快速加热连续退火对超高强TRIP钢显微组织与力学性能的影响 |
许云波1,侯晓英1,王业勤2,吴迪1 |
1. 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819
2. 莱芜钢铁集团有限公司, 莱芜 271104 |
|
EFFECTS OF RAPID HEATING CONTINUOUS ANNEALING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF ULTRA HIGH–STRENGTH TRIP–AIDED STEEL |
XU Yunbo 1, HOU Xiaoying 1, WANG Yeqin 2, WU Di 1 |
1. State Key Laboratory of Rolling Technology and Automation, Northeast University, Shenyang 110819
2. Laiwu Iron and Steel Group Co. Ltd., Laiwu 271104 |
引用本文:
许云波 侯晓英 王业勤 吴迪. 快速加热连续退火对超高强TRIP钢显微组织与力学性能的影响[J]. 金属学报, 2012, 48(2): 176-182.
,
,
,
.
EFFECTS OF RAPID HEATING CONTINUOUS ANNEALING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF ULTRA HIGH–STRENGTH TRIP–AIDED STEEL[J]. Acta Metall Sin, 2012, 48(2): 176-182.
[1] Balk S C, Kim S, Jin Y S, Kwon O. ISIJ Int, 2001; 41: 290
[2] Thomson R C, Miller M K. Acta Mater, 1998; 46: 2203
[3] Kim S J, Lee C G, Lee T H, Oh C S. ISIJ Int, 2002; 42: 1452
[4] Pereloma E V, Russell K F, Miller M K, Timokhina I B. Scr Mater, 2008; 58: 1078
[5] Pereloma E V, Timokhina I B, Hodgson P D. Mater Sci Eng, 1999; A273–275: 448
[6] Jiao S, Hassani F, Donaberger R L, Essadiqi E, Yue S. ISIJ Int, 2002; 42: 299
[7] De Meyer M, Vanderschueren D, De Cooman B C. ISIJ Int, 1999; 39: 813
[8] Chen Y, Wang L H, Dong L G, Li F P, Zhang Y. J Iron Steel Res Int, 2007; 14(suppl 1): 368
[9] Jacques P J, Girault E, Mertens A, Verlinden B, van Humbeeck J, Delannay F. ISIJ Int, 2001; 41: 1068
[10] Mahieu J, Maki J, De Cooman B C, Claessens S. Metall Trans, 2002; 33A: 2573
[11] Maki J, Mahieu J, De Cooman B C, Claessens S. Curr Opin Solid State Mater Sci, 2004; 8: 285
[12] Sakuma Y, Matsumura O, Akisue O. ISIJ Int, 1991; 31: 1348
[13] Basuki A, Aernoudt E. Scr Mater, 1999; 40: 1003
[14] Jimenez–Melero E, van Dijk N H, Zhao L, Sietsma J, Offerman S E, Wright J P, van der Zwaag S. Acta Mater, 2009; 57: 533
[15] Chen H C, Era H, Shimizu M. Metall Trans, 1989; 20A: 437
[16] Lesch C, Alvarez P, BleckW, Gil Sevillano J. Metall Mater Trans, 2007; 38A: 1882
[17] Salvatori I, Moore W B R. ISIJ Int, 2000; 40(suppl 1): 179
[18] Reis A C C, Bracke L, Petrov R, Kaluba W J, Kestens L. ISIJ Int, 2003; 43: 1260
[19] Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|