| 低温处理对SiC_p/6061Al复合材料残余应力的影响 |
| 李寰;李家宝;孙立志;王中光 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室 |
|
| EFFECT OF LOW TEMPERATURE TREATMENT ON RESIDUAL STRESSES IN SiC_p/6061Al COMPOSITE |
| LI Huan;LI Jiabao;SUN Lizhi;WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1996-05-10;in revised form 1996-09-23) |
引用本文:
李寰;李家宝;孙立志;王中光. 低温处理对SiC_p/6061Al复合材料残余应力的影响[J]. 金属学报, 1996, 32(12): 1279-1284.
,
,
,
.
EFFECT OF LOW TEMPERATURE TREATMENT ON RESIDUAL STRESSES IN SiC_p/6061Al COMPOSITE[J]. Acta Metall Sin, 1996, 32(12): 1279-1284.
| 1ArsenaultRJ,WuSB.MaterSciEng,1978;96:772LedbetterHM,AustuMW.MaterSciEng,1987;89:533CaoHC,ThoulusMD,EvansAG.ActaMetall,1988;136:20374PovirkGL,NeedlemanA,NuttSR.MaterSciEng.1990;A125:1295HagaO,KoyamaH,KawadaK,OgawaK.In:FujiwaraH,AbeT,TanakaKeds.,ProcThirdIntConfonResidualStresses,Tokushima:ElsevierSciencePublishersLTD,1991;1:766LiH,LiJB,SunLZ,LiSX,WangZG.MaterSciEng,inpress,19967SunZM,LiJB,WangZG,LiWJ.ActaMetall,1992:40:29618ShiN,WilnerB,ArsenaultRJ.ActaMetall,1992;40:28419InstructionMannualforStrainflexMSFCat.No.2903,JapanRegakuElectricalLtd.Tokyo,Japan,197210ReedRP,ClarkAF.MaterialsatLowTemperatures.CarnesPublicationServices,Inc,1983:40111著,王润等译.金属与合金的物理性能.北京:中国工业出版社,1961:32712孙正明.中国科学院金属研究所博士学位论文,199213ShiN,ArsenaultRJ.JComposTechnolRes,1991;13(4):21114WangZhirui,ChenTzi-Kang,LloydDJ.MetallTrans,1993;24A:197 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|