| 电工钢中黄铜织构行为及其对Goss织构的影响 |
| 颜孟奇, 钱浩, 杨平, 宋惠军, 邵媛媛, 毛卫民 |
| 北京科技大学材料学院, 北京 100083 |
|
| BEHAVIORS OF BRASS TEXTURE AND ITS INFLUENCE ON GOSS TEXTURE IN GRAIN ORIENTED ELECTRICAL STEELS |
| YAN Mengqi, QIAN Hao, YANG Ping, SONG Huijun, SHAO Yuanyuan, MAO Weimin |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
颜孟奇 钱浩 杨平 宋惠军 邵媛媛 毛卫民. 电工钢中黄铜织构行为及其对Goss织构的影响[J]. 金属学报, 2012, 48(1): 16-22.
,
,
,
,
,
.
BEHAVIORS OF BRASS TEXTURE AND ITS INFLUENCE ON GOSS TEXTURE IN GRAIN ORIENTED ELECTRICAL STEELS[J]. Acta Metall Sin, 2012, 48(1): 16-22.
| [1] Hu H. Acta Metall, 1960; 8: 124[2] Hu H. Trans Metall Soc AIME, 1961; 211: 130[3] Ushioda K, Hutchinson W B. ISIJ Int, 1989; 29: 862[4] Bottcher A, Lucke K. Acta Metall Mater, 1993; 41: 2503[5] Inokuti Y, Maeda C, Tanaka T. J JIM, 1985; 49: 417[6] Inokuti Y, Maeda C, Ito Y. Trans ISIJ, 1987; 27: 303[7] May J, Turnbull D. Trans Metall Soc AIME, 1958; 212: 769[8] Misha S, Darmann C, Lucke K. Metall Mater Trans, 1986; 17A: 1301[9] Shimizu R, Harase J. Acta Metall, 1989; 37: 1241[10] Harase J, Shimizu R, Takashima K. J JIM, 1988; 52: 259[11] Harase J, Shimizu R. Trans JIM, 1988; 29: 388[12] Shimizu R, Harase J. J JIM, 1989; 53: 571[13] Hayakawa Y, Szpunar J. Acta Mater, 1997; 45: 1285[14] Rajmohan N, Szpunar J, Hayakawa Y. Mater Sci Eng, 1999; A259: 8[15] Hayakawa Y, Kurosawa M. Acta Mater, 2002; 50: 4527[16] Homma H, Hutchinson B. Acta Mater, 2003; 51: 3795[17] Homma H, Hutchinson B, Kubota T. J Magn Magn Mater, 2003; 254–255: 331[18] Ko K J, Cha P R, Srolovitz D, Hwang N M. Acta Mater, 2009; 57: 838[19] Inagaki H, Suda T. Texture, 1972; 1: 129[20] Yoshitomi Y, Ushigami Y, Harase J, Nakayama T, Masui H, Takahashi N. Acta Metall Mater, 1994; 42: 2593[21] Takamaya T, Kurosawa M, Komatubara M. J Magn Magn Mater, 2003; 254–255: 334[22] Pospiech J, Jura J. Metallkunde Z, 1974; 65: 324[23] Cui F E, Yang P, Mao W M. Trans Mater Heat Treat, 2011; 32: 38(崔凤娥, 杨平, 毛卫民. 材料热处理学报, 2011; 32: 38)[24] Harase J, Shimizu R. J Magn Magn Mater, 2000; 215–216: 89[25] Yan M Q, Qian H, Yang P, Mao W M, Jiang Q W, Jin W X. J Mater Sci Technol, 2011; 27: 1065 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|