| 微量碳对淬态Fe-Si-B非晶丝表面层结构及脆性的影响 |
| 梁乃茹;李殿臣;何开元;赖祖涵 |
| 包头稀土研究院;东北大学 |
|
| EFFECTS OF MINOR-CARBON CONTENT ON SURFACE STRUCTURES AND EMBRITTLEMENT OF AS-CAST Fe-Si-B AMORPHOUS ALLOY WIRE |
| LIANG Nairu; LI Dianchen (Baotou Research institute of Rare Earth; Baotou 014010); HE Kaiyuan; LAI Zuhan (Northeastern University; Shenyang 110006)(Manuscript received 1995-03-28; in revised form 1995-10-30) |