| 添加纳米Al_2O_3对Al_2O_3陶瓷增韧和增强的影响 |
| 李广海;江安全;张立德 |
| 中国科学院固体物理研究所 |
|
| TOUGHENING AND STRENGTHENING OF Al_2O_3 CERAMICS THROUGH NANO-Al_2O_3 ADDITION |
| LI Guanghai;JIANG Anquan;ZHANG Lide (Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)(Manuscript received 1995-12-27; in revised form 1996-08-12) |
引用本文:
李广海;江安全;张立德. 添加纳米Al_2O_3对Al_2O_3陶瓷增韧和增强的影响[J]. 金属学报, 1996, 32(12): 1285-1288.
,
,
.
TOUGHENING AND STRENGTHENING OF Al_2O_3 CERAMICS THROUGH NANO-Al_2O_3 ADDITION[J]. Acta Metall Sin, 1996, 32(12): 1285-1288.
| 1HahnH.NanostructMater,1993;2:2512GleiterH.ProgMaterSci,1991;33:2233JangJSC,KochCC.ScrMetallMater,1990;24:15994HofterHJ,AverbackRS.ScrMetallMater,1990;24:24015SuryanarayanaC.IntMaterRev,1995;40:416AnddevskiRA.JMaterSci,1994;29:6147李广海,费广涛,张立德.'95秋季中国材料研讨会论文集.北京,1996:488张立德,牟季美.纳米材料学.沈阳:辽宁科学技术出版社,19949DavidgeRW,GreenTJ.JMaterSci,1968;3:629r |
|