch M. J Nucl Mater, 2004; 324: 165 | | [16] | Wongsawaeng D, Jaiyen S. J Nucl Mater, 2010; 403: 19 | | [17] | Terrani K A, Balooch M, Wongsawaeng D, Jaiyen S, Olander D R. J Nucl Mater, 2010; 397: 61 | | [18] | Zhao C, Song X P, Yang Y, Zhang B. Int J Hydrogen Energy Mater, 2013; 38: 10903 | | [19] | Dou N N. Master Thesis, University of Science and Technology Beijing, 2014 | | [19] | (窦娜娜. 北京科技大学硕士学位论文, 2014) | | [20] | Li Q, Chou K C, Jiang L J, Zhan F. Int J Hydrogen Energy Mater, 2004; 29: 843 | | [21] | Dang J, Zhang G H, Chou K C, Reddy R G, He Y, Sun Y J. Int J Refract Met Hard Mater, 2013; 41: 216 | | [22] | Li W H, Tian B H, Ma P, Wu E D. Acta Metall Sin, 2012; 48: 822 | | [22] | (李武会, 田保红, 马 坪, 吴尔冬. 金属学报, 2012; 48: 822) | | [23] | Yoo H, Kim W, Ju H. Solid State Ionics, 2014; 262: 241 | | [24] | Wang H, Prasad A K, Advani S G. Int J Hydrogen Energy Mater, 2014; 39: 11035 | | [25] | Masanori H, Yukiko H, Kuniaki W. J Alloys Compd, 2009; 487: 489 | | [26] | Filinchuk Y E, Yvon K. Inorg Chem, 2005; 44: 8191 | | [27] | Kadel R, Weiss A. J Less-Common Met, 1979; 65: 89 | | [28] | Couet A, Motta A T, Comstock R J. In: Comstock R J, Barbéris P eds., Zirconium in the Nuclear Industry: 17th International Symposium, West Conshonocken: ASTM International, 2015: 479 |
|
|