| NiTi形状记忆薄膜的力学性能 |
| 宫峰飞;沈惠敏;王业宁;姜恩永 |
| 天津大学应用物理系;天津;300072;南京大学固体微结构国家重点实验室;南京;210008;南京大学固体微结构国家重点实验室;南京;210008;南京大学固体微结构国家重点实验室;南京;210008;天津大学应用物理系;天津;300072 |
|
| MECHANICAL PROPERTIES OF NiTi SHAPE MEMORY THIN FILMS |
| GONG Fengfei;SHEN Huimin;WANG Yening;JIANG Enyong (Department of Applied Physics; Tianjin University; Tianjin 300072)(National Laboratory of Solid State Microotructures; Nanjing University) Nanjing 210008) |
引用本文:
宫峰飞;沈惠敏;王业宁;姜恩永. NiTi形状记忆薄膜的力学性能[J]. 金属学报, 1998, 34(2): 119-122.
,
,
,
.
MECHANICAL PROPERTIES OF NiTi SHAPE MEMORY THIN FILMS[J]. Acta Metall Sin, 1998, 34(2): 119-122.
1Johnson A D.J Micromech Microeng, 1991; 1: 39 2Ray C R. Mater Res Soc Symp, Proc, 1992; 276: 161 3Bruno O P, Leo P H, Reitich F. Phys Rev Lett, 1995; 74: 746 4金嘉陵.金属学报, 1984; 20: A176 (Jin J L.Acta Metall Sin,1984; 20:A176) 5张一,金嘉陵.金属学报,19852 21:A365 (Zhang Y, Jin J L. Acta Metall Sin, 1985; 21: A365) 6张一,金嘉陵金属学报,1987;23:A280 (Zhan Y,Jin J L.Acta Metall Sin,1987;23:A280) 7金嘉陵,王宏亮.金属学报,1988;24:A66 (Jin J L, Wang H L. Acta Metall Sci, 1988; 24: A66)+ |
|