STRUCTURE OF BONDING LAYER OF PLASMA SPRAY WELDING OF Co-Cr ALLOY ON PLAIN STEEL
CHEN Hancun;LIU Zhengyi;ZHUANG Yuzhi SHEN Shixi South China University of Technology; Guangzhou
Cite this article: 

CHEN Hancun;LIU Zhengyi;ZHUANG Yuzhi SHEN Shixi South China University of Technology; Guangzhou. STRUCTURE OF BONDING LAYER OF PLASMA SPRAY WELDING OF Co-Cr ALLOY ON PLAIN STEEL. Acta Metall Sin, 1991, 27(2): 37-42.

Download:  PDF(2672KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The bonding layer of plasma spray welding of Co-Cr alloy on 0.45%C steel was observed to consist of two layers: the several μm only thin sublayerand the decarburized sublayer. The former is composed of amorphous and micro-cpetalline phases together with small amount and uneven distributed complex Cr-Fealloy carbides. Its hardness is greater than HV 500 under 200g load. The later isformed by diffusion of C from subsurface of the substrate to the liquid matal pool.The characteristic welded layer consists also of two sublayers of thick columnarcasting dendrites and fine grains.
Key words:  bonding layer      plasma spray welding      Co-Cr alloy     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/37

1 Savage W F, Nippes E F, Miller T W. Weld J (New York), 1976; 55: 181-s
2 Tong Shushan, Ding Zhangxiong. Advances in Thermal Spraying. Preprint. Proceeding of the 11th International Thermal Spraying Conference, Montreal, Canada, 1986: 691x
[1] ZHOU Bangxin; JIANG Yourong(Nuclear Power Institute of China; Chengdu). TEM STUDY OF BONDING LAYER IN Cu-Al EXPLOSIVELY WELDED JOINT[J]. 金属学报, 1994, 30(15): 104-108.
[2] ZHOU Bangxin;SHENG Zhongqi;PENG Feng Southwest Center for Nuclear Reactor Engineering Research and Design. TEM STUDY OF BONDING LAYERS IN DISSIMILAR ALLOY EXPLOSIVE BONDING JOINTS[J]. 金属学报, 1989, 25(1): 7-12.
No Suggested Reading articles found!