Abstract  ABSTRACT In this paper, the method using Solid Oxygen-Ion Membrane (SOM) to produce tantalum from tantalum oxide was investigated. Experiment was carried out at 1150℃ and 3.2V of DC electrolysis potential in the flux system of 55.5wt.%CaF2- 44.5wt.%MgF2. Sintered Ta2O5 solid and liquid copper saturated with carbon loaded in zirconia tube were used as the cathode and the anode, respectively. The results of scanning electron microscopy (SEM) with an energy dispersive X-ray spectrometer (EDX) indicated that the amount of oxygen in tantalum oxide decreased obviously even approached to the zero level and tantalum was produced.
Key words:  Tantalum      SOM      electrolysis      
Received:  30 August 2005     
ZTFLH:  TG146.4  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I5/500

[1] He J L. Chin J Rare Met, 2003; 27: 23 (何季麟.稀有金属,2003;27:23)
[2] He J L. Eng Sci, 2003; 5(5): 40 (何季麟.中国工程科学,2003;5(5):40)
[3] He J L, Zhang Z G, Xu Z T. Rare Met Mater Eng, 1998; 27: 9 (何季林,张宗国,徐忠亭.稀有金属材料与工程,1998;27: 9)
[4] He J L. Eng Sci, 2001; 3(12): 85 (何季麟.中国工程科学,2001;3(12):85)
[5] Lu X G, Zhou G Z, Ding W Z, Jang G C, Xu K D. J Iron Steel Res, 2003; 15(5): 69 (鲁雄刚,周国治,丁伟中,蒋国昌,徐匡迪.钢铁研究学报, 2003;15(5):69)
[6] Pal U. JOM, 2001; 53(10): 25
[7] Pal U, Woolley D E,Kenney G B. JOM, 2001; 53(10): 32
[8] Woolley D E, Pal U. JOM, 2001; 53(10): 40
[9] Krishnan A, Lu X G, Pal U. Mater Metall Trans, 2005; 36B: 463
[10] Chen G Z, Fray D J, Farthing T W. Nature, 2000; 407: 361
[1] Jialin ZHU,Shifeng LIU,Yu CAO,Yahui LIU,Chao DENG,Qing LIU. Effect of Cross Rolling Cycle on the Deformed and Recrystallized Gradient in High-Purity Tantalum Plate[J]. 金属学报, 2019, 55(8): 1019-1033.
[2] Jing GUO,Hanjie GUO,Keming FANG,Shengchao DUAN,Xiao SHI,Wensheng YANG. Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel[J]. 金属学报, 2017, 53(7): 789-796.
[3] Dewei ZHAO, Junlei LI. Fabrication of the Porous Tantalum and Its Current Status Used as Orthopedics Implants Materials[J]. 金属学报, 2017, 53(10): 1303-1310.
[4] ZHAO Bingjian LU Xionggang LI Chonghe ZHONG Qingdong. DIRECT ELECTROCHEMICAL REDUCTION OF NiO–CeO2 POWDER FOR PREPARATION OF CeNi5 ALLOY BY SOLID–OXYGEN–ION
CONDUCTING MEMBRANE PROCESS
[J]. 金属学报, 2009, 45(10): 1255-1260.
[5] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
[6] ZOU Fenglei; GAO Kewei; ZHU Qifang; XIEJianxin. The mesomechanical analysis of the deformation of copper with continuous columnar crystals[J]. 金属学报, 2008, 44(3): 297-301 .
[7] ;. EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD[J]. 金属学报, 2008, 44(10): 1243-1246 .
[8] . PREPARATION OF TANTALUM BY ELECTRO-DEOXIDATION IN A CACL2-NACL MELT[J]. 金属学报, 2006, 42(3): 285-289 .
[9] V.E.Panin(The Institute of Strength Physics and Materials Sciences; Russian Academy of Sciences;Siberian Branch; Tomsk; 634048; Russia). PHYSICAL FUNDAMENTALS OF MESOMECHANICS OF PLASTIC DEFORMATION AND FRACTURE OF SOLIDS[J]. 金属学报, 1997, 33(2): 187-197.
[10] ZHAO Qijin;LI RIhui;ZHAO Dehou(Beijing General Research Institute for Non-Ferrous Metals;Beijing 100088); WANG Luhong;WU Jun(Jinchuan Non-Ferrous Metals Company; Jinchang 737104). INDUSTRIAL APPLICATION OF THE TECHNOLOGY PRODUCING NICKEL FOIL BY ELECTROLYSIS[J]. 金属学报, 1997, 33(11): 1194-1198.
[11] LIU Guankun; TONG Yexiang;HONG Huichan; CHEN Shengyang;GAN Luo(Zhongshan University; Guangzhou 510275)(Manuscript received 1995-10-23; in revised form 1996-08-25). STUDIES ON THE PREPARATION OF Dy-Cu ALLOY IN CHLORIDE MELT BY MOLTEN SALT ELECTROLYSIS[J]. 金属学报, 1996, 32(12): 1252-1257.
No Suggested Reading articles found!