| MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS |
MO Yongda1, JIANG Yanbin1,2, LIU Xinhua1,2, XIE Jianxin1,2( ) |
1 Key Laboratory for Advanced Materials Processing of Ministry of Education, University of Science and Technology Beijing, Beijing 100083 2 Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
MO Yongda, JIANG Yanbin, LIU Xinhua, XIE Jianxin. MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS. Acta Metall Sin, 2014, 50(11): 1367-1376.
|
|
|
Abstract The mechanical properties and work hardening behavior of columnar-grained HAl77-2 brass were investigated by means of room temperature tensile test, EBSD and TEM. The effects of grain size on the work hardening rate and tensile ductility of the alloy were discussed. Some references reported that deformation twinning developed in the equiaxed-grained brass led to a reduction in slip length of dislocation and an increase in the work hardening rate at the second stage in the curve of work-hardening vs strain. In this work, however, the results showed that the low-angle subgrain boundaries distributed parallelly were formed in the columnar grain and reduced the slip length of dislocation at the second stage, which was responsible for the rise of the work hardening rate. With increasing grain size, both the yield strength and ultimate tensile strength of the columnar-grained HAl77-2 brass decreased, but its elongation to failure increased significantly from 70.4% for the grain size of 2.0 mm to 84.4% for the grain size of 6.0 mm. Higher performance to resist the plastic instability and better deformation uniformity mainly contributed to the ductility improvement of the larger-grain-sized columnar-grained HAl77-2 brass.
|
|
Received: 02 August 2014
|
|
|
| Fund: National Key Technology R&D Program of China (No.2011BAE23B00) and National Natural Science Foundation of China (No.51104016) |
| [1] |
Kazdal Zeytin H. Mater Charact, 2008; 59: 167
|
| [2] |
Pola A, Gelfi M, Eleonora Depero L, Roberti R. Eng Fail Anal, 2008; 15: 54
|
| [3] |
Trostmann A, Morin O. Desalin Water Treat, 2010; 22: 299
|
| [4] |
Mei J, Liu X H, Jiang Y B, Chen S, Xie J X. Int J Min Met Mater, 2013; 20: 748
|
| [5] |
Huang H Y, Wang Y, Xie J X. Mater Sci Eng, 2014; A596: 103
|
| [6] |
Wang Y, Huang H Y, Xie J X. Mater Sci Eng, 2011; A530: 418
|
| [7] |
Xie J X, Wang Y, Huang H Y. Chin J Nonferrous Met, 2011; 21: 2324
|
|
(谢建新, 王 宇, 黄海友.中国有色金属学报, 2011; 21: 2324)
|
| [8] |
Gan C L, Liu X F, Huang H Y, Xie J X. Mater Sci Eng, 2013; A579: 202
|
| [9] |
Xie J X, Liu X H, Liu X F, Mei J. Chin Pat, 201110210692.9, 2011
|
|
(谢建新, 刘新华, 刘雪峰, 梅 俊. 中国专利, 201110210692.9, 2011)
|
| [10] |
Xiao G H, Tao N R, Lu K. Scr Mater, 2011; 65: 119
|
| [11] |
Zhang P, An X H, Zhang Z J, Wu S D, Li S X, Zhang Z F, Figueiredo R B, Gao N, Langdonet T G. Scr Mater, 2012; 67: 871
|
| [12] |
Thompson A W, Baskes M I, Flanagan W F. Acta Mater, 1973; 21: 1017
|
| [13] |
Hong S I, Laird C. Acta Metall Mater, 1990; 38: 1581
|
| [14] |
Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1
|
| [15] |
El-Danaf E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1999; 30A: 1223
|
| [16] |
Dong H, Thompson A W. Metall Trans, 1985; 16A: 1025
|
| [17] |
Kocks U F, Mecking H. Prog Mater Sci, 2003; 48: 171
|
| [18] |
Asgari S, El-Danaf E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1997; 28A: 1781
|
| [19] |
Sakharova N A, Fernandes J V, Vieira M F. Mater Sci Eng, 2009; A507: 13
|
| [20] |
Engler O,Randle V. Introduction to Texture Analysis: Macrotexture, Microtexture, and Orientation Mapping. 2nd Ed, New York: CRC press, 2009: 392
|
| [21] |
Dieter G E, Bacon D. Mechanical Metallurgy. 3rd Ed, New York: McGraw-Hill, 1986: 289
|
| [22] |
Duggan B J, Hatherly M, Hutchinson W B, Wakefield P T. Metall Sci, 1978; 12: 343
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|