MICROSTRUCTURE OF NODULAR CAST IRON AFTER SURFACE LASER MELTED |
ZHU Zuchang;PAN Huiquan Shanghai University of Engineering Science |
|
Cite this article:
ZHU Zuchang;PAN Huiquan Shanghai University of Engineering Science. MICROSTRUCTURE OF NODULAR CAST IRON AFTER SURFACE LASER MELTED. Acta Metall Sin, 1991, 27(2): 43-47.
|
Abstract The microstructure of nodular cast iron after surface laser melted hasbeen examined by optical microscopy, SEM and scanning Auger microprobe. It wasshown that around the nodular graphite, a double-layer structure is composed ofmartensite+retained austenite together with pseudo-ledeburite at the interface ofmelted pool/matrix. The mechanism of structure formation has also been proposed.
|
Received: 18 February 1991
|
1 Steen W M, Chen Zhenda, West D R F. In: Belforte D, Leritt M eds., The Industrical Laser Annual Handbook, Tulsa, Oklahoma, USA: Pennwell Publishing Company. 1987: 80 2 许敏,张若辉,上海工程技术大学毕业论文,1989 3 Schissler J M, Saverna J. J Heat Treating, 1985; 4(2) : 167 4 徐祖耀.马氏体相变与马氏体.北京:科学出版社,1981:526 5 周继扬,Schmitz W,Engler S.球铁,1989;4:57 6 陈熙琛.金属学问题·哈尔滨工业大学内部资料,1959:83 7 张博,明智清明,确健三等编.任善之,葛丰德,王云昭译.球墨铸铁--基础·理论·应用.北京:机械工业出版社,1988:2 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|