稀土对复合镀工艺及镀层性能的影响 |
郭忠诚 |
昆明理工大学 |
|
EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING |
GUO Zhongcheng(Department of Metallurgy; Kunming Institute of Technology;Kunming 650093)(Manuscript received 1995-09-20; in revised form 1995-12-05) |
引用本文:
郭忠诚. 稀土对复合镀工艺及镀层性能的影响[J]. 金属学报, 1996, 32(5): 516-520.
.
EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING[J]. Acta Metall Sin, 1996, 32(5): 516-520.
1ThomaM.PlatSurfFin,1984;76:532MatsufumiT.J METFinishSocJpn,1987;38:5673VestGE.MetalFinishing,1967;65:824郭忠诚.有色金属(季刊),1994:46:675郭忠诚,材料保护,1991:24:15 |
|