| Effect of boron on the microstructure and mechanical properties of as-cast TiAl alloy |
| 中国科学院金属研究所 |
|
Cite this article:
. Effect of boron on the microstructure and mechanical properties of as-cast TiAl alloy. Acta Metall Sin, 2007, 43(5): 487-492 .
|
|
|
Abstract Effect of boron on the microstructue and mechanical properties of as-cast Ti-46.5Al-8Nb alloy has been studied. It has been found that boron can refine TiAl grain size and coarsen interlamellar spacing. The interlamellar spacing () shows linearity relationship with grain size d-1/2. The Ultimate tensile strength (UTS) shows Hall-Petch dependences on grain size.
|
|
Received: 20 September 2006
|
|
|
[1] Dimiduk D M. Mater Sci Eng, 1999; A263: 281 [2] London B, Larson D E, Wheeler D A, Aimone P R. In: Darolia R, ed., Structural Intermetallic, Warrendale, PA: TMS, 1993: 151 [3] Loretto M H, Horspool D, Botten R, Hu D, Li Y G, Srivas- tava D, Sharman R, Wu X. Mate Sci Eng, 2002; A329-331: 1 [4] Larson D E. MRS Symp Process, 1990; 194: 285 [5] Inkson B J, Boothroyd C B, Humphreys C J. J Physique IV, 1993; (3): 397 [6] Godfrey A B. PhD Thesis, The University of Birmingham, 1996 [7] Cheng T T. Intermetallics, 2000; 8: 29 [8] Hu D. Intermetallics, 2001; 9: 1037 [9] Hyman M E, McCullough C, Levi C G, Mehrabian R. Metall Mater Trans, 1991; 22A: 1647 [10] Zhong J G. Error Theory and Datum Handling. Beijing: Chemical Industry Press, 1992: 342 (钟继贵.误差理论与数据处理.北京:化学工业出版社,1992: 342) [11] Larson D J, Miller M K. Mater Sci Eng, 1998; A250: 65 [12] Cui Y Y. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2004 (崔玉友.中国科学院金属研究所博士学位论文,沈阳,2004) [13] Hu D, Botten R R. Intermetallics, 2002; 10: 701 [14] Zhang W J, Deevi S C. Mater Sci Eng, 2002; A337: 17 [15] Zhao Y X. MsD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003 (赵亦翔.中国科学院金属研究所硕士学位论文,沈阳,2003) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|