| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF SPRAY DEPOSITED Al-Si-Fe-Cu-Mg ALLOY |
| YUAN Xiaoguang; XU Daming; ZHANG Shuying; LI Qingchum (Harbin Institute of Technology; Harbin 150001) |
|
Cite this article:
YUAN Xiaoguang; XU Daming; ZHANG Shuying; LI Qingchum (Harbin Institute of Technology; Harbin 150001). MICROSTRUCTURE AND MECHANICAL PROPERTIES OF SPRAY DEPOSITED Al-Si-Fe-Cu-Mg ALLOY. Acta Metall Sin, 1997, 33(3): 248-252.
|
|
|
Abstract Al-Si-Fe-Cu-Ma alloy has been produced with spray deposition technology.The microstructures of the alloys under spray deposited, extruted and T6 heat treated conditions have been investigated. The mechanical properties at room temperature and 200° have been measured. The strenghening and fracture mechanisms of the alloy have been put forward.
|
|
Received: 18 March 1997
|
1 Sumitomo Light Metal Industrles Ltd. Japan. Metal Powder Rep,1994. 49(1); 26 2 Sumitomo Electric Industries of Osaka. Japan. Metal Powder Rep. 1994: 49(4): 36 3 Oiha S N, Jha J N. Singh S N. Scr,Metall Mater, 1991, 25: 443 4 Fabietti L M. Sekhar J A. Metall Trans.1992; 26A : 3361 5 Zhou J, Duszczyk J, Korevaar B M. J Mater Sci, 1989. 25: 824 6 Zhou J. Duszczyk J, Korevaar B M. J Mater Sci. 1991. 26: 3041 7 Hayashi T, Takeda Y. Akechi K, Fujiwara T. Metal Powder Rep,1991 : 46(2): 23 8 Maellin A, Brechet Y, Fougeres R. Acta Metall Mater, 1995; 43: 1135m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|