ON AN UNKNOWN PRECIPITATE PHASE IN 2000 SERIES Al ALLOYS
JIN Yan;LI Chunzhi;LI Chunyu;YAN Minggao Institute of Aeronautical Materials; Beijing
Cite this article:
JIN Yan;LI Chunzhi;LI Chunyu;YAN Minggao Institute of Aeronautical Materials; Beijing. ON AN UNKNOWN PRECIPITATE PHASE IN 2000 SERIES Al ALLOYS. Acta Metall Sin, 1991, 27(1): 1-6.
Abstract A new precipitate phase (X phase) has been studied by means of TEMin 2024--2324 Al alloys in different aging conditions. The X phase is determined tohave a c-centered orthorhombic crysta1 structure with a=0.492nm, b=0.852nm andc=0.701nm. It is found that the X phase forms on the helical dislocation in theinitial stage of aging. At lower aging temperature, the S series precipitate phases do-minate the precipitation; while at higher aging temperature, the X phase dominates theprecipitation.
1 Hatch J E. Aluminum: Properties and Physical Metallurgy, ASM, 1984: 189 2 Sanders R E Jr. Sanders T H Jr. Staley J T. Aluminum, 1983; 59: 143 3 Gupta A K, Gaunt P, Chaturvedi M C. Philos Mag, 1987; A55: 375 4 铃木寿,营野幹宏.(车圣)金属,1981;31:277 5 幸田成康.(车圣)金属,1986;36:525 6 Auld J H. Acta Cryst, allogr 1972; A28: S98 7 Kerry S, Scott V D. Met Sci, 1984; 18: 289 8 Auld J H. Mater Sci Technol, 1986; 2: 784 9 Knowles K M, Stobbs W M. Acta Crystallogr, 1988; B44: 207 10 Muddle B C, Polmear I J. Acta Metall, 1989; 37: 777 11 Li Chunzhi, Yan Minggao. Chin J Met Sci Technol, 1987; 3: 27 12 冯端,王业宁,丘第荣.金属物理(下). 北京:科学出版社,1975: 511 13 Jin Yan. Li Chunzhi, Yan Minggao. J Mater Sci, accepted