| DD98M镍基单晶高温合金900℃高周疲劳行为 |
| 韩国明1,张振兴2,李金国1,金涛1,孙晓峰1,胡壮麒1 |
1. 中国科学院金属研究所, 沈阳 110016
2. 东北大学材料与冶金学院, 沈阳 110819 |
|
| HIGH CYCLE FATIGUE BEHAVIOR OF A NICKEL–BASED SINGLE CRYSTAL SUPERALLOY DD98M AT 900 ℃ |
| HAN Guoming 1, ZHANG Zhenxing 2, LI Jinguo 1, JIN Tao 1, SUN Xiaofeng 1, HU Zhuangqi 1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. School of Materials and Metallurgy, Northeastern University, Shenyang 110819 |
引用本文:
韩国明 张振兴 李金国 金涛 孙晓峰 胡壮麒. DD98M镍基单晶高温合金900℃高周疲劳行为[J]. 金属学报, 2012, 48(2): 170-175.
,
,
,
,
,
.
HIGH CYCLE FATIGUE BEHAVIOR OF A NICKEL–BASED SINGLE CRYSTAL SUPERALLOY DD98M AT 900 ℃[J]. Acta Metall Sin, 2012, 48(2): 170-175.
| [1] Cowles B A. Int J Fract, 1996; 80: 147[2] Gao Y, St¨olken J S, Kumar M, Ritchie R O. Acta Mater, 2007; 55: 3155[3] Liu L, Husseini N S, Torbet C J, Lee WK, Clarke R, Jones J W, Pollock T M. Acta Mater, 2011; 59: 5103[4] Yi J Z, Torbet C J, Feng Q, Pollock T M, Jones J W. Mater Sci Eng, 2007; A443: 142[5] Wright P K, Jain M, Cameron D. Superalloy 2004, TMS, 2004; 657[6] Antolovich B F, Saxena A, Antolovich S D. Superalloy 1992, TMS, 1992; 727[7] Zhang J H, Xu Y B, Wang Z G, Hu Z Q. Scr Mater, 1995; 32: 2093[8] Liu Y, Yu J J, Xu Y, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2007; A454–455: 357[9] Crompton J S, Martin JW. Metall Trans, 1984; 15A: 1711[10] Yang F M, Sun X F, Guan H R, Hu Z Q. Trans Nonferrous Met Soc China, 2003; 13: 141(杨福民, 孙晓峰, 管恒荣, 胡壮麒. 中国有色金属学报, 2003; 13: 141)[11] Ren W, Nicholas T. Mater Sci Eng, 2003; A357: 141[12] PilkeyWD. Peterson’s Stress Concentration Factors, New York: Wiley Interscience Publication, 1997: 1[13] Liu Y. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007(刘源. 中国科学院金属研究所博士学位论文, 沈阳, 2007)[14] Suresh S. translated by Wang Z G etc. Fatigue of Materials, Beijing: National Defense Industry Press, 1991: 131(Suresh S. 王中光等译. 材料的疲劳. 北京: 国防工业出版社. 1993: 131)[15] Zhang X. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006(张炫. 中国科学院金属研究所博士学位论文, 沈阳, 2006)[16] Ren W, Nicholas T. Mater Sci Eng, 2002; A332: 236[17] Luk´aˇs P, Kunz L, Svoboda M. Z Metall, 2002; 93: 661[18] Liu E Z, Zheng Z, Tong J, Ning L K, Guan X R. Acta Metall Sin, 2010; 46: 708(刘恩泽, 郑 志, 佟健, 宁礼奎, 管秀荣. 金属学报, 2010; 46: 708)[19] Zhu X, Shyam A, Jones JW, Mayer H, Lasecki J V, Allison J E. Int J Fatigue, 2006; 28: 1566 |
|