Abstract Role of the microstructure of cathode materials in the geometrical
parameter and migration process of cathode spot is studied on the basis
of the observation of microscopic trace of vacuum arc without external
magnetic field. Arc erosion pattern shows that spot craters locate on
the phases with weak voltage withstanding, whose size, morphology and
distribution determine the character of the arc spots. For the
cathode alloys with ultra-fine microstructure the spot is dispersed and
moves quickly on the cathode surface, indicating the spot motion is
controlled by the
microstructure of the electrode materials. The spot migration mode changes from the jumping
motion to a continuous one when the microstructure scale is less
than the spot size. It is concluded
that the constituent phases and their sizes are the
important factor dominating the microscopic migration mode
of arc cathode spots.
|
|
Received: 10 October 2003
|
|
|
[1] Juttner B. J Phys D: Appl Phys, 2001; 34: 3 [2] Boxman R L, Goldsmith S, Greenwood A. IEEE Trans Plasma Sci, 1997; 25: 1175 [3] Miller H C. IEEE Trans Electr Insul, 1990; 25: 765 [4] Latham R V. High Voltage Vacuum Insulation. London:Academic, 1995 [5] Lafferty J M. Vacuum Arcs, Theory and Application. NewYork: Willey, 1980 [6] Boxman R L, Martin P J, Sanders D M. Handbook ofVacuum Arc Science and Technology. Park Ridge, NewJersey: William Andrew Publishing, 1995 [7] Wang F Z, Zhang H, Ding B J, Zhu R H. Mater Sci Eng,2002; A366: 59 [8] Wang Y P, Ding B J. IEEE Trans Compon Packag Technol, 1999; 22: 467 [9] Zhang T, Inoue A. In: Johnson W L, Inoue A, Liu C T,eds., Symp Proc Bulk Metallic Glasses, Warrendale, PA:Materials Research Society, USA, 1998: 361 [10] Ding B J, Yang Z M, Wang X T. IEEE Trans ComponPackag Manuf Technol, 1996; 19: 76 [11] Wang Y P, Yang Z M, Ding B J, Zhou J E. IEEE TransDielectr Electr Insul, 1998; 5: 245K |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|