| 液淬工艺和微量元素对非晶态Fe—B—Si合金热稳定性的影响 |
| 车晓舟;朱敏;李祖鑫;戴礼智 |
| 华南理工大学机电工程系;广州;510641;华南理工大学机电工程系;广州;510641;华南理工大学机电工程系;广州;510641;钢铁研究总院;北京;100081 |
|
| INFLUENCE OF QUENCHING CONDITIONS AND MICRO-ADDITION OF CERIUM ON THERMAL STABILITY OF AMORPHOUS Fe-B-Si ALLOYS |
| CHE Xiaozhou; ZHU Min; LI Zuxin(Department of Mechano-Electronic Engineering; South China University of Technology; Guangzhou 510641)DAI Lizhi(Central Iron and Steel Research Institute; Beijing 100081)Correspondent: CHE Xiaozhou;associate professor;Tel: (020)87111317 |
引用本文:
车晓舟;朱敏;李祖鑫;戴礼智. 液淬工艺和微量元素对非晶态Fe—B—Si合金热稳定性的影响[J]. 金属学报, 1998, 34(10): 1028-1032.
,
,
,
.
INFLUENCE OF QUENCHING CONDITIONS AND MICRO-ADDITION OF CERIUM ON THERMAL STABILITY OF AMORPHOUS Fe-B-Si ALLOYS[J]. Acta Metall Sin, 1998, 34(10): 1028-1032.
1车晓舟.金属学报, 1995; 31: B418(Che X Z. Acta Metall Sin, 1995; 31: B418) 2姚斌,华中,闵春宗,王爱民,刘浩哲,丁炳哲,胡壮麟.金属学报,1996;32:867(Yao B, Hua Z, Min C Z, Wang A M, Liu H Z, Ding B Z, Hu Z Q. Acta Metall Sin, 1996; 32: 867) 3沈德久,王玉林,沈中毅,殷岫君.金属学报,1997;33:621(Shen D J, Wang Y L, Shen Z Y, Yin X J. Acta Metall Sin, 1997; 33: 621) 4晁月盛,滕功清,谢春辉,耿岩,赖祖涵.金属学报.1996;32: 1204(Chao Y S,Teng G Q,Xie C H,Geng Y,Lai Z H. Acta Metall Sin,1996; 32:1204) 5Luborsky P E, Walter J L.J Appl Phgs, 1976 47: 3648 6Gerling R,Schimansky F P,Wagner R.Int J Rapid Solidif,1990; 5:137 7Chen H S. J Appl Phys, 1978; 49: 3289 8KroegerD M,Canright G S,MaKamey CG,Easton D S,Scarbrough J O.Acta Metall,1987;35:989 9Liebermann H H, Marti J, Martis R J, Wong C P. Metall Trans, 1989; 20A: 63i |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|