| 1Cr18Ni9Ti不锈钢应力腐蚀开裂的电位扰动极化效应 |
| 牛林;曹楚南;林海潮 |
| 中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015;中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015;中国科学院金属腐蚀与防护研究所金属腐蚀与防护国家重点实验室;沈阳;110015 |
|
| EFFECT OF POTENTIAL PERTURBATION POLARIZATION ON THE STRESS CORROSION CRACKING OF 1Cr18Ni9Ti STAINLESS STEEL |
| NIU Lin; CAO Chunan; LIN Haichao (State Key Laboratary for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: NIU Lin; Tel: (024)23915893; Fax: (094)23894149; E-mail: lin.h.c@icpm.syb.ac.cn |
引用本文:
牛林;曹楚南;林海潮. 1Cr18Ni9Ti不锈钢应力腐蚀开裂的电位扰动极化效应[J]. 金属学报, 1998, 34(9): 959-965.
,
,
.
EFFECT OF POTENTIAL PERTURBATION POLARIZATION ON THE STRESS CORROSION CRACKING OF 1Cr18Ni9Ti STAINLESS STEEL[J]. Acta Metall Sin, 1998, 34(9): 959-965.
1 Hoar T P, Hines J G Corrosion, 1963; 19: 331t 2 Hehemann R F. Metall Trans A, 1985; 16A: 1909 3 Haruyama S, Asawa S. Corros Sci, 1973;13:395 4 Tanno K, Yashiro H, Kawamura Y, Umegai K, Kumagai N. Corrosion, 1993; 49: 319 5 Maier I, Galvele J R. Corrosion, 1980; 36: 309 6 Congleton J, Yang W Corros Sci, 1995; 37: 429 7 Manfredi C, Maier I A, Galvele J R. CorrosSci, 1987; 27: 887 8 Parkins R N. Corros Sci, 1980; 20: 147 9 Magniu T, Chieragatti R, Oltra R. Acta Metall Mater, 1990; 38: 1313 10 KanfmanM J, Fink J K. Acta Metall, 1988; 36: 2213 11 张天成,褚武扬,史训清,朱万旭,刘宝深.金属学报,1997;33:309(Zhang T C, Chu W Y, Shi X C, Zhu W X, Liu B C, Acta Metall Sin , 1997; 33: 309) 12 林昌健,冯祖德,林福龄,王发扬,谭建光,王元辉电化学,1995;1:439(Lin C J, Feng Z D, Lin F L, Wang F Y, Tan J G, Wang Y H. Electrochemistry, 1995;1: 439) 13 田昭武著.电化学研究方法北京:科学出版社,1984:201(Tian Z W. Research Method inElectrochemistry. Beijing: Science Press, 1984: 201) |
|