| 用可变长度热源模拟奥氏体不锈钢多层焊对接接头的焊接残余应力 |
| 邓德安1;清岛祥一2 |
1.重庆大学材料科学与工程学院; 重庆 400045
2.计算力学研究中心技术开发部; 东京 142--0041; 日本 |
|
| NUMERICAL SIMULATION OF WELDING RESIDUAL STRESSES IN A MULTI–PASS BUTT–WELDED JOINT OF AUSTENITIC STAINLESS STEEL USING VARIABLE LENGTH HEAT SOURCE |
| DENG De’an1;KIYOSHIMA Shoichi2 |
1.College of Materials Science & Engineering; Chongqing University; Chongqing 400045
2.Department of Technical Development; Research Center of Computational Mechanics; Inc.; Tokyo 142–0041; Japan |
引用本文:
邓德安 清岛祥一. 用可变长度热源模拟奥氏体不锈钢多层焊对接接头的焊接残余应力[J]. 金属学报, 2010, 46(2): 195-200.
,
.
NUMERICAL SIMULATION OF WELDING RESIDUAL STRESSES IN A MULTI–PASS BUTT–WELDED JOINT OF AUSTENITIC STAINLESS STEEL USING VARIABLE LENGTH HEAT SOURCE[J]. Acta Metall Sin, 2010, 46(2): 195-200.
| [1] Deng D, Murakawa H, Liang W. Comput Mater Sci, 2008; 42: 234
[2] Ogawa K, Deng D, Kiyoshima S, Yanagida N, Saito K. Comput Mater Sci, 2009; 45: 1031
[3] Hamada I, Yamauchi K. Nucl Eng Des, 2002; 214: 205
[4] KoshiishiM, Fujimori H, Okada M, Hirano A. Hitachi Rev, 2009; 58: 88
[5] Ueda Y, Yamakawa T. JWRI Trans, 1971; 2: 90
[6] Deng D, Murakawa H. Comput Mater Sci, 2008; 43: 681
[7] Deng D. Mater Des, 2009; 30: 359
[8] Deng D. PhD Thesis, Osaka University, 2002
[9] Hong J K, Tsai C L, Dong P. Weld J, 1998; 77: 372s
[10] Nishigawa H, Serizawa H, Murakawa H. Sci Technol Weld Join, 2007; 12: 147
[11] Ogawa K, Yanagida N, Saito K. Proc PVP2008, 2008 ASME Pressure Vessels and Piping Division Conference, July 27–31, 2008, Chicago, Illinois, USA, PVP2008–61321, CD–ROM
[12] Kiyoshima S, Deng D, Ogawa K, Yanagida N, Satio K. Comput Mater Sci, 2009; 46: 987
[13] Kiyoshima S. Quick Welder User’s Manual. Research Center of Computational Mechanics Inc., Tokyo, 2005: 23
(清岛祥一. Quick Welderユ一ザマニュアル. 计算力学研究センタ一, 东京, 2005: 23)
[14] Deng D, Murakawa H. Comput Mater Sci, 2006; 37: 269
[15] Terasaki T, Kitamura T, Akiyama T, Nakatani M. Sci Tech Weld Join, 2005; 10: 701
[16] Deng D, Murakwa H. Comput Mater Sci, 2006; 37: 209
[17] Leggatt R H. Int J Press Vessels Piping, 2008; 85: 144 |
|