    					| INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY | 
  					 
  					  										
						LIU Dingming1,2, ZHANG Bo3, WANG Jie1, WANG Aimin1( ), WANG Yandong2, ZHANG Haifeng1, HU Zhuangqi1 | 
					 
															
						1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 School of Materials and Metallurgy, Northeastern University, Shenyang 110819 3 Department of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110136 | 
					 
										
						 | 
					 
				 
				
				Cite this article: 
				
					
			      LIU Dingming, ZHANG Bo, WANG Jie, WANG Aimin, WANG Yandong, ZHANG Haifeng, HU Zhuangqi. INFLUENCE OF TEMPERATURE ON QUASI-STATIC MECHANICAL PROPERTIES OF Zr-45Ti-5Al-3V ALLOY. Acta Metall Sin, 2014, 50(12): 1498-1504.	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract   Zr alloys are widely used in pressurized-water reactors as fuel cladding materials due to their low neutron absorption cross section and excellent radiation resistance. Aside from the aforementioned properties, Zr alloys have high strength, relative low density and many other excellent physical and chemical properties that make them promising structural materials used in the aerospace environment. Zr-45Ti-5Al-3V alloy is a high strength zirconium alloy which is newly developed for use in aerospace environment. The temperature in space environment can change from -100 ℃ to more than 100 ℃, so it is necessary to study the mechanical behavior of Zr-45Ti-5Al-3V alloy under different temperatures. In this work, mechanical properties of Zr-45Ti-5Al-3V alloy under different temperatures (-100, 25, 100 and 200 ℃) and strain rates (10-4, 10-3 and 10-2 s-1) were investigated. The microstructure of the Zr-45Ti-5Al-3V alloy is characterized by SEM and XRD. It is shown that the alloy is comprised of two phases: a lath-like a phase with hcp structure is distributed uniformly in the matrix comprised of a b phase with bcc structure. Quasi-static mechanical properties of Zr-45Ti-5Al-3V alloy were studied in temperature range of -100~200 ℃ under various strain rates (10-4, 10-3 and 10-2 s-1) using the Instron 5528 electric universal material testing machine. The results showed that the alloy possessed yield strength of more than 1355 MPa at room temperature and higher fracture strength in tensile test, but the elongation was small. With increasing temperature, the yield strength and the fracture strength of the alloy decreased, while the amount of plastic deformation increased. Under the condition of compression test, the yield strength also decreased with temperature increasing, while the plasticity and fracture strength reached maximum at room temperature. The influence of strain rate on the mechanical properties of the alloy was not significant under both tensile and compression tests. 
																										     | 
														 
												  		
														
															| 
															    															    															  
															 | 
															
														 
														 														
															
																
																																																																							
																				| ZTFLH:  | 
																				
																					TG 146.414
																				 | 
																				
																					  
																				 | 
																			 
																																																																								
																				|   | 
																				
																					TG 133.25
																				 | 
																				
																					  
																				 | 
																			 
																																																			 
															 | 
														 
																																										
															| Fund: Supported by National Basic Research Program of China (No.2010CB731602) | 
														 
																											    																											 
												 
												
												
												
												 
												
												  
             
             
			              
            
									            
									               
																							
					| [1] | 
					 
					 Wang S H, Yang D Z, He S Y, Lv G. Mater Sci Technol, 2004; 12(6): 579
					 					 | 
				 
												
					 | 
					 
					 (王淑花, 杨德庄, 何世禹, 吕 钢. 材料科学与工艺, 2004; 12(6): 579)
					 					 | 
				 
												
					| [2] | 
					 
					 Li X, Wang L, Yu X M. Mater Sci Eng, 2003; A33: 2987
					 					 | 
				 
												
					| [3] | 
					 
					 Qian J,Zhu Y L,Feng Y Y,Li F B. The Basic of Space Technology. Beijing: Science Press, 1986: 520
					 					 | 
				 
												
					 | 
					 
					 (钱 骥,朱毅麟,冯英远,李凡本.空间技术基础. 北京: 科学出版社, 1986: 520)
					 					 | 
				 
												
					| [4] | 
					 
					 Zhao W J, Zhou B X, Miao Z, Peng Q, Jiang Y R, Jiang H M, Pang H. At Energy Sci Technol, 2005; 39(Sl): 2
					 					 | 
				 
												
					 | 
					 
					 (赵文金, 周邦新, 苗 志, 彭 倩, 蒋有荣, 蒋宏曼, 庞 华. 原子能科学技术, 2005; 39(增刊): 2
					 					 | 
				 
												
					| [5] | 
					 
					 Saintoyant L, Legras L, Brchet Y. Scr Mater, 2011; 64: 418
					 					 | 
				 
												
					| [6] | 
					 
					 Farhat Z N. Mater Sci Eng, 2008; A474: 96
					 					 | 
				 
												
					| [7] | 
					 
					 Kondo R, Suyalatu, Tsutsumi Y, Doi H, Nomura N, Hanawa T. Mater Sci Eng, 2011; C31: 900
					 					 | 
				 
												
					| [8] | 
					 
					 Sun C, Tan J, Ying S H, Li C. Rare Met Mater Eng, 2008; 37(4): 584
					 					 | 
				 
												
					 | 
					 
					 (孙 超, 谭 军, 应诗浩, 李 聪. 稀有金属材料与工程, 2008; 37(4): 584)
					 					 | 
				 
												
					| [9] | 
					 
					 Liang S X, Ma M Z, Jing R, Zhou Y K, Jing Q, Liu R P. Mater Sci Eng, 2012; A539: 42
					 					 | 
				 
												
					| [10] | 
					 
					 Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P. Mater Sci Eng, 2012; A532: 1
					 					 | 
				 
												
					| [11] | 
					 
					 Liang S X, Yin L X, Che H W, Jing R, Zhou Y K, Ma M Z, Liu R P. Mater Des, 2013; 52: 246
					 					 | 
				 
												
					| [12] | 
					 
					 Li Y, Zhang L, Zhu Z W, Li H, Wang A M, Zhang H F. Acta Metall Sin, 2014; 50: 19
					 					 | 
				 
												
					 | 
					 
					 (李 烨, 张 龙, 朱正旺, 李 宏, 王爱民, 张海峰. 金属学报, 2014; 50: 19)
					 					 | 
				 
												
					| [13] | 
					 
					 Liang S X, Ma M Z, Jing R, Tan C L, Liu R P. Mater Sci Eng, 2012; A541: 67
					 					 | 
				 
												
					| [14] | 
					 
					 Wang J, Zhang H W, Wang A M, Li H, Fu H M, Zhu Z W, Zhang H F. Acta Metall Sin, 2012; 48: 636
					 					 | 
				 
												
					 | 
					 
					 (王 杰, 张宏伟, 王爱民, 李 宏, 付华萌, 朱正旺, 张海峰. 金属学报, 2012; 48: 636)
					 					 | 
				 
												
					| [15] | 
					 
					 Liang S X, Yin L X, Jing R, Zhang X Y, Ma M Z, Liu R P. J Mater Res, 2013; 28: 2715
					 					 | 
				 
												
					| [16] | 
					 
					 Tan Y B, Liu W C, Yuan H, Liu R P, Zhang X Y. Metall Mater Trans, 2013; 44A: 5284
					 					 | 
				 
												
					| [17] | 
					 
					 Liang S X, Yin L X, Che H W, Tan C L, Jing R, Zhou Y K, Ma M Z, Liu R P. Mater Des, 2014; 55: 64
					 					 | 
				 
												
					| [18] | 
					 
					 Tan Y B, Yang L H, Tian C, Liu W C, Liu R P, Zhang X Y. Mater Sci Eng, 2014; A597: 171
					 					 | 
				 
												
					| [19] | 
					 
					 Tan Y B, Yang L H, Tian C, Liu R P, Zhang X Y, Liu W C. Mater Sci Eng, 2013; A577: 218
					 					 | 
				 
												
					| [20] | 
					 
					 Zhan Y Z, Zhang G D. Aerospace Mater Technol, 2003; (1): 1
					 					 | 
				 
												
					 | 
					 
					 (湛永钟, 张国定. 宇航材料工艺, 2003; (1): 1)
					 					 | 
				 
												
					| [21] | 
					 
					 Cui Z Q,Tan Y C. Metallography and Heat Treatment. Beijing: Mechanical Industry Press, 2007: 186
					 					 | 
				 
												
					 | 
					 
					 (崔忠圻,覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2007: 186)
					 					 | 
				 
												
					| [22] | 
					 
					 Xu L, Guo R P, Bai C G, Lei J F, Yang R. J Mater Sci Technol, 2014, doi:10.1016/j.jmst.2014.04.011
					 					 | 
				 
												
					| [23] | 
					 
					 Venkatesh B D, Chen D L, Bhole S D. Mater Sci Eng, 2009; A506: 117
					 					 | 
				 
												
					| [24] | 
					 
					 Singh G, Sen I, Gopinath K, Ramamurty U. Mater Sci Eng, 2012; A540: 142
					 					 | 
				 
												
					| [25] | 
					 
					 Feng D.Physics of Metals. Beijing: China Machine Press, 1999: 354
					 					 | 
				 
												
					 | 
					 
					 (冯 端. 金属物理学. 北京: 中国机械出版社, 1999: 354)
					 					 | 
				 
																																 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |