| EFFECT OF COOLING RATE AND ASPECT RATIO ON MECHANICAL PROPERTIES OF Ti-BASED AMORPHOUS ALLOY COMPOSITES |
Juan MU,Dongmei WANG,Yandong WANG( ) |
| Key Laboratory for Anisotropy and Texture of Materials (MOE), Northeastern University, Shenyang 110819 |
|
Cite this article:
Juan MU,Dongmei WANG,Yandong WANG. EFFECT OF COOLING RATE AND ASPECT RATIO ON MECHANICAL PROPERTIES OF Ti-BASED AMORPHOUS ALLOY COMPOSITES. Acta Metall Sin, 2015, 51(12): 1435-1440.
|
|
|
Abstract Amorphous alloy composite is designed to prevent rapid propagation of shear bands in amorphous phase by introducing the second crystalline phase, which can improve the plasticity of alloy. In situ formed amorphous alloy composites have attracted much interest due to excellent properties and extensive application prospect, especially the dendrite reinforced amorphous alloy composite with excellent tensile plasticity. Recent studies show that the plastic deformation behavior of amorphous alloy composite is not only related to the mechanical properties of the crystalline phase, such as elastic modulus, but also with the size, volume fraction and morphology of the crystalline phase. In addition, the mechanical properties, especially the plastic deformation ability, of amorphous alloys are closely related to topological morphology of the samples, such as aspect ratio. For the amorphous alloy composite, the relationship between mechanical properties and topological morphology of the samples are of interest. In this work, by adjusting preparation process and size of the samples, the effect of cooling rates and aspect ratios on the mechanical properties of Ti45.7Zr33Ni2.9Cu5.9Be12.5 amorphous alloy composites were systematically studied. As decreasing the cooling rate during the preparation process, the sizes of dendrites in the amorphous alloy composites increases. And the crystalline phase presents evolution from branchlets to coarse dendrite. As the cooling rate decreases, strength of the composite decreases while plasticity increases. Moreover, different from the previous reports, the mechanical properties of amorphous alloy composite are not sensitive to the aspect ratio. It is attributed to the existing of the dendrites phase and deformation-induced phase transformation in the dendrites, which may adjust stress distribution of the amorphous alloy composites during deformation process.
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51301034 and 51434008) and Fundamental Research Funds for the Central Universities (Nos.N141004001 and L1502026) |
| [1] | Li Y, Poon S, Shiflet G, Xu J, Kim D, Loffler J. MRS Bull, 2007; 32: 624 | | [2] | Inoue A, Zhang W, Tsurui T, Yavari A, Greer A. Philos Mag Lett, 2005; 85: 221 | | [3] | Hays C C, Kim C P, Johnson W L. Phys Rev Lett, 2000; 84: 2901 | | [4] | Hofmann D, Suh J, Wiest A, Duan G, Lind M, Demetriou M, Johnson W. Nature, 2008; 451: 1085 | | [5] | Choi-Yim H, Busch R, Koster U, Johnson W. Acta Mater, 1999; 47: 2455 | | [6] | Eckert J, Das J, Pauly S, Duhamel C. J Mater Res, 2007; 22: 285 | | [7] | Schuh C, Hufnagel T, Ramamurty U. Acta Mater, 2007; 55: 4067 | | [8] | Deng S T, Diao H, Chen Y L, Yan C, Zhang H F, Wang A M, Hu Z Q. Scr Mater, 2011; 64: 85 | | [9] | Zhang B, Fu H M, Zhu Z Z, Wang A M, Li H, Dong C, Hu Z Q, Zhang H F. Mater Sci Eng, 2012; A540: 207 | | [10] | Zhu Z W, Zhang H F, Hu Z Q, Zhang W, Inoue A. Scr Mater, 2010; 62: 278 | | [11] | Szuecs F, Kim C P, Johnson W L. Acta Mater, 2001; 49: 1507 | | [12] | Qiao J W, Wang S, Zhang Y, Liaw P K, Chen G L. Appl Phys Lett, 2009; 94: 151905 | | [13] | Guo H, Yan P F, Wang Y B, Tan J, Zhang Z F, Sui M L, Ma E. Nat Mater, 2007; 6: 735 | | [14] | Jang D, Greer J R. Nat Mater, 2010; 9: 215 | | [15] | Murray J L. Phase Diagrams of Binary Titanium Alloys. Novelty: ASM International, 1987: 1 | | [16] | Donachie M J. Titanium: a Technical Guide. Novelty: ASM International, 2000: 1 | | [17] | Ferguson I. Technical Report 2438-1. Abingdon: United Kingdom Atomic Energy Assoc, 1976: 1 | | [18] | Mu J, Zhu Z W, Su R, Wang Y, Zhang H F, Ren Y. Acta Mater, 2013; 61: 5008 | | [19] | Scherrer P. G?ttinger Nachrichten, 1918; 2: 98 | | [20] | Hofmann D C, Suh J Y, Wiest A, Lind M L, Demetriou M D, Johnson W. Proc Natl Acad Sci, 2008; 105: 20136 | | [21] | Chen G, Cheng J L, Liu C T. Intermetallics, 2012; 28: 25 | | [22] | Lee C J, Huang J C, Nieh T G. Appl Phys Lett, 2007; 91: 161913 | | [23] | Oh Y S, Kim C P, Lee S, Kim N J. Acta Mater, 2011; 59: 7277 | | [24] | Inoue A. Mater Trans JIM, 1995; 36: 866 | | [25] | Johnson W. MRS Bull, 1999; 24: 42 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|