Abstract Effect of niobium on the microstructural and mechanical properties of as-cast Ti-48Al-0.7B cast alloy has been systematically studied in the paper. It has been found Ti-48Al-0.7B-5Nb alloy has the minimum grain size and the optimum balance mechanical properties.
|
Received: 20 September 2006
|
|
[1] Kim Y W. JOM, 1994; 46(7): 30 [2] Meier G H , Pettit F S H. Mater Sci Technol, 1992; 8: 331 [3] Sheng W B, Yang R, Liu Y Y, Xu D S, Li D. Foundry, 2001; 50: 650 (盛文斌,杨锐,刘羽寅,徐东生,李东.铸造,2001;50: 650) [4] Liu Y, Huang B Y. Chin J Nonferrous Met, 2000; 10: 59 (刘咏,黄伯云.中国有色金属学报, 2000;10:59) [5] Isobe S, Noda T. In: Nathal M V, ed., Structural Inter- metallics, Warrendale, PA: TMS, 1997: 427 [6] Edowlig W, Donlon W T, Allison J E. Mater Res Soc Symp Proc, 1995; 364: 757 [7] Keller M M, Jones P E, Porter W J. JOM, 1997; 49: 42 [8] Liu K, Ma Y C, Gao M, Rao G B, Li Y Y, Ke W, Wu X H, Loretto M H. Intermetallics, 2005; 13: 925 [9] Dimiduk D M. Mater Sci Eng, 1999; A263: 281 [10] Hyman M E, McCullough C, Levi C G, Mehrabian R. Metall Trans, 1991; 22A: 1647 [11] Hu D. Intermetallics, 2002; 10: 851 [12] Zhong J G. Error Theory and Datum handling. Beijing: Chemical Industry Press, 1992: 342 (钟继贵.误差理论与数据处理.北京:化学工业出版社,1992: 342) [13] Jiang Z G, Ma Y C, Chen B, Zhao X J, Gao M, Liu K, Li Y Y. Intermetallics, in press [14] Cheng T T. Intermetallics, 2000; 8: 29 [15] Chen G L, Zhang W J, Liu Z C, Li S J. In: Kim Y W, ed., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 371 [16] Chen B. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2005 (陈波.中国科学院金属研究所博士学位论文,沈阳,2005) [17] Chen G L, Liu Z C, Lin J P, Zhang W J. In: Hemeker K J, ed., Structural Intermetallics, Warrendale, PA: TMS, 2001: 475 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|