| CHARACTERIZATIONS OF DLC/MAO COMPOSITE COATINGS ON AZ80 MAGNESIUM ALLOY |
| YANG Wei1, WANG Aiying1, KE Peiling1,JIANG Bailing2 |
1.Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201
2.School of Materials Science and Engineering, Xi’an University of Technology, Xi’an 710048 |
|
Cite this article:
. CHARACTERIZATIONS OF DLC/MAO COMPOSITE COATINGS ON AZ80 MAGNESIUM ALLOY. Acta Metall Sin, 2011, 47(12): 1535-1540.
|
|
|
Abstract Diamond–like carbon (DLC) coating has been widely used to modify the surface mechanical and tribological properties of materials. In most cases, a metallic buffer (e.g., Ti) is used as an interlayer between DLC coating and the substrate to improve the adhesion. In this work, the DLC coating was deposited on the AZ80 Mg alloy substrate using ion beam deposition technique. Specially, a pretreatment of microarc oxidation (MAO) was applied to the Mg alloy substrates to form the DLC/MAO composite coating instead of the metallic interlayer process. As a comparation, the DLC/Ti/MAO and DLC/Ti composite coatings were also deposited on the substrates. The surface morphology and roughness, mechanical, tribological and corrosion properties of the as–deposited coatings were studied. The results indicated that the DLC/MAO composite coating could significantly improved the hardness and wear resistance of the Mg alloy substrates compared with the MAO monolayer. Although the surface roughness of the DLC/MAO coating showed an increase due to the micropores of the MAO coating surface, the friction coefficient and the wear tracks exhibited a similar behavior to that of the DLC/Ti coating. Furthermore, the DLC/Ti/MAO/AZ80 system showed the best tribological properties among the current experimental samples. Meanwhile, the polarization curve revealed that the corrosion resistance of the MAO/AZ80, DLC/MAO/AZ80 and DLC/Ti/MAO/AZ80 film–substrate systems was greatly improved due to the existence of the MgO structure, which processed the high polarization resistance.
|
|
Received: 15 June 2011
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.51072205) and Ningbo Municipal Natural Science Foundation (No.201101A6105005) |
| [1] Guo J, Wang L P, Liang J, Xue Q J, Yan F Y. J Alloys Compd, 2009; 481: 903[2] Wang XM,WuWD, Li S Y, Chen S L, Tang Y J, Bai L, Wang H P. Rare Met Mater Eng, 2010; 39: 1251(王雪敏, 吴卫东, 李盛印, 陈松林, 唐永建, 白黎, 王海平. 稀有金属材料与工程, 2010; 39: 1251)[3] Li H K, Lin G Q, Dong C. Chin J Inorg Chem, 2010; 25:517(李红凯, 林国强, 董闯. 无机材料学报, 2010; 25: 517)[4] Robertson J. Surf Coat Technol, 1992; 50: 185[5] Cruz R, Rao J, Rose T, Lawson K, Nicholls J R. Diamond Relat Mater, 2006; 15: 2055[6] Yoshihiko U, Toshifumi K, Takema T, Yoshio H, Keiro T. Surf Coat Technol, 2011; 205: 2778[7] Davis C A. Thin Solid Film, 1993; 226: 30[8] Funada Y, Awazu K, Yasui H, Sugita T. Surf Coat Technol, 2000; 129: 308[9] McKenzie D R, Muller D, Pailthorpe B A. Phys Rev Lett, 1991; 67: 773[10] Sheeja D, Tay B K, Nung L N. Surf Coat Technol, 2005; 190: 231[11] Wu G S, Sun L L, Dai W, Song L X, Wang A Y. Surf Coat Technol, 2010; 204: 2193[12] Yamauchi N, Ueda N, Cuong N K, Sone T, Hirose Y. Surf Coat Technol, 2005; 193: 277[13] Choi J, Nakao S, Kim J, Ikeyama M, Kato T. Diamond Relat Mater, 2007; 16: 1361[14] Yamauchi N, Ueda N, Okamoto A, Sone T, Tsujikawa M, Oki S. Surf Coat Technol, 2007; 201: 4913[15] Wu G S, Dai W, Zheng H, Wang A Y. Surf Coat Technol, 2010; 205: 2067[16] Yoon S F, Yang H, Ahn R J, Zhang Q. Vacuum, 1998; 49: 67[17] Xue W B, Jin Q, Zhu Q Z, Hua M, Ma Y Y. J Alloys Compd, 2009; 482: 208[18] Wang Y M, Guo L X, Ouyang J H, Zhou Y, Jia D C. Appl Surf Sci, 2009; 255: 6875[19] Liang J, Hu L T, Hao J F. Appl Surf Sci, 2007; 253: 6939[20] Dorner–Reisel A, Schurer C, Irmer G, Muller E. Surf Coat Technol, 2004; 177–178: 830[21] Barchiche C E, Rocca E, Hazan J. Surf Coat Technol, 2008; 202: 4145[22] Statuti R P C C, Radi P A, Santos L V, Trava–Airoldi V J. Wear, 2009; 267: 1208[23] Topolovec–Miklozic K, Lockwood F, Spikes H. Wear, 2008; 265: 1893[24] Yan X B, Xu T, Chen G, Yang S G, Liu H W. Appl Surf Sci, 2004; 236: 328[25] Suzuki M, Ohana T, Tanaka A. Diamond Relat Mater, 2004; 13: 2216[26] Ikeyama M, Nakao S, Sonoda T, Choi J. Nuclear Instrum Methods Phys Res, 2009; 267B: 1675 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|