| QUANTITATIVE RELATION BETWEEN YIELD STRESS AND R-VALUE ALONG DIRECTIONS PARALLEL AND PERPENDICULAR TO ROLLED Ti PLATE |
| ZHANG Derong Shenyang Institute of Aeronautical Engineering ZHANG Derong; associate professor; Department of Aeronautics; Shenyang Institute of Aeronautical Engineering; Shenyang 110031 |
|
Cite this article:
ZHANG Derong Shenyang Institute of Aeronautical Engineering ZHANG Derong; associate professor; Department of Aeronautics; Shenyang Institute of Aeronautical Engineering; Shenyang 110031. QUANTITATIVE RELATION BETWEEN YIELD STRESS AND R-VALUE ALONG DIRECTIONS PARALLEL AND PERPENDICULAR TO ROLLED Ti PLATE. Acta Metall Sin, 1989, 25(6): 131-135.
|
|
|
Abstract An attempt was made on the quantitative prediction of the relation-ship batween yield stress and R-value along the directions parallel and perpendicul-ar to rolled Ti plate based on analysis of the previous experimental data. It is sh-own that the yield stress along one direction and another is synchronized withR-value. Based on the theory of plasticity a formula of σ_(1s)/σ_(7s)=[1+1/R_2)/(1+1/R_1)]~(1/2)was proposed. In statistic estimation, the calculated results after the formula are inbetter agreement with the experimental data. The availability of this formula wasbriefly discussed also.
|
|
Received: 18 June 1989
|
1 周维贤.TC1钛板的机械性能及其异性情况,西北工业大学科技资料,总字第1059期,1979 2 翟平.TA2M钛板机械性能及各向异性,西北工业大学科技资料,ZHZ8018,1981 3 周维贤.剖面收缩率在评估钛板成形性方面的意义,中国航空学会飞机制造技术学术交流会资料,1988 4 Hill R. The Mathematical Theory of Plasticity. Oxford at the Clarendon Press, 1950: 317--340 5 Slater R A C.王仲仁,袁祖培译.工程塑性理论及其在金属成形中的应用,机械工业出版社’1983:141 6 王仁,熊祝华,黄文彬.塑性力学基础,科学出版社,1982:176 7 Babel H W, Eitman D A, McIver R W. ASM Trans D: J Basic Eng, 1967; 89(1) : 13 8 张德荣.沈阳航空工业学院学报,1987;(1) :29 |
| No Suggested Reading articles found! |
|
|