| ANALYSIS OF THE THERMAL STABILITY OF COPPER SPECIMENS DEFORMED BY HIGH–PRESSURE TORSION |
| XIE Ziling 1;2; WU Xiaolei 2; XIE Jijia 2; HONG Youshi 2 |
1. College of Architecture and Civil Engineering; University of Wenzhou; Wenzhou 325035
2. State Key Laboratory of Nonlinear Mechanics; Institute of Mechanics; Chinese Academy of Sciences; Beijing 100190 |
|
Cite this article:
XIE Ziling WU Xiaolei XIE Jijia HONG Youshi. ANALYSIS OF THE THERMAL STABILITY OF COPPER SPECIMENS DEFORMED BY HIGH–PRESSURE TORSION. Acta Metall Sin, 2010, 46(4): 458-465.
|
|
|
Abstract The thermal stability of Cu specimens subjected to high–pressure torsion (HPT) deformation with varying strains was studied by optical icroscope (OM), differential scanning calorimetry (DSC) and transmission electron microscope (TEM). It is found that cellular subgrains with high dislocation densities are firstly formed at a low strain level, some of the cellular subgrains are transformed into dislocation–free equiaxed grains at larger strains. A single exothermal peak between 150 and 250 ℃ is shown in DSC curves, corresponding to the heat release due to recrystallization and subsequent grain growth. With the increase of strain, the peak position is shifted to a lower temperature and then is leveled off, but the stored energy of cold work, calculated according to the area under a peak, increases with strain at relatively low strain level and reaches its maximum value of 0.91 J/mol at strain of 13. Further deformation induces the stored energy of cold work to decrease due to the dynamic recovery of microstructure. A large drop in hardness appears in as–deformed samples at a temperature 45 ℃ lower than the start temperature of the exothermal peak after isochronal annealing, indicating that the recrystallization and grain growth process is closely relatine to annealing time and temperatur.
|
|
Received: 12 October 2009
|
| Fund: Supported by National Natural Science Foundation of China (Nos.10721202, 10772178 and 50571110) |
| [1] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[2] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[3] Wang J T, Kang S B, Kim H W, Horita Z. J Mater Sci, 2002; 37: 5223
[4] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S. Acta Mater, 2006; 54: 655
[5] Wu X L, Tao N R, Wei Q M, Jiang P, Lu J, Lu K. Acta Mater, 2007; 55: 5768
[6] Xie Z L, Wu X L, Xie J J, Hong Y S. Acta Metall Sin, 2008; 44: 803
(谢子令, 武晓雷, 谢季佳, 洪友士. 金属学报, 2008; 44: 803)
[7] Zhang K, Weertman J R, Eastman J A. Appl Phys Lett, 2005; 87: 61921
[8] Liao X Z, Kilmametov A R, Valiev R Z, Gao H S, Li X D, Mukherjee A K, Bingert J F, Zhu Y T. Appl Phys Lett, 2006; 88: 21909
[9] Schafler E, Kerber M B. Mater Sci Eng, 2007; A462: 139
[10] Jiang H G, Zhu Y T, Butt D P, Alexandrov I V, Lowe T C. Mater Sci Eng, 2000; A290: 128
[11] Pan J S, Tong J M, Dian M B. Foundation of Material Science. Beijing: Tsinghua University Press, 1998: 512
(潘金生, 仝健民, 田民波. 材料科学基础. 北京: 清华大学出版社, 1998: 512)
[12] Wang Y M, Jiao T, Ma E. Mater Trans, 2003; 44: 1926
[13] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. New York: Pergamon, 2004:11
[14] Zhang Y, Tao N R, Lu K. Acta Mater, 2008; 56: 2429 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|