| Zr-4合金腐蚀初期氧化膜的显微组织研究 |
| 杜晨曦1), 彭剑超2), 李慧1), 周邦新1) |
1) 上海大学材料研究所, 上海 200072
2) 上海大学微结构重点实验室, 上海 200444 |
|
| INVESTIGATION OF MICROSTRUCTURE OF OXIDE LAYERS FORMED INITIALLY ON Zr-4 ALLOY |
| DU Chenxi1), PENG Jianchao2), LI Hui1), ZHOU Bangxin1) |
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Laboratory for Microstructures, Shanghai University, Shanghai 200444 |
引用本文:
杜晨曦 彭剑超 李慧 周邦新. Zr-4合金腐蚀初期氧化膜的显微组织研究[J]. 金属学报, 2011, 47(7): 887-892.
,
,
,
.
INVESTIGATION OF MICROSTRUCTURE OF OXIDE LAYERS FORMED INITIALLY ON Zr-4 ALLOY[J]. Acta Metall Sin, 2011, 47(7): 887-892.
| [1] Zhou B X, Peng J C, Yao M Y, Li Q, Xia S, Du C X, Xu G. J ASTM Int, 8(1), DOI: 10.1520/JAI 102951[2] Ploc R A. J Nucl Mater, 1982; 110: 59[3] Ploc R A. J Nucl Mater, 1983; 115: 110[4] Ploc R A. J Nucl Mater, 1983; 113: 75[5] Wadman B, Andren H O, Falk L K L. Colloque De Physique, 1989; C8: 303[6] Wadman B, Andren H O. Zirconium in the Nuclear Industry: 9th International Symposium, ASTM STP 1132, West Conshohocken PA: ASTM International, 1991: 461[7] Kim H G, Kim T H, Jeong Y H. J Nucl Mater, 2002; 306: 44[8] Bakradze G, Jeurgens P H, Mittemeijer J. Surf Interface Anal, 2010; 42: 588[9] Charquet D, Tricot R, Wadier J F. Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, West Conshohocken PA: ASTM International, 1989: 374[10] Li B, Allnatt A R, Zhang C S, Norton P R. Surf Sci, 1995; 330: 2[11] Li C, Zhou B X. Nucl Power Eng, 1994; 15: 152(李 聪, 周邦新. 核动力工程, 1994; 15: 152)[12] Peachey L D. J Biophysic Biohem Cytol, 1958; 4: 233[13] Pemsler J P. J Electrochem Soc, 1958; 105: 315[14] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009(周邦新, 李 强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)[15] Ploc R A. J Nucl Mater, 1968; 28: 48[16] Zhou B X, Li Q, YaoMY, Liu WQ, Chu Y L. Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505, West Conshohocken PA: ASTM International, 2009: 360[17] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. Corros Prot, 2009; 30: 589(周邦新, 李强, 姚美意, 刘文庆, 褚于良. 腐蚀与防护, 2009; 30: 589)[18] Park J Y, KimH G, Jeong Y H, Jeong Y H. J NuclMater, 2004; 335: 433[19] Yilmazbayhan A, Motta A T, Comstock R J, Sabol G P, Lai B, Cai Z H. J Nucl Mater, 2004; 324: 6 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|