| SPECIFIC CONDUCTIVITY OF MODIFIED Al-Si-Mg ALLOYS |
| LIAO Shijie (Xiangtan University; Xiangtan 411105)ZHANG Xinming (Central South University of Technology; Chanasha 410083) |
|
Cite this article:
LIAO Shijie (Xiangtan University; Xiangtan 411105)ZHANG Xinming (Central South University of Technology; Chanasha 410083). SPECIFIC CONDUCTIVITY OF MODIFIED Al-Si-Mg ALLOYS. Acta Metall Sin, 1997, 33(3): 253-258.
|
|
|
Abstract In order to investigate the modified effects the specific conductivities of Al-Si-Mg alloys added by Sb, Sr and RE elements were measured respectively. The results show that the specific conductivities of alloys modified by Sb and Sr have high values, while the specific conductivity of alloy modified by RE displays low values and that the farther the distances from the bottom of the ingots, the smaller the specific conductivities of the Sb or Sr modified alloys are. It is indicated that solid solution treatment at 535℃ increases the specific conductivity of the unmodified alloy, but decreases the values of the Sb or Sr modified alloy and the higher the specific conductivity, the higher the impact toughness of the ingots is.
|
|
Received: 18 March 1997
|
1Schaefer M,Fournelle R A.Metall Mater Trans,1996;27A:1293 2李培杰,贾均,李庆春, Xoceh P.材料科学与工艺, 1995; 3(1): 84 3曾松岩,张虎,李庆春材料工程,1993;(5): 13 4张启运,刘淑棋,樊晓红金属学报,1982;18:584 5张启运,刘淑祺,胡佳金属学报,1984;20:138 6徐京娟,邓志煜,张同俊.金属物理性能分析上海:上海科学技术出版社,1988:52= |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|