EFFECT OF Ce ON MICROSTRUCTURE AND PROPERTIES OF HOT DIP ALUMINIZED TRITIUM PERMEATION BARRIER
ZHANG Hui, ZHOU Huan, LI Ning, LIU Lin
State Key Lab for Materials Processing and Die & Mould Technology, Huazhong University of Science and Technology, Wuhan 430074
Cite this article: 

ZHANG Hui ZHOU Huan LI Ning LIU Lin. EFFECT OF Ce ON MICROSTRUCTURE AND PROPERTIES OF HOT DIP ALUMINIZED TRITIUM PERMEATION BARRIER. Acta Metall Sin, 2011, 47(12): 1527-1534.

Download:  PDF(1034KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The gradient tritium permeation barrier was fabricated on CLAM steel substrate by hot dip aluminizing (HDA) and subsequent high–temperature diffusion treatment. The effect of Ce element on the microstructure and properties were investigated systematically. The Fe–Al layer with larger thickness and conspicuous serrated interface bonding with the substrate was achieved and the bonding strength of the coating was improved when the content of Ce increase. The gradient distribution of aluminized coating from surface to inter was obtained after thermal diffusion at 850 ℃for 4 h, the gradient coating reduces the thermal stress effectively. The result of the coating properties indicates that the thermal shock resistance and oxidation resistance at high temperature of the coating were also improved with the addition of Ce element.
Key words:  tritium permeation barrier      microstructure      property     
Received:  15 June 2011     
Fund: 

Supported by International Thermonuclear Experimental Reactor Project of China (No.2010GB109000)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00368     OR     https://www.ams.org.cn/EN/Y2011/V47/I12/1527

[1] Smith D L, Konys J, Muroga T. Nucl Mater, 2002; 307: 1314

[2] Smith D L, Park J H, Lyublinski I. Fusion Eng Des, 2002; 61: 629

[3] Aiello A, Ciampichetti A, Benamati G. Nucl Mater, 2004; 329: 1398

[4] Causey R A, Wampler W R. Nucl Mater, 1995; 220: 823

[5] Shan C Q, Wu A J, Li Y J. Nucl Mater, 1992; 191: 221

[6] Liu H B, Tao J, Zhang P Z, Xu J. Mater Rev, 2006; 20(9): 47

(刘红兵, 陶杰, 张平则, 徐江. 材料导报, 2006; 20(9): 47)

[7] Huang Q Y, Li C J, Li Y F, Liu S J, Song Y. Atomic Energy Sci Technol, 2007; 41(supp.): 397

(黄群英, 李春京, 李艳芬, 刘少军, 宋勇. 原子能科学技术, 2007; 41(增刊): 397)

[8] Choy K L. Prog Mater Sci, 2003; 48: 57

[9] Hao J K, Shan C Q, Jin Z J, Chen Q W. Nucl Fusion Plasma Phys, 1996; 16(2): 62

(郝嘉馄, 山常起, 金柱京, 陈庆旺. 核聚变与等离子体物理, 1996; 16(2): 62)

[10] Perujo A, Serra E. Nucl Mater, 1996; 233: 1102

[11] Chen H, Sang G. Corros Sci Prot Technol, 2010; 31(4): 268

(陈镐, 桑革. 腐蚀与防护, 2010; 31(4): 268)

[12] Sun W C. The Behavior of Rare Earth in Aluminium Alloy. Beijing: Chemical Industry Press, 1992: 28

(孙伟成. 稀土在铝合金中的行为. 北京: 化学工业出版社, 1992: 28)

[13] Bahadur A, Mohanty O N. Trans JIM, 1991; 32: 1053

[14] Zhang W, Wen J B, Zhang J M, Fan Z K. Chin Rare Earths, 2005; 26(6): 29

(张伟, 文九巴, 张金民, 范志康. 稀土, 2005; 26(6): 29)

[15] Li C P, Liu X Z, Tian J F, Gao Y Y. Acta Metall Sin, 1989; 25: A382

(李翠屏, 刘兴志, 田继丰, 高允彦. 金属学报, 1989; 25: A382)

[16] Larikov L N. Protect Coatings Met, 1971; 3: 66

[17] Li M S. High Temperature of Metals. Beijing: Metallurgical Industry Press, 2001: 187

(李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 187)

[18] Zhang W, Fan Z K, Guo X J, Wen J B, Zhang J M. J Aeronaut Mater, 2006; 26(2): 16

(张伟, 范志康, 郭献军, 文九巴, 张金民. 航空材料学报, 2006; 26(2): 16)
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[10] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[11] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[12] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[13] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[14] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[15] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
No Suggested Reading articles found!