Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate |
DING Ning1, WANG Yunfeng2, LIU Ke1, ZHU Xunming2, LI Shubo1, DU Wenbo1( ) |
1.Faculty of Materials and Manufacturing, Beijing University of Technology, Beijing 100124, China 2.Weihai Wanfeng Magnesium S&T Development Co. , Ltd. , Weihai 264209, China |
|
Cite this article:
DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate. Acta Metall Sin, 2021, 57(8): 1000-1008.
|
Abstract Magnesium alloys have attracted significant attention due to their excellent characteristics, such as low density, high specific strength, high thermal conductivity, and superior damping ability. The prominent advantages of using magnesium-alloy parts are environmental protection, energy conservation, and emission reduction, especially forged magnesium-alloy parts, which are used to reduce the weight of equipment in transportation and aerospace fields. Presently, there are relatively few investigations on the forged Mg-RE alloys. Based on Mg-Gd binary alloy, a series of Mg-Gd-Er-Zr alloys were developed, exhibiting excellent room-temperature mechanical properties and high-temperature creep resistance. In this study, the Mg-8Gd-1Er-0.5Zr (mass fraction, %) alloy was conducted using a multi-directional forging (MDF) at a high strain rate. The microstructure and texture evolution in various accumulated strains (ΣΔε) were examined, and their effects on the mechanical properties of the alloy were discussed. The results showed that the {} extension twinning was activated within most grains in the early stage of forging. With an increase in ΣΔε, the area fraction of twin decreases, while the area fraction of recrystallization increases. Continuous dynamic recrystallization (CDRX) was the dominant mechanism, supplemented by discontinuous dynamic recrystallization (DDRX) and twin-induced recrystallization (T-DRX). The grain refinement was attributed to the twin-breaking, and the grain size decreased from 33.0 μm to 13.1 μm when ΣΔε was less than 1.32. However, it was attributed to the dynamic recrystallization, and the grain size was further refined to 4.2 μm when ΣΔε was greater than 1.32. As ΣΔε increases, the texture of the alloy changed from basal to double-peak texture, and its intensity increased. When ΣΔε = 0.66, the tensile strength, yield strength, and elongation at room-temperature of the MDFed-alloy reached 295 MPa, 252 MPa, and 13.8%, respectively, which were 80%, 157%, and 13.1% higher than those of the as-solution state.
|
Received: 24 September 2020
|
|
Fund: National Key Research and Development Program of China(2016YFB0101604);Key Topics of Beijing Education Commission(KZ201810005005) |
About author: DU Wenbo, professor, Tel: (010)67392917, E-mail: duwb@bjut.edu.cn
|
1 |
Song J, Xiong S M. The correlation between as-cast and aged microstructures of high-vacuum die-cast Mg-9Al-1Zn magnesium alloy [J]. J. Alloys Compd., 2011, 509: 1866
|
2 |
Liu Y H, Wang Z H, Liu K, et al. Effects of Er on hot cracking susceptibility of Mg-5Zn-xEr magnesium alloys [J]. Acta Metall. Sin., 2019, 55: 389
|
|
刘耀鸿, 王朝辉, 刘 轲等. Er对Mg-5Zn-xEr镁合金热裂敏感性的影响 [J]. 金属学报, 2019, 55: 389
|
3 |
Xia X S, Chen Q, Zhao Z D, et al. Microstructure, texture and mechanical properties of coarse-grained Mg-Gd-Y-Nd-Zr alloy processed by multidirectional forging [J]. J. Alloys Compd., 2015, 623: 62
|
4 |
Li S Q, Tang W N, Chen R S, et al. Effect of pre-induced twinning on microstructure and tensile ductility in GW92K magnesium alloy during multi-direction forging at decreasing temperature [J]. J. Magnes. Alloy., 2014, 2: 287
|
5 |
Guo W, Wang Q D, Ye B, et al. Microstructure and mechanical properties of AZ31 magnesium alloy processed by cyclic closed-die forging [J]. J. Alloys Compd., 2013, 558: 164
|
6 |
Zhou H, Ning H Y, Ma X L, et al. Microstructural evolution and mechanical properties of Mg-9.8Gd-2.7Y-0.4Zr alloy produced by repetitive upsetting [J]. J. Mater. Sci. Technol., 2018, 34: 1067
|
7 |
Tang L C, Liu C M, Chen Z Y, et al. Microstructures and tensile properties of Mg-Gd-Y-Zr alloy during multidirectional forging at 773 K [J]. Mater. Des., 2013, 50: 587
|
8 |
Xia X S, Wang C P, Wu Y, et al. Grain refinement, microstructure and mechanical properties homogeneity of Mg-Gd-Y-Nd-Zr alloy during multidirectional forging [J]. J. Mater. Eng. Perform., 2018, 27: 5689
|
9 |
Wang B Z, Liu C M, Gao Y H, et al. Microstructure evolution and mechanical properties of Mg-Gd-Y-Ag-Zr alloy fabricated by multidirectional forging and ageing treatment [J]. Mater. Sci. Eng., 2017, A702: 22
|
10 |
Li B, Teng B G, Luo D G. Effects of passes on microstructure evolution and mechanical properties of Mg-Gd-Y-Zn-Zr alloy during multidirectional forging [J]. Acta Metall. Sin. (Engl. Lett.,), 2018, 31: 1009
|
11 |
Salandari-Rabori A, Zarei-Hanzaki A, Abedi H R, et al. Micro and macro texture evolution during multiaxial forging of a WE43 magnesium alloy [J]. J. Alloys Compd., 2018, 739: 249
|
12 |
Wu Y Z, Yan H G, Chen J H, et al. Microstructure and mechanical properties of ZK60 magnesium alloy fabricated by high strain rate multiple forging [J]. Mater. Sci. Technol., 2013, 29: 54
|
13 |
Wu Y Z. Research on the technics and mechanisms of ZK series magnesium alloys during high strain rate forging [D]. Changsha: Hunan University, 2012
|
|
吴远志. ZK系列镁合金高应变速率锻造工艺及机理的研究 [D]. 长沙: 湖南大学, 2012
|
14 |
Jiang M G, Yan H, Chen R S. Microstructure, texture and mechanical properties in an as-cast AZ61 Mg alloy during multi-directional impact forging and subsequent heat treatment [J]. Mater. Des., 2015, 87: 891
|
15 |
Shah S S A, Wu D, Wang W H, et al. Microstructural evolution and mechanical properties of a Mg-Gd-Y alloy processed by impact forging [J]. Mater. Sci. Eng., 2017, A702: 153
|
16 |
Shah S S A, Jiang M G, Wu D, et al. Dynamic recrystallization and texture evolution of GW94 Mg alloy during multi- and unidirectional impact forging [J]. Acta Metall. Sin. (Engl. Lett.,), 2018, 31: 923
|
17 |
Zheng X B, Du W B, Wang Z H, et al. Remarkably enhanced mechanical properties of Mg-8Gd-1Er-0.5Zr alloy on the route of extrusion, rolling and aging [J]. Mater. Lett., 2018, 212: 155
|
18 |
Li R J. Study on creep behaviors and mechanism of Mg-8Gd-1Er-0.5Zr alloy [D]. Beijing: BeijingUniversity of Technology, 2018
|
|
李瑞静. Mg-8Gd-1Er-0.5Zr合金蠕变性能及机理研究 [D]. 北京: 北京工业大学, 2018
|
19 |
Barnett M R, Keshavarz Z, Ma X. A semianalytical Sachs model for the flow stress of a magnesium alloy [J]. Metall. Mater. Trans., 2006, 37A: 2283
|
20 |
Zhou X J, Liu C M, Gao Y H, et al. Hot compression behavior of the Mg-Gd-Y-Zn-Zr alloy filled with intragranular long-period stacking ordered phases [J]. J. Alloys Compd., 2017, 724: 528
|
21 |
Ramezani S M, Zarei-Hanzaki A, Abedi H R, et al. Achievement of fine-grained bimodal microstructures and superior mechanical properties in a multi-axially forged GWZ magnesium alloy containing LPSO structures [J]. J. Alloys Compd., 2019, 793: 134
|
22 |
Hong M, Wu D, Chen R S, et al. Ductility enhancement of EW75 alloy by multi-directional forging [J]. J. Magnes. Alloy., 2014, 2: 317
|
23 |
Zhou X J, Zhang J, Chen X M, et al. Fabrication of high-strength AZ80 alloys via multidirectional forging in air with no need of ageing treatment [J]. J. Alloys Compd., 2019, 787: 551
|
24 |
Jiang M G, Xu C, Yan H, et al. Unveiling the formation of basal texture variations based on twinning and dynamic recrystallization in AZ31 magnesium alloy during extrusion [J]. Acta Mater., 2018, 157: 53
|
25 |
Zeng Z R, Zhu Y M, Xu S W, et al. Texture evolution during static recrystallization of cold-rolled magnesium alloys [J]. Acta Mater., 2016, 105: 479
|
26 |
Bhattacharyya J J, Agnew S R, Muralidharan G. Texture enhancement during grain growth of magnesium alloy AZ31B [J]. Acta Mater., 2015, 86: 80
|
27 |
Ding N, Du W B, Fu J L, et al. Research on multi-directional forging process and microstructure and mechanical properties after forging for Mg-8Gd-1Er-0.5Zr alloy [J]. Forg. Stamp. Technol., 2020, 45(5): 1
|
|
丁 宁, 杜文博, 付金龙等. Mg-8Gd-1Er-0.5Zr合金多向锻造工艺及锻后组织与力学性能研究 [J]. 锻压技术, 2020, 45(5): 1
|
28 |
Song B, Xin R L, Chen G, et al. Improving tensile and compressive properties of magnesium alloy plates by pre-cold rolling [J]. Scr. Mater., 2012, 66: 1061
|
29 |
Zhan M Y, Li C M, Shang J L. Investigation of the plastic deformation mechanism and twinning of magnesium alloys [J]. Mater. Rev., 2011, 25(2): 1
|
|
詹美艳, 李春明, 尚俊玲. 镁合金的塑性变形机制和孪生变形研究 [J]. 材料导报, 2011, 25(2): 1
|
30 |
Serra A, Bacon D J. Interaction of a moving {101¯2} twin boundary with perfect dislocations and loops in a hcp metal [J]. Philos. Mag., 2010, 90: 845
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|