Abstract The corrosion-resistant ultrahigh strength steel AerMet100 was fabricated by the laser melting deposition manufacturing technology. The as-solidification microstructure and mechanical properties of the laser deposited steel were investigated. The laser as-deposited steel has a rapidly solidified “zig-zag” full cellular structure and excellent room-temperature mechanical properties. The solidification mechanism of the zig-zag full cellular structure during the laser melting deposition process was discussed and a physical model based on selective epitaxial cell growth was proposed for the formation of the zig-zag full cellular structure.
|
|
Received: 26 September 2006
|
|
|
[1] Novotny P M, Maguire M. Foundry Managem Technol, 1993; 121(12): 33 [2] Hemphill R M. Steel Times, 1995; 223(5): 191 [3] Dahl J M, Novotny P M. Adv Mater Processes, 1999; 155(3): 23 [4] Garrison W M. JOM, 1990; 42(5): 20 [5] Wang H M, Zhang L Y, Li A, Cai L X, Tang H B, Lu X D. World Sci-Technol R D, 2004; 26(3): 27 (王华明,张凌云,李安,蔡良续,汤海波,吕旭东.世界科技研究与发展,2004;26(3):27) [6] Wang H M, Zhang L Y, Li A, Cai L X, Tang H B. J Beijing Univ Aeronaut Astronaut, 2004; 30: 962 (王华明,张凌云,李安,蔡良续,汤海波.北京航空航天大学学报,2004;30:962) [7] Gaumann M, Henry S, Cleton F, Wagniere J D, Kurz W. Mater Sci Eng, 1999; A271: 232 [8] Abbott D H. Met Powder Rep, 1998; 53(2): 24 [9] Abbott D H, Arcella F G. Adv Mater Processes, 1998; 153(5): 29 [10] Chang C E, Wilcox W R. J Cryst Growth, 1974; 21: 35 [11] Yang S, Huang W D, Liu W J, Su Y P, Zhou Y H. Acta Metall Sin, 2001; 37: 571 (杨森,黄卫东,刘文今,苏云鹏,周尧和.金属学报,2001; 37:571) [12] Liu Z Y, Li J G, Fu H Z. Acta Metall Sin, 1995; 31: 329 (刘忠元,李建国,傅恒志.金属学报, 1995;31:329) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|