TEM OBSERVATION OF THE FINE STRUCTURE OF BAINITE
LI Fengzhao; AO Qing; GU Yingni; JIANG Jiang; SUN Dongsheng (Shandong University of Technology; Jinan 250061)DAI Jiyan; PENG Hongying (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

LI Fengzhao; AO Qing; GU Yingni; JIANG Jiang; SUN Dongsheng (Shandong University of Technology; Jinan 250061)DAI Jiyan; PENG Hongying (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). TEM OBSERVATION OF THE FINE STRUCTURE OF BAINITE. Acta Metall Sin, 1997, 33(3): 241-247.

Download:  PDF(3739KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fine structure of bainite, morphology and distribution of carbide in steels and morphology of bainite in Cu-Zn-Al alloy have been investigated with TEM. Interfacial structure ledges and interfacial lattice images of Cu-Zn-Al alloy have also been observed with HREM. Addition of minor alloying elements can fine the structure of bainitic ferrite markedly. The bainitic ferrite is composed of subunits or subchunks. The carbides with different morphologies are distributed between the laths. inside the plates and at the boundaries of subunits. There are abundant fine structures in bainitic ferrite. In the primary bainite of Cu-Zn-Al alloy there are interfacial structure ledges. whose heights are within 3-40 nm.corresponding to 15-200 atomic layers. The phase reaction mechanism of bainite is discussed in this article.
Key words:  bainitic ferrite      fine structure      subunit      interfacial structure ledge     
Received:  18 March 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I3/241

1Bhadeshia H K D H, Christian J W. Metall Trans.1990;21A:767
2 RCynolds W T Jr,Li F Z, Shui C K,Aaronson H I. Metall Trans,1990;21A:1443
3 Bhadeshia H K D H Bainite in Steels. London:The Institute of Materials, 1992: 348, 380
4 Bramfitt B L,Speer J G .Metall Trans,1990;21A:817
5康沫狂,杨思品,管敦惠.钢中贝氏体上海:上海科学技术出版社、1990:381
6方鸿生,郑燕康,陈秀云,黄云庆,曹建军,姜忠良中国机械工程学会第二届材料年会论文集,中国机械工程学会材料学会、1990:115
7 Oblack J M, Hehamann R F.Trans formation and Hardenability in Steels,Ann Arbor,MI:ClimaxMolybdenum Company,1967:15
8俞德刚,朱钰如,陈大军,唐晓宏、张惠娟金属学报,1994;30:A385
9王家军,方鸿生,郑燕康,严隽珏.兵器材料科学与工程,1993;16:3
10Spanos G. Metall Mater Trans,1994:25A:1967
11 Fang H S,Wang J J,Zheng Y K,Metall Mater Trans,1994:25A:2001
12 Aaronson H I, Hall M G Metall Mater Trans,1994:25A:1797
[1] WANG Xixia, GUO Hui, WANG Ding, BAI Yin, YANG Shanwu, HE Xinlai. INFLUENCE OF COHERENT AUSTENITE TWIN BOUNDARIES ON THE VARIANT SELECTION OF BAINITIC FERRITE IN Fe-C-Mn-Si STEELS[J]. 金属学报, 2012, 48(4): 385-392.
[2] ZHANG Weihu ZHANG Fuchun ZHANG Zhiyong YAN Junfeng . FIRST–PRINCIPLE ANALYSYS ON FINE STRUCTURE OF Pb0.5Sr0.5TiO3[J]. 金属学报, 2009, 45(2): 217-222.
[3] DONG Dan-Yang; Changsheng LIU. INVESTIGATION OF HYPERFINE STRUCTURE OF LASER CLADDING Fe-Si COATING[J]. 金属学报, 2008, 44(2): 188-192 .
[4] . Refinement of Grain and Enhancement of Impact Energy Absorption for Low-Alloy Ultra-High Strength Bainite Steels Containing Silicon[J]. 金属学报, 2007, 43(3): 315-320 .
[5] BO Xiangzheng; FANG Hongsheng; WANG Jinjun; HUANG Weigang; ZHANG Boqing (Department of Materials Science and Engineering; Tsinghua University; Beijing 100084). INVESTIGATION OF THE ULTRA-FINE STRUCTURE OF SURFACE RELIEF EFFECTS ASSOCIATED WITH BAINITE IN AN Fe-C-Si-Mn ALLOY[J]. 金属学报, 1998, 34(3): 225-231.
[6] LUO Chengping(C.P.Luo);LIU Jiangwen;XIAO Xiaoling(Department of Mechanical Engineering; South China University of Technology; Guangzhou 510641)Correspondent:LUO Chengping; professor; Tel:(020)85511617; Fax: (020)87111312;E-mail: mecpluo@letterbox.scut.edu.cn. FINE STRUCTURE AND CRYSTALLOGRAPHY OF ISOTHERMAL LOWER BAINITE IN AN EXPERIMENTAL STEEL 38Si2Mn2Mo[J]. 金属学报, 1998, 34(10): 1009-1015.
[7] FANG Hongsheng; YANG Zhigang; WANG Jiajun; ZHENG Yankang(Tsinghua University; Beijing 100084)(Manuscript received 1995-11-10). RESEARCH ASPECTS OF TRANSFORMATION AND APPLICATION OF BAINITE AND MARTENSITE[J]. 金属学报, 1996, 32(4): 337-350.
[8] LI Chunming; FANG Hongsheng; ZHENG Yankang; WANG Jiajun; YANG Zhigang (Tsinghua University; Beijing 100084)(Manuscript received 1995-04-03; in revised form 1995-07-07). SUBUNITS AND THEIR SYMPATHETIC NUCLEATION-LEDGEWISE GROWTH OF BAINITE IN A Cu-Zn-Al ALLOY[J]. 金属学报, 1996, 32(1): 1-5.
[9] YANG Liu; ZHU Degui; ZHANG Jun; CHEN Jian (Southwestern Jiaotong University; Chengdu). IN SITU OBSERVATION OF GROWTH OF BAINITE IN Fe-Ni ALLOY[J]. 金属学报, 1994, 30(8): 344-347.
[10] LI Douxing; PING Dehai; NING Xiaoguang; YE Hengqiang (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; Shenyang). FINE STRUCTURE OF BOTH INTERFACES AND INTERFACIAL REACTION PRODUCTS[J]. 金属学报, 1992, 28(7): 1-18.
[11] TENG Feng'en;WANG Yuming;XU Yue Jilin University; Chang chun. FINE STRUCTURE ANALYSIS OF DEFORMED AUSTENITE STAINLESS STEEL 1Cr18Ni9[J]. 金属学报, 1992, 28(1): 45-47.
[12] JIN Qiang;FANG Hongsheng;CAO Jianjun;ZHENG Yankang;CHEN Xiuyun Tsinghua University; Beijing. LEDGE STRUCTURE AT BROAD FACES OF FERRITE PLATES IN LOWER BAINITE[J]. 金属学报, 1990, 26(6): 5-9.
[13] ZHU Min;LI Cuobin YANG Dazhi Dalian University of Technology Department of Materials Engineering; Dailian University of Technology; Dailian 116024. FINE STRUCTURE VARIATION OF POLYCRYSTALLINE Cu-Zn-Al SHAPE MEMORY ALLOY UNDER MARTENSITE DEFORMATION[J]. 金属学报, 1990, 26(1): 72-75.
No Suggested Reading articles found!