| MICROSTRUCTURE AND PROPERTIES OF Al2O3 CERAMIC COATING BY PLASMA SPRAYING AND LASER REMELTING ON MAGNESIUM ALLOY |
| 大连理工大学 |
|
Cite this article:
. MICROSTRUCTURE AND PROPERTIES OF Al2O3 CERAMIC COATING BY PLASMA SPRAYING AND LASER REMELTING ON MAGNESIUM ALLOY. Acta Metall Sin, 2007, 43(5): 493-497 .
|
|
|
Abstract Al2O3 ceramic coating is prepared by plasma spraying and laser remelting on AZ91HP Mg alloy. The results show that the plasma-sprayed Al2O3 coating consists of -Al2O3 and -Al2O3 phases with the macrostructure of lamellar stacking. After laser remelting, the coating exhibited obvious layer characteristic due to influence of temperature distribution, thermophysical parameters and layer thickness. According to the microstructural difference, the coating can be divided into the melted zone composed of the -Al2O3 columnar crystal, the sintered zone with flocculent-structure characteristic, the residual plasma-sprayed layer with loosen structure, Al-Si transition layer and the substrate. Because of fine structure and high density, the hardness, wear and corrosion resistances of the laser remelted coating are much higher than those of the plasma-sprayed coating and as-received Mg alloy.
|
|
Received: 27 July 2006
|
|
|
[1] Ye H, Zhang J, Sun Z F, Yang H, Zhan J. J Wuhan Univ Technol, 2004; 26(4): 9 (叶宏,张津,孙智富,杨惠,詹捷.武汉理工大学学报,2004;26(4):9) [2] Qi B S, Wang C G. Mechanical Engineering Non-Metal Material. Shanghai: Shanghai Jiaotong University Press, 1996: 96 (齐宝森,王成国.机械工程非金属材料.上海:上海交通大学出版社,1996:96) [3] Majumdar J D, Galun R, Mordike B L, Manna I. Mater Sci Eng, 2003; A361: 119 [4] Majumdar J D, Ramesh B, Chandra A K, Nath I M. JOM, 2004; 56: 101 [5] Dallaire S, Dube D, Fiset M. Wear, 1999; 231: 102 [6] Li J F, Li L, Stott F H. Surf Coat Technol, 2004; 180-181: 500 [7] Wang X B, Liang Y, Yang S L. Surf Coat Technol, 2001; 137: 209 [8] Conde A, Zubiri F, Damborenea J D. Mater Sci Technol, 2002; 334: 233 [9] Yu G, Liu Y L, Li Y, Ye L Y, Guo X H, Zhao L. Chin J Nonferrous Met, 2002; 12: 1087 (余刚,刘跃龙,李瑛,叶立元,郭小华,赵亮.中国有色金属学报,2002;12:1087) [10] Zhang Y J, Yan C W, Wang F H, Cao C N. Mater Prot, 2002; 35(4): 4 (张永君,严川伟,王福会,曹楚南.材料保护,2002;35(4): 4) [11] Zhang X. World Nonferrous Met, 2002; (9): 10 (张珣.世界有色金属,2002;(9):10) [12] Bian F G, Li G L, Liu J H, Liu J J. Mater Prot, 2002; 35(2): 1 (边风刚,李国禄,刘金海,刘家浚.材料保护, 2002;35(2): 1) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|