|
|
|
| 304不锈钢孔蚀过程原位图象采集与分析 |
| 苏润西;宋诗哲 |
| 天津大学材料学院;天津;300072;天津大学材料学院;天津;300072 |
|
| IN-SITU IMAGE GRAB AND ANALYSIS FOR PITTING PROCESS OF 304 STAINLESS STEEL |
| SU Runxi; SONG Shizhe (School of Materials Science and Engineering; Tianjin University; Tianjin 300072)Correspondent. SONG Shizhe; professor; Tel: (022)27405823; Fax: (022)27404724;E-mail: szsong@tju. edu. cn |
引用本文:
苏润西;宋诗哲. 304不锈钢孔蚀过程原位图象采集与分析[J]. 金属学报, 1998, 34(9): 966-970.
,
.
IN-SITU IMAGE GRAB AND ANALYSIS FOR PITTING PROCESS OF 304 STAINLESS STEEL[J]. Acta Metall Sin, 1998, 34(9): 966-970.
1 Itzhak D, Dinstein I,Zilberberg T CorrosSci, 1981; 21: 17 2 Costa J M , Sagues F, Vilarrasa M. Corros Sci, 1991;32:665 3 苏润西,宋诗哲第九届全国电化学会议论文摘要集,泰安,1997:425(Su R X,Song S Z Proc 9th CSE National Meeting, Tai'an China, 1997:425) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|