Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) 合金的微观组织与磁致伸缩性能 |
李晓诚1), 丁雨田1, 2), 胡勇1, 2) |
1) 兰州理工大学甘肃省有色金属新材料省部共建国家重点实验室, 兰州 730050
2) 兰州理工大学温州泵阀工程研究院, 温州 325105 |
|
MICROSTRUCTURE AND MAGNETOSTRICTION OF THE Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) ALLOYS |
LI Xiaocheng1), DING Yutian1, 2), HU Yong1, 2) |
1) State Key Laboratory of Gansu Advanced Nonferrous Metal Materials, Lanzhou University of Technology, Lanzhou 730050
2) Wenzhou Pump $\&$ Valve Engineering Research Institute, Lanzhou University of Technology, Wenzhou 325105 |
引用本文:
李晓诚 丁雨田 胡勇. Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) 合金的微观组织与磁致伸缩性能[J]. 金属学报, 2012, 48(1): 11-15.
,
,
.
MICROSTRUCTURE AND MAGNETOSTRICTION OF THE Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) ALLOYS[J]. Acta Metall Sin, 2012, 48(1): 11-15.
[1] Clark A E. Ferromagnetic Materials. Vol.1 Amsterdam: North–Holland, 1980: 531[2] Clark A E, Abbundi R, Gilmor W R. IEEE Trans Magn, 1978; 14: 542[3] Clark A E, Teter J P, McMasters O D. J Appl Phys, 1988; 63: 3910[4] Branwood A, Janio A L, Pierey A R. J Appl Phys, 1987; 61: 3796[5] Teter J P, Clark A E, McMasters O D. J Appl Phys, 1987; 61: 3787[6] Jiles D C. Acta Mater, 2003; 51: 5907[7] Greenough R D, Shulze M P, Jenner A G I, Wilkinson A J. IEEE Trans Magn, 1991; 27: 5346[8] Jiles D C. J Appl Phys, 1994; 27: 1[9] Zhang T L, Jiang C B, Zhang H, Xu H B. Smart Mater Struct, 2004; 13: 473[10] Zhang M C, Gao X X, Zhou S Z, Shi Z H. J Alloys Compd, 2004; 381: 226[11] Clark A E, Wun–Fogle M, Restorff J B, Lograsso T A, Cullen J R. IEEE Trans Magn, 2001; 37: 2678[12] Ma T Y, Jiang C B, Xiao F, Xu H B. J Alloys Compd, 2006; 414: 276[13] Liu H Y, Li Y X, Meng F B. J Alloys Compd, 2006; 408: 133[14] Palit M, Pandian S, Balamuralikrishnan R, Singh A K, Das N, Chandrasekaran V, Markandeyulu G. J Appl Phys, 2006; 100: 074913[15] Clark A E, Teter J P, Wun–Fogle M. J Appl Phys, 1991; 69: 5771[16] Teter J P, Clark A E, Wun–Fogle M. IEEE Trans Magn, 1990; 26: 1748[17] Zhou S Z, Gao X X, Zhang M C, Zhao Q, Shi Z H. J Mater Sci Technol, 2000; 16: 175[18] Zhao Y, Jiang C B, Zhang H, Xu H B. J Alloys Compd, 2003; 354: 263[19] Li K S, Xu J, Yang H C, Yuan Y Q, Yu D B, Ying Q M, Zhang S G. J Alloys Compd, 2004; 43: 8032[20] Wang B W, Wu C H, Chuang Y C, Jin X M, Li J Y. J Alloys Compd, 1996; 237: 58[21] Shi Y G, Tang S L, Yu J Y, Zhai L, Zhang X K, Du YW, Yang C P. J Appl Phys, 2009; 105: 07A925[22] Pandian S, Chandrasekaran V, Markandeyulu G, Iyer K J L, Rama Rao K V S. J Appl Phys, 2002; 92: 6082[23] Wang BW, Wu C H, Deng W, Tang S L, Jin X M, Chuang Y C, Li J Y. J Appl Phys, 1996; 79: 2587[24] Guo H Q, Yang H Y, Shen B G, Yang L Y, Li R Q. J Alloys Compd, 1990; 190: 255[25] Cui Y, Jiang C B, Xu H B. Acta Metall Sin, 2011; 47: 214(崔 跃, 蒋成保, 徐惠彬. 金属学报, 2011; 47: 214)[26] Westwood P, Abell J S. J Appl Phys, 1990; 67: 998[27] Chelvane J A, Palit M, Basumatary H, Pandian S, Chandrasekaran V. Scr Mater, 2009; 61: 548[28] Mei W, Okane T, Umeda T. J Alloys Compd, 1997; 248: 132 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|