| 人工神经网络在不锈钢-铝固液相压力复合研究中的应用 |
| 张鹏;崔建忠;张奇志;杜云慧;富江涛;巴立民 |
| 东北大学 |
|
| ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM |
| ZHANG Peng;CUI Jianzhong;ZHANG Qizhi;DU Yunhui;FU Jiangtao;BA Limin (Northeastern University;Shenyang 110006)(Manuscript received 1996-05-21;in revised form 1996-07-11) |
引用本文:
张鹏;崔建忠;张奇志;杜云慧;富江涛;巴立民. 人工神经网络在不锈钢-铝固液相压力复合研究中的应用[J]. 金属学报, 1996, 32(12): 1275-1278.
,
,
,
,
,
.
ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM[J]. Acta Metall Sin, 1996, 32(12): 1275-1278.
| 1富江涛.东北大学硕士论文,19962HopfieldJJ.ProcNatAcadSciUSA,1982;79:25543PsaltisD,SiderisA,TamanmuyaA.IEEEControlSystMag,1988;8:174严六明,钦佩,李重河.科学通报,1994;39(1):945王殿辉,诸良银.有色金属,1994;46(1):296SongRG,ZhangQZ,TsengMK,ZhangBJ.MaterSciEng,1995;C3:39t |
|