EFFECT OF LOADING RATE AND TEMPERATURE ON DUCTILE-BRITTLE TRANSITION OF A CARBON STEEL
LIU Yongning;ZHU Jinhua;ZHOU Huijiu;A Kildegaard;J. A. Kristensen Department of Materials Science and Engineering; Xi'an Jiaotong University Department of Mechanical Engineering; Aalborg University; Denmark Department of Materials Science and Engineering;Xi'an Jiaotong University; Xi'an 710049
Cite this article:
LIU Yongning;ZHU Jinhua;ZHOU Huijiu;A Kildegaard;J. A. Kristensen Department of Materials Science and Engineering; Xi'an Jiaotong University Department of Mechanical Engineering; Aalborg University; Denmark Department of Materials Science and Engineering;Xi'an Jiaotong University; Xi'an 710049. EFFECT OF LOADING RATE AND TEMPERATURE ON DUCTILE-BRITTLE TRANSITION OF A CARBON STEEL. Acta Metall Sin, 1990, 26(3): 44-49.
Abstract The dynamic fracture toughness of a mild steel has been studied atdifferent loading rates and temperatures. The material exhibits a transition fromtough to brittle fracture with the changing of loading rate alone. Analysis of thefracture process by the theory of thermal activation suggests that the fracture activ-ation energy approximates the bond energy on the {100} plane of a unit cell. The tough-ness can be resolved into two parts, J_(Id)=J_a+J_t. where J_a is the athermal part, beingindependent on temperature and loading rate, while J_t=(K/K_0)~(1/″) exp (Q_f/nkT), whichcontrols the fracture process is temperature and loading rate dependent. the transi-tion of fracture mechanism caused by both temperature and loading rate is associatedwith the thermal movement of atoms.
1 Hahn G T. Metall Trans, 1984; 15A: 947 2 Knott J F. In: Valluri S R, Taplin D M R, Ramarao P, Knott J F, Dubey R eds., Advances in Fracture Rescarch (Fracture 84) . Vol. I, Oxford: Pergamon, 1984: 83 3 Ritchie R O, Server W L, Wullaert R A. Metall Trans, 1979; 10A: 1557 4 Bowen P. Pruce S G, Knott J F. Acta Metall, 1987; 35: 1735 5 Thomson R M. J Phys Chem Solids, 1987; 48: 965 6 Serrver W L, Wulla R A, Ritchie R O. Trans ASME, Ser H: J Eng Mater Technol. 1980; 102: 192 7 Blumenauer H, Wagner I. In: Valluri S R, Taplin D M R, Ramarao P. Knott J E、Dubey R eds., Advances in Fracture Research (Fracture 84) , Vol. V, Oxford: Pergamon, 1984: 3145 8 Kocks U F, Argon A S, Ashby M F. Thermodynamics and Kinetics of Slip, Pergamon. 1975 9 Bryan R H, Bass B R, Merkle J G. Pugh C E, Robinson G C, Whitman G D. Eng Fract Mech. 1986; 23: 81 10 Guy A O, Introduction to Materials Science, New York: McGrama-Hill. 1972: 465 11 方俊鑫,陆栋.固体物理学(上册),上海科学技术出版社,1980 12 Knott J F. J Iron Steel Inst. 1966; 204: 104w