Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (6): 136-142    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE AND FRACTURE FEATURE OF ZTA-SiC_w COMPOSITE
ZHANG Jinsong;XIA Fei;LUO Chuan;CAO Lihua;ZHAO Kuanfang;HU Wanping Institute of Metal Research; Academia Sinica; Shenyang ZHANG Jinsong; Research assistant; Institute of Metal Research; Academia Sinica;Shenyang 110015
Cite this article: 

ZHANG Jinsong;XIA Fei;LUO Chuan;CAO Lihua;ZHAO Kuanfang;HU Wanping Institute of Metal Research; Academia Sinica; Shenyang ZHANG Jinsong; Research assistant; Institute of Metal Research; Academia Sinica;Shenyang 110015. MICROSTRUCTURE AND FRACTURE FEATURE OF ZTA-SiC_w COMPOSITE. Acta Metall Sin, 1989, 25(6): 136-142.

Download:  PDF(1848KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A ZTA-SiC_W ceramic composite of room temperature strength 935-1110 MPa and fracture toughness 9.7MPa·m~(1/2) was prepared by the sol-gel process.Its microstructure and fracture feature have been examined by means of X-raydiffraction analysis and electron microscope observations. The results show that thewhiskers are well dispersed and the matrix has an obvious texture character. Betweenthe whisker and matrix, there is a great number of transcrystalline and trans-crystalline connective relation other than part of conventional polycrystalline connective ones. Certain secondary cracks closely related with local whisker groupare found on the fracture surface. It may be a new reinforcing and tougheningmechanism by whisker group, of which the whiskers in the local whisker grouparrest synergetically the crack propagation accompaning with the formation of se-condary cracks.
Key words:  ceramic composite      microstructure      fracture     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/136

1 Roy R. Scicnce, 1987; 238: 1664
2 Pierre A C, Uhlmann D R, Hordonneau A. Rev Int Hautes Temp Refract, 1986; 23: 29
3 Claussen N, Weisskopf K-L, Ruehle M. J Am Ceram Soc, 1986; 69: 288
4 Swab J. Ceram Eng Sci Proc, 1987; 8: 886
5 Claussen N, Petson G. J Phys (Paris) Collpque, 1986; 47: 693
6 Homeny J, Vaughn W L, Ferber M K. Am Ceram Soc Bull, 1987; 66: 333
7 Wei G C, Becher P F. Am Ceram Soc Bull, 1985; 64: 298
8 Garvie R C, Nicholson P S. J Am Ceram Soc, 1972; 55: 303e
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!