PREPARATION OF ALUMINIUM DOPED ZINC OXIDE FILMS AND THE STUDY OF THEIR MICROSTRUCTURE, ELECTRICAL AND OPTICAL PROPERTIES
HongMing Zhou;;
中南大学材料科学与工程学院
Cite this article:
HongMing Zhou. PREPARATION OF ALUMINIUM DOPED ZINC OXIDE FILMS AND THE STUDY OF THEIR MICROSTRUCTURE, ELECTRICAL AND OPTICAL PROPERTIES. Acta Metall Sin, 2006, 42(5): 505-510 .
Abstract Aluminium doped zinc oxide polycrystalline thin films (AZO) were prepared on microscope glass substrates by sol-gel dip-coating process. Zinc acetate solutions of 0.5 M in isopropanol stabilized by diethanolamine and doped with a concentrated solution of aluminium nitrate in ethanol were used. The quantity of aluminium in the sol was varied from 1 to 3 at. %, and the deposition times was varied from 5 to 15. Crystalline ZnO thin films were obtained following an annealing process at temperatures between 300℃ and 500℃ for 1 h. The coatings have been characterized by X-ray diffraction (XRD), optical spectroscopy (UV-Vis), scanning electron microscope (SEM), and electrical resistance measurement. With the annealing temperature increased from 300℃ to 500℃, the film was oriented more preferentially along the (0 0 2) direction, the grain size of the film increased, the transmittance also became higher and the electrical resistivity decreased. The X-ray diffraction analysis revealed single-phase ZnO hexagonal zincite structure. Optical transmittance over 90% in the near UV and VIS regions and electrical resistivity as low as 3.2×10-3 Ω·cm were obtained under such conditions, doping concentration 1 at. %, annealing temperature 500℃, deposition times 10.
[1] Nishino J, Kawarada T, Ohisho S, Saitoh H, Maruyama K, Kamata K. J Mater Sci Lett, 1997; 16: 629 [2] Ritala M, Asikanen T, LeskelaM, Skarp J. Mater Res Soc Symp Proc, 1996; 426: 513 [3] Wang R, King L L H, Sleight A W. J Mater Res, 1996; 11: 1659 [4] Gupta V, Mansingh A. J Appl Phys, 1996; 80: 1063 [5] Bertolotti M M, Laschena M V, Rossi M, Ferrari A, Qian L S, Quaranta F, Valentini A. J Mater Res, 1990; 5: 1929 [6] Schuler T, Aegerter M A. Thin Solid Films, 1999; 351: 125 [7] Hayamizu S, Tabata H, Tanaka H, Kawai T. J Appl Phys, 1996; 80: 787 [8] Anna Selvan J A, Keppner H, Shah A. Mater Res Soc Symp Proc, 1996; 426: 497 [9] Nakada T, Murakami N, Kunioka A. Mater Res Soc Symp Proc, 1996; 426: 411 [10] Szyszka B, Jager S. J Non-Cryst Solids, 1997; 218: 74 [11] Deschanvres J L, Bochu B, Joubert J C. J Phys, 1993; 3: 485 [12] Messaoudi C, Sayah D, Abd-Lefdil M. Phys Status Solidi, 1995; 151: 93 [13] Tokumoto M S, Smith A, Santilli C V, Pulcinelli S H, Elkaim E, Briois V. J Non-Cryst Solids, 2000; 273: 302 [14] Tokumoto M S, Smith A, Santilli C V, Pulcinelli S H, Craievich A F, Elkaim E, Traverse A, Briois V. Thin Solid Films, 2002; 416: 284 [15] Schuler T, Aegerter M A. Thin Solid Films, 1999; 351: 125 [16] Tokumoto M S, Pulcinelli S H, Santilli C V, Craievich A F. J Non-Cryst Solids, 1999; 247: 176 [17] Kamalasanan M N, Chandra S. Thin Solid Films, 1996; 288: 112 [18] Lee J H, Park B O. Thin Solid Films, 2003; 426: 94 [19] Jimenez G A E, Soto U J A. Sol Energy Mater Sol Cells, 1998; 52: 345 [20] Valle G G, Hammer P, Pulcinelli S H, Santilli C V. J Eur Ceram Soc, 2004; 24: 1009 [21] Silva R F, Zaniquelli M E D. J Non-Cryst Solids, 1999; 247: 248 [22] Ohyama M, Kozuka H, Yoko T. Thin Solid Films, 1997; 306: 78 [23] Talahashi Y, Kanamori M, Kondoh A, Minoura H, Ohya Y. Jpn J Appl Phys, 1994; 33: 6611 [24] Sernelius B E, Berggren K F, Jin Z C, Hamberg I, Granqvist C G. Phys Rev, 1998; 37: 10244 [25] Tang W, Cameron D C. Thin Solid Films, 1994; 238: 83 [26] Nanto H, Minami T, Shooji S, Takata S. J Appl Phys, 1984; 55: 1029 [27] Ohyama M, Kozuka H, Yoko T. J Ceram Soc Jpn, 1996; 104: 296 [28] Nunes P, Fortunato E, Tonello P, Braz F, Vilarinho P, Martins R. Vacuum, 2002; 64: 281 [29] Gray J. J Am Ceram Soc, 1954; 37: 534 [30] Sukkar M H, Tuller H L. Adv Ceram, 1984; 55: 71 [31] Ge C Q, Xia Z L, Guo A Y. Electron Components Mater, 2004; 23(9): 31 (葛春桥,夏志林,郭爱云.电子元件与材料,2004;23(9):31) [32] Tian M B, Liu D L. Manual of Membrane Science and Technology. Beijing: China Machine Press, 1991: 471 (田民波,刘德令.薄膜科学与技术手册,北京:机械工业出版 社,1991:471) [33] Major S, Banerjee A, Chopra K L. Thin Solid Films, 1984; 122: 31 [34] Meng Y, Lin J, Liu J, Shen J, Jiang Y M, Yang X L, Zhang Z J. Photoelectron Technol, 2001; 21: 89 (孟扬,林剑,刘键,沈杰,蒋益明,杨锡良,章壮健. 光电子技术,2001;21:89)