INFLUENCE OF AUSTENITIC DENDRITES ON MECHANICAL PROPERTIES OF DUCTILE IRON |
ZHOU Jiyang;XIE Zuhua;ZHONG Fengqi Dalian University of Technology |
|
Cite this article:
ZHOU Jiyang;XIE Zuhua;ZHONG Fengqi Dalian University of Technology. INFLUENCE OF AUSTENITIC DENDRITES ON MECHANICAL PROPERTIES OF DUCTILE IRON. Acta Metall Sin, 1992, 28(3): 92-94.
|
Abstract Impact toughnese of ductile nodular cast iron loaded perpendicular to theaustenitic dendrites is found to be 43% higher than thatparallel to ones. Yet tensile strength andelongation of the former are 23% and 30% lower than the later respectively. It is believed thatthe dendritic segregation may cause such differences.
|
Received: 18 March 1992
|