Al-20Mg合金高压凝固力学性能研究* |
接金川1,2, 邹鹑鸣1, 王宏伟1, 魏尊杰1( ) |
1 哈尔滨工业大学材料科学与工程学院金属精密热加工国家级重点实验室, 哈尔滨 115110 2 大连理工大学材料科学与工程学院, 大连 116024 |
|
MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE |
JIE Jinchuan1,2, ZOU Chunming1, WANG Hongwei1, WEI Zunjie1( ) |
1 National Key Laboratory of Metal Precision Hot Forming, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 115110 2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
接金川, 邹鹑鸣, 王宏伟, 魏尊杰. Al-20Mg合金高压凝固力学性能研究*[J]. 金属学报, 2014, 50(8): 971-978.
Jinchuan JIE,
Chunming ZOU,
Hongwei WANG,
Zunjie WEI.
MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE[J]. Acta Metall Sin, 2014, 50(8): 971-978.
[1] |
Mcmillan P F. Nat Mater, 2002; 1: 19
|
[2] |
Sharma S M, Sikka S K. Prog Mater Sci, 1996; 40: 1
|
[3] |
Zaug J M, Soper A K, Clark S M. Nat Mater, 2008; 7: 890
|
[4] |
Liao S C, Mayo W E, Pae K D. Acta Mater, 1997; 45: 4027
|
[5] |
Wei Z J, Wang Z L,Wang H W, Cao L. J Mater Sci, 2007; 42: 7123
|
[6] |
He D W, He M, Kiminami C S, Kuo K H, Zhang F X, Xu Y F, Wang W K. J Mater Res, 2001; 16: 910
|
[7] |
Zhang G Z, Yu X F, Wang X Y, Jia G L, Gao Y Y, Hao Z Y, Guo X B. Acta Metall Sin, 1999; 35: 285
|
[7] |
(张国志, 于溪凤, 王向阳, 贾光霖, 高允彦, 郝兆印, 郭学彬. 金属学报, 1999; 35: 285)
|
[8] |
Zhang J, Zhang H F, Dong P, Quan M X, Hu Z Q. Acta Metall Sin, 2004; 40: 211
|
[8] |
(张 甲, 张海峰, 董 盼, 全明秀, 胡壮麒. 金属学报, 2004; 40: 211)
|
[9] |
Canadinc D, Maier H J, Gabor P, May J. Mater Sci Eng, 2008; A496: 114
|
[10] |
Cui G R, Ma Z Y, Li S X. Scr Mater, 2008; 58: 1082
|
[11] |
Jie J C, Zou C M, Wang H W, Wei Z J. Mater Lett, 2010; 64: 869
|
[12] |
Jie J C, Zou C M, Brosh E, Wang H W, Wei Z J, Li T J. J Alloys Compd, 2013; 578: 394
|
[13] |
Starink M J, Zahra A M. Acta Mater, 1998; 46: 3381
|
[14] |
Zhang D L, Massalski T B, Paruchuri M R. Metall Mater Trans, 1994; 25A: 73
|
[15] |
Schoenitz M, Dreizin E L. J Mater Res, 2003; 18: 1827
|
[16] |
Scudino S, Sperling S, Sakaliyska M, Thomas C, Feuerbacher M, Kim K B, Ehrenberg H, Eckert J. Acta Mater, 2008; 56: 1136
|
[17] |
Scudino S, Sakaliyska M, Surreddi K B, Eckert J. J Alloys Compd, 2009; 483: 2
|
[18] |
Mourik P V, Maaswinkel N M, Keijser T H D, Mittemeijer E J. J Mater Sci, 1989; 24: 3779
|
[19] |
Vacher P, Boudrahem S. Acta Mater, 2006; 54: 4365
|
[20] |
Hall E O. Proceedings Phys Soc London, 1951; 64B: 747
|
[21] |
Petch N J. J Iron Steel Inst, 1953; 174: 25
|
[22] |
Mukai T, Higashi K, Tanimura S. Mater Sci Eng, 1994; A176: 181
|
[23] |
Chen X, Yan J, Karlsson A. Mater Sci Eng, 2006; A416: 139
|
[24] |
Deng D. Mater Des, 2009; 30: 359
|
[25] |
Lados D A, Apelian D, Wang L. Mater Sci Eng, 2010; A527: 3159
|
[26] |
Wang T G, Zhao S S, Hua W G, Li J B, Gong J, Sun C. Mater Sci Eng, 2010; A527: 454
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|