| 利用第一原理研究合金化对γ-TiAl,抗氧化性能的影响 |
| 平发平,胡青苗,杨锐 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| INVESTIGATION ON EFFECTS OF ALLOYING ON OXIDATION RESISTANCE OFγ-TiAl BY USING FIRST PRINCIPLE |
| PING Faping, HU Qingmiao, YANG Ru |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang |
引用本文:
平发平,胡青苗,杨锐. 利用第一原理研究合金化对γ-TiAl,抗氧化性能的影响[J]. 金属学报, 2013, 29(4): 385-390.
PING Faping,
HU Qingmiao,
YANG Ru.
INVESTIGATION ON EFFECTS OF ALLOYING ON OXIDATION RESISTANCE OFγ-TiAl BY USING FIRST PRINCIPLE[J]. Acta Metall Sin, 2013, 29(4): 385-390.
| [1] Clemens H, Kestler H. Adv Eng Mater, 2000; 2: 551 [2] Kim Y W. JOM, 1989; 41: 24 [3] Subramanian P R, Mendiratta M G, Dimiduk D M, Stucke M A. Mater Sci Eng, 1997; A239-240: 1 [4] Becker S, Rahmel A, Schorr M, Schutze M. Oxid Met, 1992; 38: 425 [5] Brady M, Brindley W, Smialek J, Locci I. JOM, 1996; 48: 46 [6] Niewolak L, Shemet V, Gil A, Singheiser L, Quadakkers J W. Adv Eng Mater, 2001; 3: 496 [7] Haanappel V A C, Sunderkotter J D, Stroosnijder M F. Intermetallics, 1999; 7: 529 [8] Nickel H, Zheng N X, Elschner A, Quadakkers W J. Mikrochim Acta, 1995; 119: 23 [9] Perkins R A, Chiang K T, Meier G H. Scr Metall, 1987; 21: 1505 [10] Shida Y, Anada H. Mater Trans JIM, 1994; 35: 623 [11] Shida Y, Anada H. Oxid Met, 1996; 45: 197 [12] Shida Y, Anada H. Corros Sci, 1993; 35: 945 [13] Wang F H, Tang Z L, Wu W T. Oxid Met, 1997; 48: 381 [14] Taniguchi S, Shibata T. Intermetallics, 1996; 4: S85 [15] Li H, Liu L M, Wang S Q, Ye H Q. Acta Metall Sin, 2006; 42: 897 (李虹, 刘利明, 王绍青, 叶恒强. 金属学报, 2006; 42: 897) [16] Li H, Wang S Q, Ye H Q. J Mater Sci Technol, 2009; 25: 569 [17] Liu S Y, Shang J X, Wang F H, Liu S Y, Yue Z, Xu H B. Phys Rev, 2009; 80B: 085414 [18] Liu S Y, Shang J X, Wang F H, Yue Z. Phys Rev, 2009; 79B: 075419 [19] Liu S Y, Shang J X, Wang F H, Yue Z. J Physics: Condens Matter, 2009; 21: 225005 [20] Luthra K L. Oxid Met, 1991; 36: 475 [21] Rahmel A, Spencer P J. Oxid Met, 1991; 35: 53 [22] Kresse G, Furthmuller J. Phys Rev, 1996; 54B: 11169 [23] Kresse G, Furthmuller J. Comput Mater Sci, 1996; 6: 15 [24] Blochl P E. Phys Rev, 1994; 50B: 17953 [25] Kresse G, Joubert D. Phys Rev, 1999; 59B: 1758 [26] Perdew J P, Burke K, Ernzerhof M. Phys Rev Lett, 1996; 77: 3865 [27] He J, Behera R K, Finnis M W, Li X, Dickey E C, Phillpot S R, Sinnott S B. Acta Mater, 2007; 55: 4325 [28] Li X, Finnis M W, He J, Behera R K, Phillpot S R, Sinnott S B, Dickey E C. Acta Mater, 2009; 57: 5882 [29] Abrahams S C, Bernstei J L. J Chem Phys, 1971; 55: 3206 [30] Matsunaga K, Tanaka T, Yamamoto T, Ikuhara Y. Phys Rev, 2003; 68B: 085110 [31] Boettger J C. Phys Rev, 1997; 55B: 750 [32] Damour H, Schiferl D, Denner W, Schulz H, Holzapfel W B. J Appl Phys, 1978; 49: 4411 [33] Li M S. High Temperature Corrosion of Metals. Beijing: Metallurgical Industry Press, 2001: 11 (李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 11) [34] Wang L, Maxisch T, Ceder G. Phys Rev, 2006; 73B: 195107 [35] Martinez J I, Hansen H A, Rossmeisl J, Norskov J K. Phys Rev, 2009; 79B: 045120 [36] Sousa C, Illas F. Phys Rev, 1994; 50B: 13974 [37] Marquez A M, Plata J J, Ortega Y, Sanz J F. J Phys Chem, 2011; 115C: 16970 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|