| Research Status of Ductility-Dip Crack Occurring in Nuclear Nickel-Based Welding Materials |
YU Chun1, XU Jijin1, WEI Xiao2, LU Hao1( ) |
1.School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China 2.Advanced Micro-Fabrication Equipment, Inc. (AMEC), Shanghai 201201, China |
|
Cite this article:
YU Chun, XU Jijin, WEI Xiao, LU Hao. Research Status of Ductility-Dip Crack Occurring in Nuclear Nickel-Based Welding Materials. Acta Metall Sin, 2022, 58(4): 529-540.
|
|
|
Abstract Nickel-based alloys and their welding materials have been the key materials in establishing key nuclear equipment due to their excellent corrosion-resistance and high-temperature mechanical properties. Therefore, the welding quality of nickel-based alloys is greatly responsible for the safe service of nuclear plants. However, ductility-dip crack (DDC) was commonly observed in the heat-affected zone during multipass welding. DDC is hard to detect by common nondestructive testing due to the micro‐size of the crack (approximately 100 μm in length). Hence, the high‐temperature DDC problem is a potential threat to the safety of nuclear plants. In this paper, the development of nuclear-level nickel-based alloys and their welding materials is reviewed. To solve the stress corrosion cracking occurring in the welding joint of Inconel 600, Inconel 690 was developed. However, a new reliability problem, DDC, was introduced. Researchers in the world developed Inconel 52, Inconel 52M, and Inconel 52MSS gradually from the design of the chemical components, and the DDC sensibility decreased. Presently, the DDC problem has not been solved completely. The evaluation methods of DDC were introduced, the cracking mechanisms were summarized, and the factors affecting the DDC were analyzed on the view of chemical components and microstructure. In conclusion, the research on DDC has been prospected briefly.
|
|
Received: 13 December 2021
|
|
|
About author: LU Hao, professor, Tel: (021)34202548, E-mail: luhao@sjtu.edu.cn
|
| 1 |
International atomic energy agency. Nuclear power reactors in the world [EB/OL]. Vienna, July 2021.
|
| 2 |
Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735
|
| 3 |
Jang C, Lee J, Kim J S, et al. Mechanical property variation within Inconel 82/182 dissimilar metal weld between low alloy steel and 316 stainless steel [J]. Int. J. Press. Vessels Pip., 2008, 85: 635
|
| 4 |
Li Y F, Wang J Q, Han E H, et al. Multi-scale study of ductility-dip cracking in nickel-based alloy dissimilar metal weld [J]. J. Mater. Sci. Technol., 2019, 35: 545
|
| 5 |
Cheung C, Erb U, Palumbo G. Application of grain boundary engineering concepts to alleviate intergranular cracking in alloys 600 and 690 [J]. Mater. Sci. Eng., 1994, A185: 39
|
| 6 |
Frédérick G, Hernalsteen P. Comparative evaluation of preventive measures against primary side stress corrosion cracking of mill annealed Inconel 600 steam generator tubes [J]. Int. J. Press. Vessels Pip., 1986, 25: 47
|
| 7 |
Hsu S S, Tsai S C, Kai J J, et al. SCC behavior and anodic dissolution of Inconel 600 in low concentration thiosulfate [J]. J. Nucl. Mater., 1991, 184: 97
|
| 8 |
Rios R, Magnin T, Noel D, et al. Critical analysis of alloy 600 stress corrosion cracking mechanisms in primary water [J]. Metall. Mater. Trans., 1995, 26A: 925
|
| 9 |
Fuchs G E, Hayden S Z. The microstructure and tensile properties of mitrogen containing vacuum atomized alloy 690 [J]. Scr. Metall. Mater., 1991, 25: 1483
|
| 10 |
Grönwall B, Ljungberg L, Hübner W, et al. Intercrystalline stress corrosion cracking of Inconel 600 inspection tubes in the Ågesta reactor [J]. Nucl. Eng. Des., 1967, 6: 383
|
| 11 |
Kai J J, Yu G P, Tsai C H, et al. The effects of heat treatment on the chromium depletion, precipitate evolution, and corrosion resistance of Inconel alloy 690 [J]. Metall. Trans., 1989, 20A: 2057
|
| 12 |
Magnin T, Noël D, Rios R. Microfractographic aspects of stress corrosion cracking of Inconel 600 in a pressurized water reactor environment [J]. Mater. Sci. Eng., 1994, A177: L11
|
| 13 |
Miglin B P, Theus G J. Stress corrosion cracking of alloy 600 and 690 in all volatile treated water at elevated temperatures [R]. Polo Alto: Electric Power Research Institute, 1988
|
| 14 |
Kai J J, Tsai C H, Huang T A, et al. The effects of heat treatment on the sensitization and SCC behavior of Inconel 600 alloy [J]. Metall. Trans., 1989, 20A: 1077
|
| 15 |
Casales M, Salinas-Bravo V M, Martinez-Villafañe A, et al. Effect of heat treatment on the stress corrosion cracking of alloy 690 [J]. Mater. Sci. Eng., 2002, A332: 223
|
| 16 |
Crum J R, Scarberry R C. Corrosion testing of Inconel alloy 690 for PWR steam generators [J]. J. Mater. Energy Syst., 1982, 4: 125
|
| 17 |
Dutta R S, Tewari R, De P K. Effects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of Alloy 690 [J]. Corros. Sci., 2007, 49: 303
|
| 18 |
Strauss S D. Inconel 690 is alloy of choice for steam-generator tubing [J]. Power, 1996, 140: 29
|
| 19 |
Collins M G, Lippold J C. An investigation of ductility dip cracking in nickel-based filler materials—Part I [J]. Weld. J., 2003, 82: 288s
|
| 20 |
Davé V R, Cola M J, Kumar M, et al. Grain boundary character in alloy 690 and ductility-dip cracking susceptibility [J]. Weld. J., 2004, 83: 1s
|
| 21 |
Lippold J C. Recent developments in weldability testing [A]. Hot Cracking Phenomena in Welds [M]. Berlin: Springer, 2005: 271
|
| 22 |
Noecker II F F, DuPont J N. Metallurgical investigation into ductility dip cracking in Ni-based alloys: Part II [J]. Weld. J., 2009, 88: 62s
|
| 23 |
Ramirez A J, Lippold J C. High temperature behavior of Ni-base weld metal: Part II—Insight into the mechanism for ductility dip cracking [J]. Mater. Sci. Eng., 2004, A380: 245
|
| 24 |
Wu W T, Tsai C H. Hot cracking susceptibility of fillers 52 and 82 in alloy 690 welding [J]. Metall. Mater. Trans., 1999, 30A: 417
|
| 25 |
Young G A, Capobianco T E, Penik M A, et al. The mechanism of ductility dip cracking in nickel-chromium alloys [J]. Weld. J., 2008, 87: 31s
|
| 26 |
Lippold J C, Nissley N E. Ductility-dip cracking in high chromium, Ni-Base filler metals [A]. Hot Cracking Phenomena in Welds II [M]. Berlin: Springer, 2008: 409
|
| 27 |
Ramirez A J, Garzón C M. Thermodynamic and kinetic approach to ductility-dip cracking resistance improvement of Ni-base alloy ERNiCrFe-7: Effect of Ti and Nb additions [A]. Hot Cracking Phenomena in Welds II [M]. Berlin: Springer, 2008: 427
|
| 28 |
Fink C, Zinke M, Jüttner S. An investigation of ductility-dip cracking in the base metal heat-affected zone of wrought nickel base alloys—Part II: Correlation of PVR and STF results [J]. Weld. World, 2016, 60: 951
|
| 29 |
Collins M G, Lippold J C, Kikel J M. Quantifying ductility-dip cracking susceptibility in nickel-base weld metals using the strain-to-fracture test [A]. 6th International Conference on Trends in Welding Research [C]. Phoenix, AZ, 2003: 586
|
| 30 |
Collins M G, Ramirez A J, Lippold J C. An investigation of ductility dip cracking in nickel-based weld metals—Part II [J]. Weld. J., 2003, 82: 348s
|
| 31 |
Kikel J M, Parker D M. Ductility dip cracking susceptibility of filler metal 52 and alloy 690 [A]. Trends in Welding Research: Proceedings of the 5th International Conference [C]. Pine Mountain, GA, 1998: 757
|
| 32 |
Torres E A, Caram R, Ramirez A J. Grain boundary sliding phenomenon and its effect on high temperature ductility of Ni-base alloys [J]. Mater. Sci. Forum, 2010, 638-642: 2858
|
| 33 |
Hall E L, Briant C L. The microstructural response of mill-annealed and solution-annealed Inconel 600 to heat treatment [J]. Metall. Trans., 1985, 16A: 1225
|
| 34 |
Lippold J C, Nissley N E. Further investigations of ductility-dip cracking in high chromium, Ni-base filler metals [J]. Weld. World, 2007, 51: 24
|
| 35 |
Kiser S D, Zhang R, Baker B A. A new welding material for improved resistance to ductility dip cracking [A]. 8th International Conference on Trends in Welding Research [C]. Pine Mountain, GA, 2009: 639
|
| 36 |
Lee H T, Jeng S L. Characteristics of dissimilar welding of alloy 690 to 304L stainless steel [J]. Sci. Technol. Weld. Joining, 2001, 6: 225
|
| 37 |
Jeng S L, Chang Y H. The influence of Nb and Mo on the microstructure and mechanical properties of Ni-Cr-Fe GTAW welds [J]. Mater. Sci. Eng., 2012, A555: 1
|
| 38 |
Jeng S L, Lee H T, Huang J Y, et al. Effects of Nb on the microstructure and elevated-temperature mechanical properties of alloy 690-SUS 304L dissimilar welds [J]. Mater. Trans., 2008, 49: 1270
|
| 39 |
Jeng S L, Lee H T, Weirich T E, et al. Microstructual study of the dissimilar joints of alloy 690 and SUS 304L stainless steel [J]. Mater. Trans., 2007, 48: 481
|
| 40 |
Yushchenko K, Savchenko V, Chervyakov N, et al. Comparative hot cracking evaluation of welded joints of alloy 690 using filler metals Inconel® 52 and 52 MSS [J]. Weld. World, 2011, 55: 28
|
| 41 |
Hope A T, Lippold J C. Development and testing of a high-chromium, Ni-based filler metal resistant to ductility dip cracking and solidification cracking [J]. Weld. World, 2017, 61: 325
|
| 42 |
Chen J Q. Research on ductility-dip cracking of filler metal 52M[D]. Shanghai: Shanghai Jiao Tong University, 2014
|
|
陈静青. FM-52M熔敷金属高温失塑裂纹机理研究 [D]. 上海: 上海交通大学, 2014
|
| 43 |
Chen J Q, Lu H, Cui W, et al. Effect of grain boundary behaviour on ductility dip cracking mechanism [J]. Mater. Sci. Technol., 2014, 30: 1189
|
| 44 |
Nissley N E, Lippold J C. Ductility-dip cracking susceptibility of filler metal 52 and 52M Ni-base filler metals [A]. 7th International Conference on Trends in Welding Research [C]. Pine Mt, GA,2005: 327
|
| 45 |
Wei X. Investigation and assessment of ductility dip cracking susceptibility in Inconel 690 overlay [D]. Shanghai: Shanghai Jiao Tong University, 2019
|
|
魏 啸. Inconel 690熔覆金属高温失塑裂纹敏感性及评价方法研究 [D]. 上海: 上海交通大学, 2019
|
| 46 |
Nissley N E, Lippold J C. Development of the strain-to-fracture test [J]. Weld. J., 2003, 82: 355
|
| 47 |
Nissley N E, Lippold J C. Ductility-dip cracking susceptibility of austenitic alloys [A]. 6th International Conference on Trends in Welding Research [C]. Phoenix, AZ, 2003: 64
|
| 48 |
Qin R Y, Wang H, He G. Investigation on the microstructure and ductility-dip cracking susceptibility of the butt weld welded with ENiCrFe-7 nickel-base alloy-covered electrodes [J]. Metall. Mater. Trans., 2015, 46A: 1227
|
| 49 |
Moon J, Jang J H, Kim S D, et al. Different aspect of solidification cracking susceptibility and hot ductility behavior of borated stainless steels and the effects of boron content [J]. Mater. Charact., 2020, 164: 110319
|
| 50 |
Chen J Q, Yu C, Chen J M, et al. Assessment of ductility dip cracking susceptibility on Ni based alloy by FEM simulation [J]. Sci. Technol. Weld. Joinning, 2012, 17: 656
|
| 51 |
Mo W L, Lu S P, Li D Z, et al. Effects of filler metal composition on the microstructure and mechanical properties for ER NiCrFe-7 multi-pass weldments [J]. Mater. Sci. Eng., 2013, A582: 326
|
| 52 |
Torres E A, Montoro F, Righetto R D, et al. Development of high-temperature strain instrumentation for in situ SEM evaluation of ductility dip cracking [J]. J. Microsc., 2014, 254: 157
|
| 53 |
Unfried J S, Ramirez A J. Intergranular cracking in alloy 690 with Nb, Mo, and Hf Additions: In situ SEM high temperature deformation study [J]. Mater. Sci. Forum, 2012, 706-709: 945
|
| 54 |
Unfried J S, Torres E A, Ramirez A J. In situ observations of ductility-dip cracking mechanism in Ni-Cr-Fe alloys [A]. Hot Cracking Phenomena in Welds III [M]. Berlin: Springer, 2011: 295
|
| 55 |
Kadoi K, Uegaki T, Shinozaki K, et al. New measurement technique of ductility curve for ductility-dip cracking susceptibility in alloy 690 welds [J]. Mater. Sci. Eng., 2016, A672: 59
|
| 56 |
Kadoi K, Hiraoka M, Shinozaki K, et al. Ductility-dip cracking susceptibility in dissimilar weld metals of alloy 690 filler metal and low alloy steel [J]. Mater. Sci. Eng., 2019, A756: 92
|
| 57 |
Nissley N E. Intermediate temperature grain boundary embrittlement in nickel-base weld metals [D]. Ohio: The Ohio State University, 2006
|
| 58 |
Zheng L, Schmitz G, Meng Y, et al. Mechanism of intermediate temperature embrittlement of Ni and Ni-based superalloys [J]. Crit. Rev. Solid State Mater. Sci., 2012, 37: 181
|
| 59 |
Rhines F N, Wray P J. Investigation of the intermediate temperature ductility minimum in metals [J]. Trans. ASM, 1961, 54: 117
|
| 60 |
Capobianco T E, Hanson M E. Auger spectroscopy results from ductility dip cracks opened under ultra-high vacuum [A]. 7th International Conference on Trends in Welding Research [C]. Pine Mt, GA, 2005: 767
|
| 61 |
Nishimoto K, Saida K, Okauchi H, et al. Microcracking in multipass weld metal of alloy 690 Part 2—Microcracking mechanism in reheated weld metal [J]. Sci. Technol. Weld. Joinning, 2006, 11: 462
|
| 62 |
Nishimoto K, Saida K, Okauchi H, et al. Microcracking in multipass weld metal of alloy 690 Part 3—Prevention of microcracking in reheated weld metal by addition of La to filler metal [J]. Sci. Technol. Weld. Joinning, 2006, 11: 471
|
| 63 |
Vallant R. The influence of different Nb-contents on the hot cracking susceptibility of Ni-base weld metals type 70/20 [A]. Hot Cracking Phenomena in Welds [M]. Berlin: Springer, 2005: 141
|
| 64 |
Yamanaka K, Minami T, Tokimasa K, et al. Intergranular corrosion test method for nickel-based alloy 690 [J]. J. Jpn. Inst. Met, 1985, 49: 125
|
|
山中 和夫, 南 孝男, 時政 勝行 等. Ni基690合金に適用できる粒界腐食試験法 [J]. 日本金属学会誌, 1985, 49: 125
|
| 65 |
Yamaguchi M, Shiga M, Kaburaki H. Grain boundary decohesion by impurity segregation in a nickel-sulfur system [J]. Science, 2005, 307: 393
|
| 66 |
Lee H T, Jeng S L, Kuo T Y. The microstructure and fracture behavior of the dissimilar alloy 690-SUS 304L joint with various Nb addition [J]. Metall. Mater. Trans., 2003, 34A: 1097
|
| 67 |
Jeng S L, Lee H T, Rehbach W P, et al. Effects of Nb on the microstructure and corrosive property in the alloy 690-SUS 304L weldment [J]. Mater. Sci. Eng., 2005, A397: 229
|
| 68 |
Nagano H, Yamanaka K, Kobayashi K, et al. Development and manufacturing system for alloy 690 tubing for PWR steam Generators [J]. Sumitomo Search, 1989, 40: 57
|
| 69 |
Mo W L, Zhang X, Lu S P, et al. Effect of Nb content on microstructure, welding defects and mechanical properties of NiCrFe-7 weld metal [J]. Acta Metall. Sin., 2015, 51: 230
|
|
莫文林, 张 旭, 陆善平 等. Nb含量对NiCrFe-7焊缝金属组织、缺陷和力学性能的影响 [J]. 金属学报, 2015, 51: 230
|
| 70 |
Jeng S L, Lee H T, Kuo T Y, et al. The effects of Mn and Nb on the microstructure and mechanical properties of alloy 152 welds [J]. Mater. Des., 2015, 87: 920
|
| 71 |
Li S, Chen B, Ma Y C, et al. Effects of nitrogen content on microstructure and mechanical property of alloy 690 [J]. Acta Metall. Sin., 2011, 47: 816
|
|
李 硕, 陈 波, 马颖澈 等. N含量对690合金显微组织和室温力学性能的影响 [J]. 金属学报, 2011, 47: 816
|
| 72 |
Lee H T, Jeng S L, Yen C H, et al. Dissimilar welding of nickel-based alloy 690 to SUS 304L with Ti addition [J]. J. Nucl. Mater., 2004, 335: 59
|
| 73 |
Jeng S L, Chang Y H. Microstructure and flow behavior of Ni-Cr-Fe welds with Nb and Mo additions [J]. Mater. Sci. Eng., 2013, A560: 343
|
| 74 |
Nissley N E, Lippold J C. Ductility-dip cracking susceptibility of nickel-based weld metals Part 1: Strain-to-fracture testing [J]. Weld. J., 2008, 87: 257
|
| 75 |
Nissley N E, Lippold J C. Ductility-dip cracking susceptibility of nickel-based weld metals Part 2: Microstructural characterization [J]. Weld. J., 2009, 88: 131
|
| 76 |
Noecker II F F, DuPont J N. Metallurgical investigation into ductility dip cracking in Ni-based alloys: Part I [J]. Weld. J., 2009, 88: 7
|
| 77 |
Han B. Investigation on ductility dip cracking susceptibility of deposited metal with new type 690 nickel alloy strip by electroslag cladding [D]. Beijing: China Academy of Machinery Science & Technology, 2018
|
|
韩 波. 新型690镍基合金带极堆焊熔敷金属DDC裂纹敏感性研究 [D]. 北京: 机械科学研究总院, 2018
|
| 78 |
Mo W L, Hu X B, Lu S P, et al. Effects of boron on the microstructure, ductility-dip-cracking, and tensile properties for NiCrFe-7 weld metal [J]. J. Mater. Sci. Technol., 2015, 31: 1258
|
| 79 |
Nishimoto K, Saida K, Fujiya Y. Amelioration of microcracking in multipass weld metal of alloy 690 by adding rare earth metals [A]. ASME 2009 Pressure Vessels and Piping Conference [C]. Prague: ASME, 2009: 1063
|
| 80 |
Nishimoto K, Saida K, Okauchi H. Microcracking in multipass weld metal of alloy 690 Part 1—Microcracking susceptibility in reheated weld metal [J]. Sci. Technol. Weld. Joining, 2006, 11: 455
|
| 81 |
Saida K, Taniguchi A, Okauchi H, et al. Prevention of microcracking in dissimilar multipass welds of alloy 690 to type 316L stainless steel by Ce addition to filler metal [J]. Sci. Technol. Weld. Joining, 2011, 16: 553
|
| 82 |
Zimina L N, Burova N N, Makushok O V. Effect of hafnium on the structure and properties of wrought nickel-base alloys [J]. Met. Sci. Heat Treat., 1986, 28: 130
|
| 83 |
Feng X L, Hope A, Lippold J C. Effect of Cr on eutectic phase formation and solidification temperature range in Ni-Cr-Hf system [J]. Mater. Lett., 2014, 116: 79
|
| 84 |
Pouranvari M, Ekrami A, Kokabi A H. Solidification and solid state phenomena during TLP bonding of IN718 superalloy using Ni-Si-B ternary filler alloy [J]. J. Alloys Compd., 2013, 563: 143
|
| 85 |
Chellali M R, Zheng L, Schlesiger R, et al. Grain boundary segregation in binary nickel-bismuth alloy [J]. Acta Mater., 2016, 103: 754
|
| 86 |
Rapetti A, Christien F, Tancret F, et al. Surfactant effect of impurity sulphur in ductility dip cracking of a high-chromium nickel model alloy [J]. Scr. Mater., 2021, 194: 113680
|
| 87 |
Platt P, Sayers J, Horner D A, et al. Hydrogen-induced brittle fracture in nickel based alloy 82 weld metal [J]. Corros. Sci., 2019, 153: 118
|
| 88 |
Sahlaoui H, Sidhom H, Philibert J. Prediction of chromium depleted-zone evolution during aging of Ni-Cr-Fe alloys [J]. Acta Mater., 2002, 50: 1383
|
| 89 |
Jiao S Y, Zhang M C, Zheng L, et al. Investigation of carbide precipitation process and chromium depletion during thermal treatment of alloy 690 [J]. Metall. Mater. Trans., 2010, 41A: 26
|
| 90 |
Lim Y S, Kim J S, Kim H P, et al. The effect of grain boundary misorientation on the intergranular M23C6 carbide precipitation in thermally treated alloy 690 [J]. J. Nucl. Mater., 2004, 335: 108
|
| 91 |
Sennour M, Chaumun E, Crépin J, et al. TEM investigations on the effect of chromium content and of stress relief treatment on precipitation in alloy 82 [J]. J. Nucl. Mater., 2013, 442: 262
|
| 92 |
Li H, Xia S, Zhou B X, et al. C-Cr segregation at grain boundary before the carbide nucleation in alloy 690 [J]. Mater. Charact., 2012, 66: 68
|
| 93 |
Li H, Xia S, Zhou B X, et al. The dependence of carbide morphology on grain boundary character in the highly twinned alloy 690 [J]. J. Nucl. Mater., 2010, 399: 108
|
| 94 |
Li H, Xia S, Zhou B X, et al. The growth mechanism of grain boundary carbide in alloy 690 [J]. Mater. Charact., 2013, 81: 1
|
| 95 |
Mo W L, Lu S P, Li D Z, et al. Effects of M23C6 on the high-temperature performance of Ni-based welding material NiCrFe-7 [J]. Metall. Mater. Trans., 2014, 45A: 5114
|
| 96 |
Qin R Y, Duan Z L, He G. Microstructure and ductility-dip cracking susceptibility of circumferential multipass dissimilar weld between 20MND5 and Z2CND18-12NS with Ni-base filler metal 52 [J]. Metall. Mater. Trans., 2013, 44A: 4661
|
| 97 |
Lee T H, Suh H Y, Han S K, et al. Effect of a heat treatment on the precipitation behavior and tensile properties of alloy 690 steam generator tubes [J]. J. Nucl. Mater., 2016, 479: 85
|
| 98 |
Ramirez A J, Lippold J C. New insight into the mechanism of ductility-dip cracking in Ni-base weld metals [A]. Hot Cracking Phenomena in Welds [M]. Berlin: Springer, 2005: 19
|
| 99 |
Chen J Q, Lu H, Yu C, et al. Ductility dip cracking mechanism of Ni-Cr-Fe alloy based on grain boundary energy [J]. Sci. Technol. Weld. Joinning, 2013, 18: 346
|
| 100 |
Wu D, Li D Z, Lu S P. Microstructures and intermediate temperature brittleness of newly developed Ni-Fe based weld metal for ultra-supercritical power plants [J]. Mater. Sci. Eng., 2017, A684: 146
|
| 101 |
Wei X, Xu M J, Chen J Q, et al. Fractal analysis of Mo and Nb effects on grain boundary character and hot cracking behavior for Ni-Cr-Fe alloys [J]. Mater. Charact., 2018, 145: 65
|
| 102 |
Yu X, Lim Y C, Smith R, et al. Reducing hot cracking tendency of dissimilar weld overlay by magnetic arc oscillation [J]. Mater. Sci. Technol., 2014, 30: 930
|
| 103 |
Hua C, Lu H, Yu C, et al. Reduction of ductility-dip cracking susceptibility by ultrasonic-assisted GTAW [J]. J. Mater. Process. Technol., 2017, 239: 240
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|