<001>和<011>取向DD407单晶高温合金枝晶间距和微观偏析 |
杨初斌,刘林,赵新宝,刘刚,张军,傅恒志 |
西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
DENDRITE ARM SPACINGS AND MICROSEGREGATIONS IN <001> AND <011> ORIENTATED SINGLE CRYSTAL SUPERALLOYS DD407 |
YANG Chubin, LIU Lin, ZHAO Xinbao, LIU Gang, ZHANG Jun, FU Hengzhi |
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
杨初斌 刘林 赵新宝 刘刚 张军 傅恒志. <001>和<011>取向DD407单晶高温合金枝晶间距和微观偏析[J]. 金属学报, 2011, 47(10): 1246-1250.
,
,
,
,
,
.
DENDRITE ARM SPACINGS AND MICROSEGREGATIONS IN <001> AND <011> ORIENTATED SINGLE CRYSTAL SUPERALLOYS DD407[J]. Acta Metall Sin, 2011, 47(10): 1246-1250.
[1] Huang Q Y, Li H K. Superalloys. Beijing: Metallurgical Industry Press, 2004: 2(黄乾尧, 李汉康. 高温合金. 北京: 冶金工业出版社, 2004: 2)[2] Hu ZQ, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31(3): 1(胡壮麒, 刘丽荣, 金 涛, 孙晓峰. 航空发动机, 2005; 31(3): 1)[3] Han G M, Yu J J, Sun Y L, Sun X F, Hu Z Q. Mater Sci Eng, 2010; A527: 5383[4] Zhang S H, Zhang J, Lou L H. J Mater Sci Technol, 2011; 27: 107[5] Ding G L, Tewari S N. J Cryst Growth, 2002; 236: 420[6] Zhao X B, Liu L, Yu Z H, Zhang W G, Fu H Z. Mater Charact, 2010; 61: 7[7] He G, Li J G, Mao X M, Fu H Z. Acta Metall Sin, 1995; 31: 469(何国, 李建国, 毛协民, 傅恒志. 金属学报, 1995; 31: 469)[8] Gandin C A, Eshelman M, Trivedi R. Metall Mater Trans, 1996; 27A: 2727[9] Grugel R N, Zhou Y. Metall Trans, 1989; 20A: 969[10] Huang T W, Liu L, Zhang W G, Zhang J, Fu H Z. Acta Metall Sin, 2009; 45: 1225(黄太文, 刘林, 张卫国, 张军, 傅恒志. 金属学报, 2009; 45: 1225)[11] Polock T M, Murphy W H, Goldman E H, Uram D L, Tu J S. In: Antolovich S D, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale: TMS, 1992: 125[12] Ma D X, Grafe U. Mater Sci Eng, 1999; A270: 339[13] Kearsey R M, Beddoes J C, Jaansalu K M, Thompson W T, Au P. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale: TMS, 2004: 801[14] Karunaratne M S A, Cox D C, Carter P, Reed R C. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S L, Schirra J J eds., Superalloys 2000, Warrendale: TMS, 2000: 263[15] Seo S M, Lee J H, Yoo Y S, Jo C Y, Miyahara H, Ogi K. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S R eds., Superalloys 2008, Warrendale: TMS, 2008: 277[16] Zhao X B, Liu L, Zhang W G, Liu G, Zhang J, Fu H Z. Mater Lett, 2009; 63: 2635[17] Hunt J D. Solidification and Casting of Metals. London: The Metals Society, 1979: 3[18] Kurz W, Fisher D J. Acta Metall, 1981; 29: 11[19] Trivedi R. Metall Trans, 1984; 15A: 977[20] Han S H, Trivedi R. Acta Metall Mater, 1994; 1: 25[21] An G Y, Liu L X. J Cryst Growth, 1987; 80: 383[22] Zhao X B. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2010(赵新宝. 西北工业大学博士学位论文, 西安, 2010)[23] Till W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428[24] Schneider M C, Gu J P, Beckermann C, Boettinger W J, Kattner U R. Metall Mater Trans, 1997; 28A: 1517[25] Ma D, Sahm P R. Giesserei–Forschung, 1990; 82: 869[26] Basaran M. Metall Trans, 1981; 12A: 1235[27] Gu L Y, Liu Z Y, Shi Z X. Trans Nonferrous Met Soc China, 1996; 6: 110(顾林喻, 刘忠元, 史正兴. 中国有色金属学报, 1996; 6: 110)[28] Karunaratne M S A, Carter P, Reed R C. Mater Sci Eng, 2000; 281A: 229[29] Zhao N R, Wang Z H, Li J G, Jin T, Sun X F, Yang H C, Hu Z Q. J Mater Eng, 2008; 2: 58(赵乃仁, 王志辉, 李金国, 金涛, 孙晓峰, 杨洪才, 胡壮麒. 材料工程, 2008; 2: 58) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|