| Cu对TA15-2钛合金表面Stellite 12基激光合金化涂层组织结构及耐磨性的影响* |
李嘉宁1,2, 巩水利1( ), 王娟3, 单飞虎1, 李怀学1, 吴冰1 |
1 北京航空制造工程研究所高能束流加工技术重点实验室, 北京 100024 2 北京航空材料研究院, 北京 100095 3 山东大学材料科学与工程学院, 济南 250061 |
|
| INFLUENCE OF Cu ON MICROSTRUCTURES AND WEAR RESISTANCE OF STELLITE 12 MATRIX LASER ALLOYING COATINGS ON TA15-2 TITANIUM ALLOY |
LI Jianing1,2, GONG Shuili1( ), WANG Juan3, SHAN Feihu1, LI Huaixue1, WU Bing1 |
1 Science and Technology on Power Beam Processes Laboratory, Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024 2 Beijing Institute of Aeronautical Materials, Beijing 100095 3 School of Materials Science and Engineering, Shandong University, Jinan 250061 |
引用本文:
李嘉宁, 巩水利, 王娟, 单飞虎, 李怀学, 吴冰. Cu对TA15-2钛合金表面Stellite 12基激光合金化涂层组织结构及耐磨性的影响*[J]. 金属学报, 2014, 50(5): 547-554.
Jianing LI,
Shuili GONG,
Juan WANG,
Feihu SHAN,
Huaixue LI,
Bing WU.
INFLUENCE OF Cu ON MICROSTRUCTURES AND WEAR RESISTANCE OF STELLITE 12 MATRIX LASER ALLOYING COATINGS ON TA15-2 TITANIUM ALLOY[J]. Acta Metall Sin, 2014, 50(5): 547-554.
| [1] |
Mao X N, Zhao Y Q, Yang G J. Rare Met Lett, 2007; 26(5): 1
|
| [1] |
(毛小南, 赵永庆, 杨冠军. 稀有金属快报, 2007; 26(5): 1)
|
| [2] |
Li J N, Gong S L, Liu H, Li H X. Mater Lett, 2013; 92: 235
|
| [3] |
Yue T M, Su Y P. Appl Surf Sci, 2008; 255: 1692
|
| [4] |
Gu D D, Meng G B, Li C, Meiners W, Poprawe R. Scr Mater, 2012; 67: 185
|
| [5] |
Li J N, Gong S L. Physica, 2013; 47E: 193
|
| [6] |
Zhang S, Zhang C H. Acta Metall Sin, 2002; 38: 1100
|
| [6] |
(张 松, 张春华. 金属学报, 2002; 38: 1100)
|
| [7] |
Wu X L, Hong Y S. Surf Coat Technol, 2001; 141: 141
|
| [8] |
Zhu Y Y, Li Z G, Li R F, Li M, Daze X L, Feng K, Wu Y X. Appl Surf Sci, 2013; 280: 50
|
| [9] |
Yarrapareddy E, Kovacevic R. Surf Coat Technol, 2008; 202: 1951
|
| [10] |
Adraider Y, Pang Y X, Nabhani F, Hodgson S N, Zhang Z Y. Surf Coat Technol, 2011; 205: 5345
|
| [11] |
Li Y Z, Wang C S, Li T, Yao B. Chin J Lasers, 2010; 37: 1356
|
| [11] |
(李耀忠, 王存山, 李 婷, 姚 标. 中国激光, 2010; 37: 1356)
|
| [12] |
Wang H Y. Trans Nonferrous Met Soc China, 2011; 21: 1322
|
| [13] |
Sebastiani M, Mangione V, De Felicis D, Bemporad E, Carassiti F. Wear, 2012; 290-291(30): 10
|
| [14] |
Radu I, Li D Y. Wear, 2005; 259: 453
|
| [15] |
Li J N, Gong S L, Yu H J, Chen C Z. J Phys Chem, 2013; 117C: 4568
|
| [16] |
Dai Q X. Metal Material Science. Beijing: Chemical Industry Press, 2005: 36
|
| [16] |
(戴起勋. 金属材料学. 北京: 化学工业出版社, 2005: 36)
|
| [17] |
Guo B G, Zhou J S, Zhang S T, Zhou H D, Pu Y P, Chen J M. Appl Surf Sci, 2007; 253: 9301
|
| [18] |
Shi S H, Fu G Y. Heat Treatment Met, 1999; (3): 14
|
| [18] |
(石世宏, 傅戈雁. 金属热处理, 1999; (3): 14)
|
| [19] |
Li J N, Chen C Z, Zhang C F. Mater Res Innovat, 2011; 15: 344
|
| [20] |
Zhang B W. Physical Fundamentals of Nanomaterials. Beijing: Chemical Industry Press, 2009: 110
|
| [20] |
(张邦维. 纳米材料物理基础. 北京: 化学工业出版社, 2009: 110)
|
| [21] |
Wang J F,Fan X H,Zhang C J. Solid State Physics. Jinan: Shandong University Press, 2003: 163
|
| [21] |
(王矜奉,范希会,张承琚. 固体物理. 济南: 山东大学出版社, 2003: 163)
|
| [22] |
Wang H Y, Zuo D W, Wang M D, Shao J B. Acta Metall Sin, 2009; 45: 971
|
| [22] |
(王宏宇, 左敦稳, 王明娣, 邵建兵. 金属学报, 2009; 45: 971)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|